journal article·2024-12

Microstructures and mechanical behaviors of a directional lamellar Ti-48Al-2Cr-2Nb alloy produced by laser additive manufacturing

Xinyu Zhang, Zhenhua Ye, Chuanwei Li, Jianfeng Gu

Publisher page

Abstract

Extremely large thermal gradient is considered as a unique characteristic of additive manufacturing, which can be utilized to fabricate directionally solidified alloys. In this study, we successfully fabricated a bulk Ti-48Al-2Cr-2Nb alloy with directional solidified features by the approach of direct laser deposition. The microstructural characterizations revealed that our additively manufactured (AMed) alloy was dominantly featured by a directional α 2/γ lamellar microstructure. Moreover, there occurs an intriguing phenomenon that the orientation relationship between α 2 and γ lamellae appears a slight deviation from the well-known Blackburn relationship, which was seldom observed in previous reports. Additionally, some amounts of β o and C14-type laves phases also formed and dispersed in the lamellar microstructure. Mechanical investigations indicate that the AMed alloy achieved an improvement in yield strength at room temperature. Moreover, its yield strength can remain 630 MPa at 800 °C, comparable to the value at room temperature, and only a slight decrease occurred when the temperature was increased to 900 °C, which is superior to that of the cast one. Then, the related strengthening mechanisms were discussed based on the directional lamellar features and the particularity in orientation relationship.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys10.1002/adem.201200231 ↗
2. Pressure-induced excellent corrosion resistance of Ti-45Al-8Nb alloy
3. Phase formation and nanohardness of Ti–48Al–2Cr–2Nb-1.5C alloy by melt spinning: the effect of cooling rates10.1016/j.vacuum.2024.112985 ↗
4. Advances in gamma titanium aluminides and their manufacturing techniques10.1016/j.paerosci.2012.04.001 ↗
5. Intermetallics: why is it so difficult to introduce them in gas turbine engines?10.1016/j.intermet.2006.01.064 ↗
6. Microstructures and mechanical properties of Ti–45Al–8.5Nb–(W,B,Y) alloy by SPS–HIP route
7. Enhanced high-temperature tensile property by gradient twin structure of duplex high-Nb-containing TiAl alloy10.1016/j.actamat.2018.09.007 ↗
8. Polysynthetic twinned TiAl single crystals for high-temperature applications10.1038/nmat4677 ↗
9. An overview of direct laser deposition for additive manufacturing; part I: transport phenomena, modeling and diagnostics10.1016/j.addma.2015.07.001 ↗
10. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
11. High-strength Damascus steel by additive manufacturing10.1038/s41586-020-2409-3 ↗
12. Additive manufacturing of g-TiAl: processing, microstructure, and properties10.1002/adem.201500588 ↗
13. Laser metal deposition of the intermetallic TiAl alloy10.1007/s11661-017-4042-9 ↗
14. Effect of substrate temperature on microstructure and mechanical properties of TiAl alloy fabricated using the twin-wire plasma arc additive manufacturing system10.1007/s10853-022-07228-2 ↗
15. Microstructure characteristics and failure mechanisms of Ti-48Al-2Nb-2Cr titanium aluminide intermetallic alloy fabricated by directed energy deposition technique
16. Selective electron beam melting of Tie48Ale2Nbe2Cr: microstructure and aluminium loss10.1016/j.intermet.2014.01.004 ↗
17. Alternative-band microstructure and LPSO phase in TiAl alloy produced by direct laser deposition10.1016/j.matchar.2020.110315 ↗
18. The effects of heat treatment on the microstructure and mechanical property of laser melting deposition c-TiAl intermetallic alloys10.1016/j.matdes.2009.10.045 ↗
19. Microstructure modification of twin-wire directed energy deposition-arc fabricated γ-TiAl alloy via deposition current control10.1016/j.msea.2022.144028 ↗
20. Study of microstructure evolution and preference growth direction in a fully laminated directional micro-columnar TiAl fabricated using laser additive manufacturing technique10.1016/j.matlet.2019.01.137 ↗
21. Formation of columnar lamellar colony grain structure in a high Nb- TiAl alloy by electron beam melting
22. Blackburn · 1970
23. On the formation and stability of precipitate phases in a near lamellar γ-TiAl based alloy during creep10.1016/j.intermet.2018.04.017 ↗
24. Microstructure control of Ti-45Al-8.5Nb-(W, B, Y) alloy during the solidification process10.1016/j.actamat.2016.04.021 ↗
25. Temperature-dependent mechanical properties and fracture behavior of directionally solidified Ti47Al2Cr2Nb alloy10.1016/j.jmrt.2023.05.182 ↗
26. Elevated temperature compressive deformation behaviors of γ-TiAl-based Ti–48Al–2Cr–2Nb alloy additively manufactured by electron beam melting10.1016/j.intermet.2020.106859 ↗
27. Study of microstructure evolution and preference growth direction in a fully laminated directional micro-columnar TiAl fabricated using laser additive manufacturing technique10.1016/j.matlet.2019.01.137 ↗
28. Anisotropic tensile behavior of Ti-47Al-2Cr-2Nb alloy fabricated by direct laser deposition
29. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
30. Microstructure selection during the directionally peritectic solidification of Ti–Al binary system10.1016/j.intermet.2004.07.010 ↗
31. Stochastic modeling of columnar-to- equiaxed transition in Ti–(45–48 at%) Al alloy ingots10.1016/j.msea.2005.09.077 ↗
32. Crystal growth of TiAl alloys10.1016/S0966-9795(98)00056-9 ↗
33. Thermal process maps for predicting solidification microstructure in laser fabrication of thin-wall structures10.1016/j.jmatprotec.2006.03.155 ↗
34. Effects of processing parameters on crystal growth and microstructure formation in laser powder deposition of single-crystal superalloy10.1016/j.jmatprotec.2014.08.025 ↗
35. The Al–B–Nb–Ti system: III. Thermodynamic re-evaluation of the constituent binary system Al–Ti10.1016/j.jallcom.2007.10.061 ↗
36. Effect of stress orientation on microstructural evolution during creep of near-lamellar Ti-47Al-2Cr-2Nb10.1016/j.msea.2012.10.033 ↗
37. Phase stability of a γ-TiAl based alloy upon annealing: comparison between experiment and thermodynamic calculations10.1016/S1359-6462(03)00293-8 ↗
38. The β phase evolution in Ti-6Al-4V additively manufactured by laser metal deposition due to cyclic phase transformations10.1016/j.matlet.2017.12.140 ↗
39. High-temperature structural intermetallics10.1016/S1359-6454(99)00301-8 ↗
40. Mapping deformation mechanisms in lamellar titanium aluminide10.1016/j.actamat.2017.11.028 ↗
41. Plastic flow of γ -TiAl-based polysynthetically twinned crystals: micromechanical modeling and experimental validation10.1016/S1359-6454(98)00132-3 ↗
42. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
43. Yielding behavior of aluminum-rich single crystalline γ-TiAl10.1016/S1359-6454(03)00451-8 ↗
44. A systematic study of interatomic potentials for mechanical behaviours of Ti-Al alloys
45. Phase transformation mechanisms involved in two-phase TiAl-based alloys–I. Lamellar structure formation10.1016/1359-6454(95)00167-4 ↗
46. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
47. Interfacial ledge structures in Ni3Al-Ni3Cb eutectic composites10.1007/BF02818645 ↗
48. Dislocation wall and cell structures and long-range internal stresses in deformed metal crystals10.1016/0001-6160(83)90007-X ↗
49. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