journal article·2024-11

Liquid-solid composite bonding of femtosecond laser surface modified SiC ceramics and 7A52 aluminum alloy

Deku Zhang, Sihao Xiu, Kehong Wang, Qingchun Han, Lin Zhang, Xiaopeng Li

Publisher page

Abstract

This article proposes a method for achieving the connection of SiC and 7A52 aluminum alloy using femtosecond laser surface modification of SiC ceramics. The influence of laser power on the morphology, chemical composition, and wettability of the SiC ceramic surface and the liquid-solid composite bonding mechanism of SiC and 7A52 after femtosecond laser modification was investigated. After femtosecond laser modification, the ceramic structure was constructed with a periodic groove structure of appropriate size, which increased the bonding area between the solder and the ceramic surface. Additionally, thermal decomposition occurred on the SiC surface, resulting in a recasting layer, which improved the wetting effect of the solder on the ceramic surface and enhanced the diffusion of Al and Mg elements to the joint interface. The existence of periodic groove structures changes the fracture path of the joint and improves the strength of the liquid-solid composite joint, which is approximately 45.9 % higher than the original joint strength.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Advanced ceramic materials synthesis · Laser Material Processing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Progress in tribological research of SiC ceramics in unlubricated sliding-a review[J]10.1016/j.matdes.2020.108528 ↗
2. Joining of dense Si3N4 ceramics with tape cast Lu-Al-Si-O-N interlayer[J]10.1016/j.ceramint.2017.12.070 ↗
3. Wetting and joining of porous Si3N4 and dense Si3N4 ceramics with in-situ formed β-spodumene/spinel glass-ceramic interlayer[J]
4. Research on properties and applications of new lightweight aluminum alloy materials[J]10.54097/yd6e9h95 ↗
5. Synthesis of B4C and BN reinforced Al7075 hybrid composites using stir casting method[J]10.1016/j.jmrt.2020.03.043 ↗
6. Investigation on mechanical properties and wear performance of functionally graded AZ91-SiCp composites via centrifugal casting[J]10.1016/j.mtcomm.2020.101169 ↗
7. The effect of reinforced SiC on the mechanical properties of the fabricated hypoeutectic Al-Si alloy by centrifugal casting[J]10.1016/j.jestch.2019.02.009 ↗
8. Micro/nanoengineering of functionalized metal surfaces based on short/ultra-short-pulsed lasers: a review[J]
9. Experimental investigation and optimization of femtosecond laser processing parameters of silicon carbide–based on response surface methodology[J]10.1016/j.ceramint.2022.01.344 ↗
10. Metallization of ceramic substrates by laser induced decomposition of coordination complexes[J]10.1016/j.jeurceramsoc.2016.04.016 ↗
11. Conductive aluminum line formation on aluminum nitride surface by infrared nanosecond laser[J]10.1016/j.apsusc.2013.09.109 ↗
12. Femtosecond laser processing of AlN ceramics for gradient wettability control[J]10.1149/2162-8777/abd262 ↗
13. Structural transformations in femtosecond laser-processed n-type 4H-SiC[J]10.1016/j.apsusc.2016.05.041 ↗
14. High-aspect-ratio grooves fabricated in silicon by a single pass of femtosecond laser pulses[J]10.1063/1.4709726 ↗
15. Influence of surface morphology and processing parameters on polishing of silicon carbide ceramics using femtosecond laser pulses[J]10.1016/j.surfin.2022.102528 ↗
16. Laser-induced Si3N4–TiN ceramics degradation[J]10.1016/j.ceramint.2019.10.087 ↗
17. Femtosecond laser surface modification-based brazing of Si3N4 ceramics to 7A52 aluminum alloy[J]10.1007/s10853-023-09116-9 ↗
18. Direct joining of 2D carbon/carbon composites to Ti-6Al-4V alloy with a rectangular wave interface[J]10.1016/j.msea.2007.11.013 ↗
19. Wettability in metal matrix composites[J]10.3390/met11071034 ↗
20. Wenzel, Robert N. Resistance of solid surfaces to wetting by water[J]. Trans. Faraday Soc., 1936, 28(8): 988–994. Doi:https://doi.org/10.1021/ie50320a024.10.1021/ie50320a024 ↗
21. Joining of nanosecond laser irradiation modified-AlN and cu[J]10.1016/j.ceramint.2021.06.229 ↗
22. Thermodynamics and kinetics of the formation of Al2O3/MgAl2O4/MgO in Al-silica metal matrix composite[J]10.1007/s11661-007-9448-3 ↗