A novel process for improving fatigue properties of TIG welded AZ31B mg alloy joints by laser bionic treatment
Source abstract
Abstract
It is crucial to obtain better fatigue life for the safe application of materials, and nature provides a new idea for effectively improving fatigue property. A ‘soft-hard’ alternating structure imitated biological morphology was fabricated on the surface of welded joints by laser bionic treatment (LBT) for improving the fatigue property of TIG welded AZ31B Mg alloy joints. After LBT, the grains in the weld zone were refined with the average grain size about 5.55 μm and decreased by 76.1%, resulting in an increase of hardness of 12.0% to about 60.12 HV0.1, and formed a ‘soft-hard’ structure on the surface of welded joints. By adjusting the distribution angle of laser bionic stripe, the high cycle fatigue strength of welded joints was increased by 129.4% at most. The fracture morphology of welded joints was changed by LBT. The weld zone of bionic welded joints was deformed by twinning and slip, while the laser-treated zone was only deformed by slip. The mechanisms of strengthening fatigue properties were discussed based on the microstructure and structural characteristics from EBSD analyze.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Influence of grain size and grain boundary misorientation on the fatigue crack initiation mechanisms of textured AZ31 Mg alloy
2. The high cycle fatigue property of mg-Gd-Y-Zn-Mn alloy enhanced by LPSO phase10.1016/j.matlet.2021.130367 ↗
3. Fatigue of welded magnesium alloy joints10.2320/matertrans.45.419 ↗
4. Effect of the rotation rate on the low-cycle fatigue behavior of friction-stir welded AZ31 magnesium alloy10.1016/j.engfracmech.2020.106925 ↗
5. Crack initiation mechanism of extruded AZ31 magnesium alloy in the very high cycle fatigue regime10.1016/j.msea.2008.02.003 ↗
6. Enhanced very high cycle fatigue performance of extruded mg–12Gd–3Y–0.5Zr magnesium alloy10.1016/j.msea.2010.12.092 ↗
7. Fatigue behaviour of friction stir processed AZ91 magnesium alloy produced by high pressure die casting10.1016/j.matchar.2006.04.025 ↗
8. Fatigue and tensile behavior of cast, hot-rolled, and severely plastically deformed AZ31 magnesium alloy10.1007/s11661-007-9109-6 ↗
9. Fatigue performance of pulsed current gas tungsten arc, friction stir and laser beam welded AZ31B magnesium alloy joints10.1016/j.matdes.2010.03.013 ↗
10. Fatigue crack growth behaviour of pulsed current gas tungsten arc, friction stir and laser beam welded AZ31B magnesium alloy joints10.1016/j.jmatprotec.2011.02.003 ↗
11. Effects of microstructural inhomogeneities and micro-defects on tensile and very high cycle fatigue behaviors of the friction stir welded ZK60 magnesium alloy joint10.1016/j.ijfatigue.2019.01.016 ↗
12. Effect of texture and banded structure on the crack initiation mechanism of a friction stir welded magnesium alloy joint in very high cycle fatigue regime10.1016/j.ijfatigue.2020.105617 ↗
13. Tensile property of a hot work tool steel prepared by biomimetic coupled laser remelting process with different laser input energies10.1016/j.apsusc.2012.05.082 ↗
14. Tensile property of H13 die steel with convex-shaped biomimetic surface10.1016/j.apsusc.2007.05.008 ↗
15. Effect of laser surface melting on high temperature tensile properties of AZ91D magnesium alloy10.1016/j.jallcom.2017.03.354 ↗
16. Effect of strain rate and temperature on fracture and microstructure evolution of AZ91D magnesium alloy processed by laser surface melting10.1007/s11661-018-4792-z ↗
17. Effect of laser bionic treatment on the microstructure and mechanical properties of TIG welded AZ31B magnesium alloy joints10.1016/j.msea.2022.142864 ↗
18. The role of twinning–detwinning on fatigue fracture morphology of mg–3%Al–1%Zn alloy10.1016/j.msea.2008.04.056 ↗
19. Deformation behavior and microstructure characteristics of the laser-welded Ti-6Al-4V joint under variable amplitude fatigue10.1016/j.matchar.2022.112606 ↗
20. An experimental analysis of fatigue behavior of AZ31B magnesium alloy welded joint based on infrared thermography10.1016/j.matdes.2013.10.036 ↗
21. Basal slip dominant fatigue damage behavior in a cast mg-8Gd-3Y-Zr alloy10.1016/j.ijfatigue.2018.08.001 ↗
22. Role of twinning and texture on fatigue resistance enhancement of Mg-6Gd-3Y-1Nd-0.5Zr alloys10.1016/j.ijfatigue.2021.106471 ↗
23. Transition of dominant deformation mode in bulk polycrystalline pure mg by ultra-grain refinement down to sub-micrometer10.1016/j.actamat.2020.07.055 ↗
24. Achieving gradient heterogeneous structure in mg alloy for excellent strength-ductility synergy
25. The role of deformation twinning in the fracture behavior and mechanism of basal textured magnesium alloys10.1016/j.msea.2014.02.010 ↗
26. The effect of laser shock peening, shot peening and their combination on the microstructure and fatigue properties of Ti-6Al-4V titanium alloy10.1016/j.ijfatigue.2021.106465 ↗
27. Study of the interaction of a short fatigue crack with grain boundaries in a cast Al alloy using X-ray microtomography, Acta
28. Cyclic deformation and fatigue damage in single-crystal magnesium under fully reversed strain-controlled tension-compression in the {101¯0} direction10.1016/j.scriptamat.2014.10.020 ↗
29. Towards revealing the relationship between deformation twin and fatigue crack initiation in a rolled magnesium alloy10.1016/j.matchar.2021.111362 ↗
30. Role of misorientation in fatigue crack growth behavior for NG-TIG welded joint of Ni-based alloy10.1016/j.msea.2017.10.090 ↗
31. Ultrasonic-vibration-enhanced plasticity of an entropic alloy at room temperature10.1016/j.actamat.2021.117569 ↗
32. Materials science perspective of metal fatigue resistance10.1179/mst.1993.9.6.453 ↗