journal article·2024-01

Fabrication of TA2–304 SS laminated metal composite using directed energy deposition-arc: Microstructure, mechanical property, and corrosion resistance

Gang Mou, Haiyang Sheng, Hongliang Xiang, Chen Shen, Kaikui Zheng, Yuhan Ding, Xueming Hua

Publisher page

Abstract

Conventional fabricating methods of TA2–304 SS laminated metal composite (LMC) (e.g., hot rolling, hot stamping, and explosive welding) have difficulty in removing brittle Ti Fe intermetallic compounds (IMCs) and are not suitable for the preparation of the small size structure components or transition joints. Additive manufacturing of LMCs has the potential to achieve the desired microstructure, properties, and structure. In this study, TA2–304 SS LMC, which has been extensively employed in pipe flanges of nuclear plants and bows of sonar dome, was well fabricated by utilizing directed energy deposition-arc (DED-arc) and copper‑nickel alloy transition interlayers, and the formation of brittle Ti Fe IMCs was suppressed. The results of this study indicated that the standard deviation of the height of the surface morphology reconstructed by adopting Python VTK technique was evaluated as 0.67. Furthermore, copper‑nickel transition interlayers possessed the capability of isolating Ti from Fe atoms through the formation of laminar-distributed microstructure. Specifically, the Interlayer1 was comprised of (Fe, Cr) grains with different shapes and small-size (Cu) equiaxial grains, Interlayer2 covered large-size (Cu, Ni) dendritic grains and intergranular (Cu), and the TA2 layer comprised α-Ti and Ti 2Cu. The result also showed that thermal cycle-induced recovery and recrystallization and diffusion-induced elemental interaction accounted for the different microstructures. Moreover, the interface between the TA2 and Interlayer2 layers contained TiCu 4 + (Cu), Ti 3Cu 4 + TiCu 4, Ti 2Cu + TiCu, and TiCu + Ti 2 Cu eutectoid microstructures, which resulted in the highest hardness of 450Hv as well as crack initiation and extension. Furthermore, due to the uniform-distribution of microstructure in the absence of brittle IMCs, the average shear strength was 234.0 MPa, which reached the strength of the conventional method and conformed to the standard requirements. Multiple groups of galvanic reactions between different transition materials can result in reduced corrosion resistance, and the oxidation-reduction reactions can lead to the formation of massive oxides.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Evolution mechanism of microstructure and bond strength based on interface diffusion and IMCs of Ti/steel clad plates fabricated by double-layered hot rolling10.1016/j.jmatprotec.2022.117780 ↗
2. Investigation on the interfacial microstructure and mechanical properties of Ti alloy/HSLA steel clad plates fabricated by vacuum roll-cladding10.1016/j.msea.2022.143774 ↗
3. Effect of pulse current treatment on interface structure and mechanical behavior of TA1/304 clad plates10.1016/j.msea.2022.143583 ↗
4. Additive manufacturing of a functionally graded material from Ti-6Al-4V to invar: experimental characterization and thermodynamic calculations10.1016/j.actamat.2016.12.070 ↗
5. Stainless steel to titanium bimetallic structure using LENSTM
6. Recent development in modeling and analysis of functionally graded materials and structures10.1016/j.paerosci.2015.07.001 ↗
7. Advances in additive manufacturing of metal-based functionally graded materials10.1080/09506608.2019.1709354 ↗
8. Effect of post-weld heat treatment on the interface microstructure of explosively welded titanium–stainless steel composite10.1016/j.msea.2008.04.032 ↗
9. Deformation and fracture of Ti/439 stainless steel clad composite at intermediate temperatures10.1016/j.msea.2015.11.041 ↗
10. Microstructures and mechanical properties of laser melting deposited Ti6Al4V/316L functional gradient materials10.1016/j.msea.2021.141355 ↗
11. Microstructure investigation and fracture mechanism of TC4−304L dissimilar joints fabricated by the cold metal transfer arc-brazing method10.1016/j.jmrt.2021.11.070 ↗
12. Influence of annealing on the microstructure, interfacial compounds and mechanical properties of hot rolling bonded Ti/steel clad plate with bimetallic interlayered steel and vanadium10.1016/j.msea.2019.138227 ↗
