Investigation of microstructure, corrosion and mechanical properties of iron and holmium modified Sn-3.0Ag0.5Cu solder alloy with ultrasonic treatment
Source abstract
Abstract
This research investigated the microstructure, corrosion behavior and mechanical properties of iron and holmium modified Sn-3.0Ag-0.5Cu solder alloy with ultrasonic treatment. The results demonstrated that the distribution of the phases in the ultrasonically treated solder alloys became homogeneous and the microstructure of ultrasonically treated solder alloys were more refined. The average grain size of ultrasonically treated solder alloys was reduced from 206.7 μm to 184.1 μm. A significant increase in the tensile strength from 38.75 MPa to 47.38 MPa was found in the ultrasonically treated solder alloys. The polarization curves results indicated that the solder alloys treated with ultrasound possessed lower corrosion current density and the results of atomic force microscopy suggested that roughness of corrosion products morphology was reduced. Furthermore, the electrochemical impedance spectroscopy (EIS) results indicated that the ultrasonically treated solder alloys had larger diameter of the semicircular loops and higher total impedance values.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Metallurgy and Material Forming · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. A critical review on performance, microstructure and corrosion resistance of Pb-free solders [J]10.1016/j.measurement.2018.12.051 ↗
2. Influence of CrFeCoNiCu high-entropy alloy and ultrasonic stirring on the thermal, electrochemical and mechanical properties of Zn-30Sn high-temperature solder alloy[J]10.1016/j.matchar.2023.112977 ↗
3. Effects of Ni modified MWCNTs on the microstructural evolution and shear strength of Sn-3.0 ag-0.5 cu composite solder joints[J]10.1016/j.matchar.2020.110287 ↗
4. Influence of bi on microstructures evolution and mechanical properties in Sn–ag–cu lead-free solder[J]10.1016/j.jallcom.2003.12.005 ↗
5. Influences of mono-Ni (P) and dual-cu/Ni (P) plating on the interfacial microstructure evolution of solder joints[J]10.1007/s11661-018-4983-7 ↗
6. Microstructures and properties of Sn-bi-in low-temperature Lead-free solders[J]
7. Characterization of low-melting-point Sn-bi-in lead-free solders[J]10.1007/s11664-016-4366-z ↗
8. Elastic modulus and coefficient of thermal expansion of 91.84Sn-3.33Ag-4.83Bi Pb-free solder[J]10.1007/s11664-022-10159-y ↗
9. Effects on undercooling and interfacial reactions with cu substrates of adding bi and in to Sn-3Ag solder[J]10.1007/s11664-010-1347-5 ↗
10. Evolution of interfacial structures and mechanical performance of sapphire and Sn–9Zn–2Al joints by ultrasound[J]10.1111/ijac.13324 ↗
11. Microstructure and interfacial reaction of Sn–Zn–x(Al, ag) near-eutectic solders on Al and cu substrates[J]10.1007/s10854-014-1877-3 ↗
12. Electrodeposition and characterisation of Sn–Ag–Cu solder alloys for flip-chip interconnection[J]10.1016/j.electacta.2010.08.102 ↗
13. Effect of additions of ZrO2 nano-particles on the microstructure and shear strength of Sn–Ag–Cu solder on Au/Ni metallized Cu pads[J]10.1016/j.microrel.2011.03.042 ↗
14. A review: on the development of low melting temperature Pb-free solders[J]10.1016/j.microrel.2014.02.025 ↗
15. Electronics without lead[J]10.1126/science.1110168 ↗
16. Effect of 0.5 wt% cu in Sn− 3.5% ag solder on the interfacial reaction with Au/Ni metallization[J]10.1021/cm034692c ↗
17. Influence of Fe and Ho additions on Sn-3.0 Ag-0.5 Cu solder alloy: microstructure, electrochemical and mechanical properties[J]10.1016/j.matchar.2023.113307 ↗
