journal article·2025-02

Effect mechanism of diamagnetism element Cu in-situ alloying on the microstructure and magnetic properties of SLM-formed NiFeMo alloy

Falin Xiong, Jiaoxi Yang, Donghai Guo, Wenfu Liu, Zihan Fu, Feng Yang, Ran Li, Qi Liu, Huaixue Li

Publisher page

Abstract

NiFeMo alloy formed using additive manufacturing techniques with high saturation magnetic induction ( B S) and low coercivity ( H C) are crucial in aerospace applications. In this study, we successfully formed Cu-modified (NiFeMo) 100-xCu x alloys via in-situ alloying selective laser melting (SLM). The effect of in-situ alloying Cu content on the microstructure and magnetic properties of SLM-formed NiFeMo has been investigated, and efforts have been devoted to developing new technologies for modulating the properties of SLM-formed magnetic materials. The microstructure and magnetic properties of the alloy samples were analyzed using scanning electron microscopy (SEM), X-ray diffraction (XRD), electron backscattering diffraction (EBSD), DC B H hysteresis loop tester (MATS-2010S), and transmission electron microscopy (Titan-G2). The results demonstrate that (NiFeMo) 100-xCu x alloys possess an FCC γ-(Ni, Fe) solid solution structure within the range of added Cu content in this study. In the central region of the melt pool, columnar crystals grow in the direction of the temperature gradient, and the average grain size ( D) decreases gradually with increasing Cu content from in-situ alloying. Cu atoms induced changes in the crystal structure by displacing atoms in the γ-(Ni, Fe) solid solution, resulting in lattice distortion. The (NiFeMo) 98Cu 2 alloy exhibited an average crystal plane spacing d of about 0.2261 nm along the (1 1 ¯ 1 ¯ ) γ-(Ni, Fe) direction and a lattice distortion ∆ε of about 1.09 %. The saturation magnetic induction varied with increasing Cu additions, exceeding 0.7 T for NiFeMo alloy with Cu additions of 0.8 wt%, 1.1 wt%, and 1.4 wt%. The coercivity generally decreased with increasing Cu content, attaining values below 17 A/m when Cu (x = 0.5 wt%, 0.8 wt%) was added to the NiFeMo alloy. Therefore, controlling the in-situ alloying Cu content within the range of 0.8–1.4 wt% is beneficial for enhancing the soft magnetic performance of the SLM-formed NiFeMo alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Entropy Alloys Studies · Microstructure and Mechanical Properties of Steels · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Magnetic properties of Fe–Ni permalloy produced by selective laser melting10.1016/j.jallcom.2019.152315 ↗
2. Recent advances and future directions in magnetic materials10.1016/j.actamat.2003.08.011 ↗
3. Magnetic properties of in-situ synthesized FeNi3 by selective laser melting Fe-80%Ni powders10.1016/j.jmmm.2013.02.014 ↗
4. Studies of magnetic properties of permalloy (Fe–30%Ni) prepared by SLM technology10.1016/j.jmmm.2011.08.030 ↗
5. Magnetic and structural properties of high relative cooling power (Fe70Ni30)92Mn8 magnetocaloric nanoparticles10.1088/0022-3727/48/30/305003 ↗
6. Magnetocaloric properties of Fe-Ni-Cr nanoparticles for active cooling10.1038/srep35156 ↗
7. Gradient microstructure, mechanical properties and phase composition of Ni-Cr-Fe alloy under additive manufacturing process
8. Magnetism in NiFeMo disordered alloys: experiment and theory10.1016/j.physb.2010.07.028 ↗
9. Impact of particles surface smoothing on DC permeability of NiFeMo soft magnetic powder compacts10.1016/j.jmmm.2021.168298 ↗
10. The influence of mechanical milling on structure and soft magnetic properties of NiFe and NiFeMo alloys10.1016/j.jmmm.2007.03.111 ↗
11. Magnetic properties of high permeability NiFeMo/cu composite wires10.1016/j.jallcom.2006.01.126 ↗
12. Additive manufacturing of soft magnets for electrical machines—a review
13. Controlling the grain orientation during laser powder bed fusion to tailor the magnetic characteristics in a Ni-Fe based soft magnet10.1016/j.actamat.2018.07.064 ↗
14. Additively manufactured Ni-15Fe-5Mo Permalloy via selective laser melting and subsequent annealing for magnetic-shielding structures: process, micro-structural and soft-magnetic characteristics10.1016/j.jmmm.2019.165754 ↗
