journal article·2024-10

Comparative study of intergranular acicular nano-precipitate evolution and their effects on creep failure behavior for BM and HAZ in a novel Fe-Ni-based alloy joint

Yaqi Wang, Xia Liu, Chendong Shao, Yuan Gao, Manjie Fan, Xin Huo, Fenggui Lu

Publisher page

Abstract

Intergranular acicular nano-precipitate evolution and their effects on creep failure behavior for the base metal (BM) and heat affected zone (HAZ) in a novel cost-effective Fe-Ni-based alloy joint were investigated comparatively. It was found that the BM tended to initiate acicular nano-precipitates perpendicular to grain boundaries, while their formation was suppressed at the HAZ. After creep at 650 °C under 300 MPa, nano-precipitates composed of γ´-Ni 3(Al, Ti), M 23C 6 and σ phase at BM would expand along the grain boundaries (GBs) with significant GB migration. Creep cavities were more prone to initiate at the precipitate-free zone and the acicular nano-precipitate roots due to the precipitation strengthening reduction and local strength mismatch. Furthermore, grain boundary embrittlement induced by acicular precipitates and the presence of recrystallized grains at the crack tip also promoted the crack propagation. In contrast, the welding thermal cycle contributed to the M 23C 6 redistribution at the GBs, which decreased element diffusion rate and dragging grain boundary movement, thereby exhibiting better creep crack resistance at the HAZ. The finding provided profound implications for the comprehensive understanding of acicular nano-precipitate evolution in the newly designed Fe-Ni-based alloy joint under service condition.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Solute-dislocation interactions and creep-enhanced cu precipitation in a novel ferritic-martensitic steel10.1016/j.actamat.2020.05.054 ↗
2. Research and development of heat-resistant materials for advanced USC power plants with steam temperatures of 700°C and above10.15302/J-ENG-2015031 ↗
3. A physically-based constitutive model for a novel heat resistant martensitic steel under different cyclic loading modes: microstructural strengthening mechanisms10.1016/j.ijplas.2023.103611 ↗
4. Microstructural evolution and its influence on the impact toughness of GH984G alloy during long-term thermal exposure10.1016/j.jmst.2020.06.005 ↗
5. Deformation behavior, microstructure evolution, and rupture mechanism of the novel G115 steel welded joint during creep10.1016/j.matchar.2023.113275 ↗
6. Characterization on the gradient microstructure near the fusion interface of dissimilar metal between high Cr heat-resistant steel and Ni-based alloy 61710.1016/j.matchar.2019.03.001 ↗
7. Evolution of grain structure, γ´ precipitate and hardness in friction welding and post weld heat treatment of a new Ni-Fe based superalloy10.1016/j.msea.2020.139596 ↗
8. Creep rupture of a Ni-Fe based model alloy under simulated fireside corrosion in coal-fired boilers10.1016/j.corsci.2023.111536 ↗
9. Phenomenological and microstructural analysis of intermediate temperatures creep in a Ni–Fe-based alloy for advanced ultra-supercritical fossil power plants10.1016/j.actamat.2015.09.006 ↗
10. Evaluation of Ni-Fe base alloys as inert anode for low-temperature aluminium electrolysis10.1016/j.jmst.2021.08.028 ↗
11. Microstructural evolution of a new Ni-Fe-based superalloy deformed by creep10.1016/j.matchar.2023.112917 ↗
12. Interplay between high-temperature creep deformation behavior and nanoscale precipitate evolution in a newly designed Fe–Ni-based superalloy10.1016/j.msea.2024.146234 ↗
13. Effect of long-term aging on microstructural stability and tensile deformation of a Fe–Ni-based superalloy10.1016/j.msea.2022.143298 ↗
14. Microstructure optimization for higher strength of a new Fe–Ni-based superalloy10.1016/j.msea.2023.144632 ↗
15. The microstructure and mechanical performance optimization of a new Fe-Ni-based superalloy for Gen IV nuclear reactor: the critical role of Nb alloying strategy10.1016/j.matchar.2023.113240 ↗
16. Creep deformation behavior of the Ni–Fe-based GH984G alloy10.1016/j.msea.2022.143819 ↗
17. Creep rupture strength for weld joint of 23Cr-45Ni-7W alloy10.2320/matertrans.M2016242 ↗
18. Effect of Cr and Ni/Fe ratio on the microstructure and mechanical properties of γ’-strengthened Ni–Fe-based alloys10.1007/s11661-022-06932-7 ↗
19. Strain mapping near a triple junction in strained Ni-based alloy using EBSD and biaxial nanogauges10.1016/j.actamat.2011.01.051 ↗
20. Effect of solidified grain boundary on interfacial creep failure behavior for steel/nickel dissimilar metal welded joint10.1016/j.msea.2020.140482 ↗
21. High-temperature creep property deterioration of the alumina-forming austenitic steel: effect of σ phase10.1016/j.msea.2022.143126 ↗
22. Strengthening mechanisms and creep rupture behavior of advanced austenitic heat resistant steel SA-213 S31035 for A-USC power plants10.1016/j.msea.2020.138991 ↗
23. Deformation mechanism of Mg-Gd-Y-Zr alloy during hot ring rolling10.1016/j.matchar.2021.111154 ↗
24. Precipitation behavior of γ’ precipitates in 21Cr-32Fe-41Ni heat-resistant alloy at different aging temperatures10.1016/j.jallcom.2023.170405 ↗
25. Local characterization of the diffusion process during discontinuous precipitation: a review10.1515/ijmr-2001-0125 ↗
26. Early stages of discontinuous precipitation reaction in an advanced Cr-Fe-Ni alloy isothermally aged at 800°C10.1016/j.matchar.2021.111628 ↗
27. On the morphology of grain boundary discontinuous reactions and phase identification in an advanced Cr–Fe–Ni alloy10.1007/s10853-020-04690-8 ↗
28. Microstructural assessment of 310S stainless steel during creep at 800 C
29. Grain boundary discontinuous precipitation reactions10.1179/imr.1981.26.1.153 ↗
30. Investigation of dissolution and precipitation behaviours of precipitates in welded joints of high Cr ferritic heat resistant steels10.1007/BF03263417 ↗
31. Control of discontinuous and continuous precipitation of γ’-strengthened high-entropy alloys through nanoscale Nb segregation and partitioning10.1016/j.jallcom.2020.154903 ↗
32. The structure and energy of grain boundaries10.1016/B978-008044164-1/50008-6 ↗
33. Development of grain boundary precipitate-free zones in a Ni-Mo-Cr-W alloy10.1007/s11661-017-4019-8 ↗
34. High temperature creep properties of a linear friction welded newly developed wrought Ni-based superalloy10.1016/j.msea.2017.10.091 ↗
35. Microstructural evolution during high temperature dwell-fatigue of austenitic stainless steels10.1016/j.ijfatigue.2020.105990 ↗