18. Structure and properties of lead-free solders bearing micro and nano particles[J]10.1016/j.mser.2014.06.001 ↗
19. Corrosion characterization of tin–lead and lead free solders in 3.5 wt.% NaCl solution[J]10.1016/j.corsci.2007.11.025 ↗
20. Microstructure, mechanical properties, and interfacial reaction with Cu substrate of Zr-modified SAC305 solder alloy[J]10.1016/j.jallcom.2018.12.098 ↗
21. Effects of cobalt on the nucleation and grain refinement of Sn-3Ag-0.5Cu solders[J]10.1016/j.jallcom.2016.04.265 ↗
22. Heterogeneous nucleation of βSn on NiSn4, PdSn4 and PtSn4[J]10.1016/j.actamat.2014.02.044 ↗
23. Revisiting mechanisms to inhibit Ag3Sn plates in Sn–Ag–Cu solders with 1 wt.% Zn addition[J]10.1016/j.jallcom.2010.03.191 ↗
24. High stability and aging resistance Sn-1Ag-0.5 Cu solder alloy by Fe and Bi minor alloying[J]10.1016/j.mee.2019.01.011 ↗
25. Effect of ag content and the minor alloying element Fe on the mechanical properties and microstructural stability of Sn-Ag-Cu solder alloy under high-temperature annealing[J]10.1007/s11664-012-2343-8 ↗
26. Fe addition to Sn-3.5 Ag solder for the suppression of Kirkendall void formation[J]10.1016/j.scriptamat.2013.04.010 ↗
27. Influence of Ce addition on Sn-3.0 Ag-0.5 Cu solder joints: thermal behavior, microstructure and mechanical properties[J]10.1016/j.jallcom.2016.12.191 ↗
28. Effect of Nd addition on the corrosion behavior of SAC305 solder alloy[J]10.1016/j.corsci.2023.111264 ↗
29. Effects of Ho content on microstructures and mechanical properties of Mg-Ho-Zn alloys[J]10.1016/j.matchar.2019.01.023 ↗
30. Effects of holmium additions on microstructure and properties of A356 aluminum alloys[J]10.3390/met8100849 ↗
31. Sonocrystallization: the use of ultrasound for improved industrial crystallization10.1021/op050109x ↗
32. Effect of high-intensity ultrasonic on the microstructure and grain refinement of Al-5Ti-1B master alloy
33. Effects of ultrasonic stirring on microstructures of Al-7wt% Si alloy ingot10.1088/1742-6596/1074/1/012026 ↗
34. Effect of ultrasonic treatment during solidification on corrosion behavior of Mg-3Al-1Zn and Mg-4Zn magnesium alloys10.1149/1945-7111/abcde5 ↗
35. Microstructure and mechanical properties of AZ91 alloy produced with ultrasonic vibration10.1016/j.msea.2007.09.071 ↗
36. Electrochemical behavior of a new solder material (Sn–In–Ag)[J]10.1016/S0167-577X(03)00326-4 ↗
37. Potentiodynamic polarization measurement of Sn-8.5Zn-XAl-0.5Ga alloy in 3.5% NaCl solution10.1149/1.2209569 ↗
38. Comparison of corrosion behaviour of zinc in NaCl and in NaOH solutions. Part I: Corrosion layer characterization10.1016/j.corsci.2010.08.003 ↗
39. Validation of corrosion rates measured by the Tafel extrapolation method[J]10.1016/j.corsci.2005.05.046 ↗
40. Corrosion resistance of Pb-free and novel nano-composite solders in electronic packaging[J]
41. Effect of nanocrystalline grain size on the electrochemical and corrosion behavior of nickel[J]10.1016/j.corsci.2004.04.007 ↗
42. Electrochemical corrosion behaviour of Sn-Zn-xBi alloys used for miniature detonating cords [J]10.1016/j.jmst.2019.03.026 ↗
43. The influence of the marine aerobic Pseudomonas strain on the corrosion of 70/30 cu-Ni alloy10.1016/j.corsci.2007.04.009 ↗
44. Electrochemical corrosion behaviour of Pb-free SAC 105 and SAC 305 solder alloys: a comparative study[J]10.17576/jsm-2017-4602-14 ↗
45. Corrosion characterization of new tin–silver binary alloys in nitric acid solutions [J]10.1016/j.corsci.2008.02.003 ↗
46. Microstructure, mechanical, and thermal properties of the Sn–1Ag–0.5 Cu solder alloy bearing Fe for electronics applications[J]10.1016/j.msea.2012.04.115 ↗