journal article·2024-12

Ordering-facilitated lower hydrogen embrittlement sensitivity in a prototype high-entropy alloy

Pengfei Wu, Wei Zhang, Yonggang Tong, Yongle Hu, Weiying Huang, Kefu Gan

Publisher page

Abstract

The ageing treatment (450 °C/60 h) led to the spinodal decomposition at grain boundaries (GBs) and the development of chemical short-range orders (CSROs) in the alloy matrix, increasing the strength and effectively reducing the hydrogen embrittlement (HE) sensitivity of the equiatomic FeMnNiCoCr alloy. Firstly, the emergence of NiMn- and Cr-rich orders at GB regions reduces hydrogen diffusion rates along GBs and limits hydrogen enrichment at these sites. Secondly, CSROs promote hydrogen accumulation within the grain interior and impede hydrogen penetration, resulting in a shallower hydrogen-affected depth in the aged sample. Moreover, the modulation of hydrogen distribution by microstructure initiates transgranular cracking in the aged sample.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Additive Manufacturing Materials and Processes · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Hydrogen embrittlement phenomena and mechanisms
2. Hydrogen influence on some advanced high-strength steels10.1016/j.corsci.2017.06.012 ↗
3. High-entropy alloys10.1038/s41578-019-0121-4 ↗
4. High-entropy ceramics: review of principles, production and applications10.1016/j.mser.2021.100644 ↗
5. Microstructures and properties of high-entropy alloys10.1016/j.pmatsci.2013.10.001 ↗
6. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off10.1038/nature17981 ↗
7. Interstitial atoms enable joint twinning and transformation induced plasticity in strong and ductile high-entropy alloys
8. A precipitation-hardened high-entropy alloy with outstanding tensile properties10.1016/j.actamat.2015.08.076 ↗
9. Multicomponent intermetallic nanoparticles and superb mechanical behaviors of complex alloys10.1126/science.aas8815 ↗
10. A mechanically strong and ductile soft magnet with extremely low coercivity10.1038/s41586-022-04935-3 ↗
11. A non-equiatomic FeNiCoCr high-entropy alloy with excellent anti-corrosion performance and strength-ductility synergy10.1016/j.corsci.2021.109341 ↗
12. Origins of strengthening and toughening effects in twinned nanocrystalline alloys of low stacking fault energy with heterogeneous grain structure10.1016/j.jmps.2023.105305 ↗
13. A strong ferritic high-resistivity multicomponent alloy with tunable ordered coherent multicomponent nanoprecipitates10.1016/j.actamat.2022.118209 ↗
14. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
15. Hydrogen embrittlement in compositionally complex FeNiCoCrMn FCC solid solution alloy10.1016/j.cossms.2017.11.002 ↗
16. Effects of interstitial C and N on hydrogen embrittlement behavior of non-equiatomic metastable FeMnCoCr high-entropy alloys10.1016/j.corsci.2021.109933 ↗
17. Defeating hydrogen-induced grain-boundary embrittlement via triggering unusual interfacial segregation in FeCrCoNi-type high-entropy alloys10.1016/j.actamat.2022.118410 ↗
18. First-principles study of hydrogen-induced embrittlement in Fe grain boundary with Cr segregation10.2355/isijinternational.55.1131 ↗
19. First-principles investigation into the effect of Cr on the segregation of multi-H at the Fe Σ3 (111) grain boundary10.1016/j.jnucmat.2013.06.015 ↗
20. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
21. A nano-sized NbC precipitation strengthened FeCoCrNi high entropy alloy with superior hydrogen embrittlement resistance10.1016/j.corsci.2022.110636 ↗
22. Effect of V/Mo ratio on the evolution of carbide precipitates and hydrogen embrittlement of tempered martensitic steel10.1016/j.corsci.2020.108929 ↗
23. Dual role of nanosized NbC precipitates in hydrogen embrittlement susceptibility of lath martensitic steel10.1016/j.corsci.2019.108345 ↗
24. Segregation-driven grain boundary spinodal decomposition as a pathway for phase nucleation in a high-entropy alloy10.1016/j.actamat.2019.07.052 ↗
25. Decomposition of the single-phase high-entropy alloy CrMnFeCoNi after prolonged anneals at intermediate temperatures10.1016/j.actamat.2016.04.005 ↗
26. Grain boundary decohesion by nanoclustering Ni and Cr separately in CrMnFeCoNi high-entropy alloys10.1126/sciadv.aay0639 ↗
27. High strength and high ductility of a severely deformed high-entropy alloy in the presence of hydrogen10.1016/j.corsci.2023.111097 ↗
28. Gradient-structured high-entropy alloy with improved combination of strength and hydrogen embrittlement resistance10.1016/j.corsci.2022.110253 ↗
29. Microstructure and defect effects on strength and hydrogen embrittlement of high-entropy alloy CrMnFeCoNi processed by high-pressure torsion10.1016/j.msea.2022.143179 ↗
30. Beating hydrogen with its own weapon: Nano-twin gradients enhance embrittlement resistance of a high-entropy alloy10.1016/j.mattod.2018.07.015 ↗
31. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5 Al–0.6 C TWIP steel10.2355/isijinternational.49.1952 ↗
32. Hydrogen embrittlement of twinning-induced plasticity steels: contribution of segregation to twin boundaries10.1016/j.scriptamat.2022.115187 ↗
33. Diffusion of hydrogen in FCC alloys of nickel with iron10.1016/0001-6160(67)90135-6 ↗
34. The role of precipitation in hydrogen diffusivity and mechanical properties of a high entropy alloy10.1016/j.ijhydene.2023.07.046 ↗
35. The influence of L12 ordered precipitates on hydrogen embrittlement behavior in CoCrNi-based medium entropy alloys10.1016/j.actamat.2023.119328 ↗
36. Effects of alloy composition and strain hardening on tensile fracture of hydrogen-precharged type 316 stainless steels10.1016/j.ijhydene.2007.10.046 ↗
37. A decohesion pathway for hydrogen embrittlement in nickel: mechanism and quantitative prediction10.1016/j.actamat.2019.11.062 ↗
38. Hydrogen embrittlement of an interstitial equimolar high-entropy alloy10.1016/j.corsci.2018.03.040 ↗