15. Additive manufacturing of soft magnetic permalloy from Fe and Ni powders: control of magnetic anisotropy10.1016/j.jmmm.2018.11.084 ↗
16. Selective laser melting of permalloy magnetic core with complex geometry10.1016/j.jmmm.2023.170962 ↗
17. In situ alloying of a modified Inconel 625 via laser powder bed fusion: microstructure and mechanical properties10.3390/met11060988 ↗
18. Additive manufacturing of beta-NiAl by means of laser metal deposition of pre-alloyed and elemental powders10.3390/ma14092246 ↗
19. Emerging metallic systems for additive manufacturing: in-situ alloying and multi-metal processing in laser powder bed fusion10.1016/j.pmatsci.2021.100795 ↗
20. Additive manufacturing of functionally graded Co–Fe and Ni–Fe magnetic materials10.1016/j.jallcom.2020.153817 ↗
21. Effect of Si element and TiB2 nucleating agent on microstructure and magnetic properties of Cu-based immiscible composites by laser melting deposition10.1016/j.jallcom.2022.167938 ↗
22. Microstructure of a modulated Ti-6Al-4V – Cu alloy fabricated via in situ alloying in laser powder bed fusion10.1016/j.mtla.2023.101731 ↗
23. Magnetic shielding promotion via the control of magnetic anisotropy and thermal post processing in laser powder bed fusion processed NiFeMo-based soft magnet
24. Laser additive processing of Ni-Fe-V and Ni-Fe-Mo Permalloys: microstructure and magnetic properties10.1016/j.matlet.2017.01.059 ↗
25. Microstructure-magnetic shielding development in additively manufactured Ni-Fe-Mo soft magnet alloy in the as fabricated and post-processed conditions10.1016/j.jallcom.2021.161112 ↗
26. The effect of heat treatment on structure and magnetic properties of additively manufactured Fe-Co-V alloys
27. Ultra-fine microstructure and exceptional low coercivity developed in a high-Bs Fe-Si-B-P alloy by co-alloying Ni, Mo, and Cu10.1016/j.scriptamat.2023.115666 ↗
28. Effect of Co, Cu, and Mo alloying metals on electrochemical and magnetic properties of Fe-B alloy10.1016/j.jallcom.2023.169652 ↗
29. Soft magnetic Fe-Si-B-Cu nanocrystalline alloys with high Cu concentrations10.1016/j.jallcom.2017.06.128 ↗
30. The role of Cu content on structure and magnetic properties of Fe–Si–B–P–Cu nanocrystalline alloys10.1007/s10853-018-3131-5 ↗
31. Recurring effects of Cu addition on magnetic properties in Fe-based bulk metallic glasses10.1016/j.jnoncrysol.2015.04.041 ↗
32. Effects of metallurgical defects on magnetic properties of SLM NiFeMo permalloy10.1016/j.matchar.2023.112672 ↗
33. Magnetostrictive improvement in Er-doped biodegradable Fe81Ga19 alloys manufactured by selective laser melting10.1016/j.jmrt.2023.05.114 ↗
34. Laser powder bed fusion of ultrahigh strength Fe-Cu alloys using elemental powders
35. Additive manufacturing of rare earth permanent magnetic materials: research status and prospects10.3390/met14040446 ↗
36. Magnetic spin exchange interaction in SmCo5/Co nanocomposite magnet for large energy product10.1016/j.jcis.2020.12.085 ↗
37. Unveiling heterogeneous microstructure and good combinations of high yield strength and low coercivity of in-situ formed NbC/FeNiCo medium-entropy composites10.1016/j.powtec.2023.118365 ↗
38. Architecture and magnetism of alnico10.1016/j.actamat.2014.04.044 ↗
39. Crystallographic-orientation-dependent magnetic properties of Fe–Ni permalloy in-situ alloyed using additive manufacturing10.1016/j.jmatprotec.2022.117733 ↗
40. Effect of post-sinter annealing on structure and coercivity of (Zr, Ti)-doped Nd-Ce-Fe-B magnets10.1016/j.jallcom.2024.174479 ↗
41. High-temperature strength-coercivity balance in a FeCo-based soft magnetic alloy via magnetic nanoprecipitates10.1016/j.jmst.2020.11.057 ↗
42. Influence of Co on microstructure and coercivity of (Ni0.5Fe0.5)80B10Si2Cu1Zr7 alloy10.1016/j.jnoncrysol.2021.120677 ↗
43. Magnetic properties enhancement of multi-element-doped SmCo7 nanocrystalline alloys
44. Microstructure evolution and soft magnetic properties of Cu–10Fe alloys10.1007/s10853-023-09054-6 ↗