13. Additive manufacturing of Ti-6Al-4V/V-interlayer/17-PH steel functionally graded material using angular and spheroidal V powders10.1016/j.matlet.2023.133936 ↗
14. Effect of Nb interlayer on microstructure and property of Ti-6Al-4V/690 MPa grade steel clad plate by vacuum rolling10.1016/j.msea.2023.145450 ↗
15. Functional bimetallic joints of Ti6Al4V to SS410
16. Interfacial microstructure and properties of a vacuum hot roll-bonded titanium-stainless steel clad plate with a niobium interlayer10.1007/s40195-013-0283-9 ↗
17. Interfacial features of TiAl alloy/316L stainless steel joint brazed with Zr−Cu−Ni−Al amorphous filler metal10.1016/S1003-6326(21)65607-8 ↗
18. Investigation of interfacial structure and mechanical properties of titanium clad steel sheets prepared by a brazing-rolling process10.1016/j.msea.2017.06.095 ↗
19. Hot roll bonding between commercially pure titanium and high-strength low-alloy steel using Fe interlayer10.1007/s42243-019-00322-x ↗
20. Mechanical properties and interfacial structure of hot-roll bonding TA2/Q235B plate using DT4 interlayer10.1016/j.msea.2017.03.118 ↗
21. Microstructure and mechanical property of titanium steel by vacuum roll-cladding with interlayer10.1080/02670836.2022.2065729 ↗
22. Interfacial microstructure and properties of a vacuum roll-cladding titanium-steel clad plate with a nickel interlayer10.1016/j.msea.2019.03.008 ↗
23. Experimental investigation of explosive welding of cp-titanium/AISI 304 stainless steel10.1016/j.matdes.2008.06.016 ↗
24. Additive manufacturing of multiple materials by selective laser melting: Ti-alloy to stainless steel via a cu-alloy interlayer
25. Direct energy deposition of functionally graded layers for the Ti–Fe compound10.1016/j.vacuum.2023.112750 ↗
26. Fabrication and characterization of a functionally graded material from Ti-6Al-4V to SS316 by laser metal deposition
27. Characterization of a functionally graded material of Ti-6Al-4V to 304L stainless steel with an intermediate V section10.1016/j.jallcom.2018.01.156 ↗
28. Development and characterization of Ti-6Al-4V to 304L stainless steel gradient components fabricated with laser deposition additive manufacturing10.1016/j.matdes.2016.05.016 ↗
29. Additive manufacturing of Inconel 718 – Ti6Al4V bimetallic structures
30. Additive fabrication of 316L/Inconel625/Ti6Al4V functionally graded materials by laser synchronous preheating10.1007/s00170-019-04061-x ↗
31. Enhanced interface strength in steel-nickel bimetallic component fabricated using wire arc additive manufacturing with interweaving deposition strategy10.1016/j.jmst.2020.04.019 ↗
32. A functionally graded material from TC4 to 316L stainless steel fabricated by double-wire + arc additive manufacturing10.1016/j.matlet.2021.130141 ↗
33. Effect of axial magnetic field on cold metal transfer arc-brazing of Ti6Al4V to 304L steel10.1016/j.jmatprotec.2019.116322 ↗
34. Effects of Ni addition on removing Fe-Ti intermetallic compounds in cold metal transfer arc-brazed TC4/304L dissimilar joints10.1016/j.jmapro.2019.01.012 ↗
35. Quantitative micro-electrochemical study of duplex stainless steel 2205 in 3.5wt% NaCl solution10.1007/s12613-021-2291-5 ↗
36. Corrosion resistance enhancement of marine alloys by rapid solidification10.1007/BF01161194 ↗
37. The role of iron content on the corrosion behavior of 90Cu-10Ni alloys in 3.5% NaCl solutions10.1108/00035591211242032 ↗
38. Lippold · 2015
39. Microstructure and mechanical properties of cold metal transfer welding-brazing of titanium alloy (TC4) to stainless steel (304L) using V-shaped groove joints10.1016/j.jmatprotec.2018.09.019 ↗
40. Study of copper dissolution and passivation processes by electrochemical impedance spectroscopy10.5006/1.3279875 ↗
41. Effect of HAc on the metastable pitting corrosion of 304 SS in NaCl solution
42. Multiscale characterization of erosion of TA2 titanium alloy welded joints
43. Characterization of corrosion behavior of TA2 titanium alloy welded joints in seawater environment
44. Corrosion product film formed on the 90/10 copper–nickel tube in natural seawater: composition/structure and formation mechanism10.1016/j.corsci.2014.11.028 ↗