journal article·2025-06

Thermal stability of microstructure and mechanical properties of high‑chromium ferritic-martensitic steel at 450 and 540 °C

Nadezhda Polekhina, Valeria Osipova, Kseniya Spiridonova, Igor Litovchenko, Sergey Akkuzin, Evgeny Moskvichev, Vyacheslav Chernov, Maria Leontyeva-Smirnova

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Zinkle, structural alloys for nuclear energy applications
2. Yan · 2015
3. Microstructure stability of V and Ta microalloyed 12%Cr reduced activation ferrite/martensite steel during long-term aging at 650 °C10.1016/j.jmst.2013.04.028 ↗
4. Effect of thermal ageing on microstructure, tensile and impact properties of reduced activated ferritic-martensitic steel10.1016/j.msea.2017.01.030 ↗
5. Microstructure-based prediction of thermal aging strength reduction factors for grade 91 ferritic-martensitic steel10.1016/j.msea.2020.140116 ↗
6. The microstructure and mechanical properties of ferritic-martensitic steel EP-823 after high-temperature thermomechanical treatment10.3390/met12010079 ↗
7. Special features of the surface layer structure of ferritic-martensitic EP-823-Sh steel after prolonged exposure to the flowing lead at 630 °C under low oxygen concentration10.1016/j.jnucmat.2022.154039 ↗
8. Thermal stability of the microstructure of 12% chromium ferritic–martensitic steels after long-term aging at high temperatures10.1134/S1063784216020092 ↗
9. Influence of dynamic strain aging on ferritic/martensitic steel and stability analysis10.1016/j.fusengdes.2021.112581 ↗
10. Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants10.1088/1468-6996/9/1/013002 ↗
11. Static recovery of tempered lath martensite microstructures during long-term aging in 9–12% Cr heat resistant steels10.1016/j.matlet.2009.08.024 ↗
12. On the contribution of carbides and micrograin boundaries to the creep strength of tempered martensite ferritic steels10.1016/j.actamat.2006.08.046 ↗
13. Liu · Mater. Res. Express. · 2019 · 6
14. Microstructure and long-term creep properties of 9–12% Cr steels10.1016/j.ijpvp.2007.06.010 ↗
15. Nano-sized MX carbonitrides contribute to the stability of mechanical properties of martensite ferritic steel in the later stages of long-term aging10.1016/j.actamat.2019.06.012 ↗
16. Investigation on gradual degradation of mechanical property and microstructure in 9% Cr heat-resistant steels via interrupted creep test10.1007/s10853-023-08296-8 ↗
17. Microstructural stability and mechanical property of a medium-Si 12% Cr reduced activation ferritic/martensitic steel at high temperatures10.1007/s11665-022-06675-x ↗
18. Long-term thermal aging effects in ferritic-martensitic steel HT910.1016/j.matchar.2024.114418 ↗
19. Creep strength breakdown and microstructure evolution in a 3%co modified P92 steel10.1016/j.msea.2015.12.027 ↗
20. Effects of isothermal aging on microstructure and mechanical property of low-carbon RAFM steel10.1007/s40195-019-00883-6 ↗
21. Micrograin structure evolution associated with grain boundary characteristics in grade 91 steel during long-term creep exposure10.1016/j.msea.2021.141993 ↗
22. Effect of long-term aging on the microstructural evolution in a P91 steel10.3390/ma15082847 ↗
23. On the nucleation of Laves phase particles during high-temperature exposure and creep of tempered martensite ferritic steels10.1016/j.actamat.2014.08.008 ↗
24. The effect of microstructure evolution on the mechanical properties of martensite ferritic steel during long-term aging10.1016/j.actamat.2017.03.045 ↗
25. Synergistic strengthening of high-Cr martensitic heat-resistant steel and application of thermo-mechanical treatments
26. The influence of processing modes on second-phase particles of ferritic-martensitic steel EP-82310.1007/s11182-023-02907-2 ↗
27. Microstructure and mechanical properties of 12% Cr ferritic-martensitic steel after aging at 450°C during 5000 hours
28. Optimization of niobium content in direct quenched high-strength steels
29. Crystallographic features of lath martensite in low-carbon steel10.1016/j.actamat.2005.11.001 ↗
30. Crystallographic analysis of lath martensite in a 13Cr-5Ni steel by electron backscattering diffraction10.1007/s42243-018-0023-5 ↗
31. Investigation of special misorientations in lath martensite of low-carbon steel using the method of orientation microscopy10.1134/S0031918X1603008X ↗
32. JMatPro
33. Humphreys · 2004 · 628
34. Effect of thermal aging for up to 22 thousand hours on the structural and phase state of ferritic–martensitic steels EK181 and ChS13910.1134/S0031918X22050118 ↗
35. Effect of alloying on interfacial energy of precipitation/matrix in high-chromium martensitic steels10.1007/s10853-016-0654-5 ↗
36. Possible effect of Co on coarsening of M23C6 carbide and Orowan stress in a 9% Cr steel10.2355/isijinternational.41.356 ↗
37. Ma precipitates and particles coarsening of 9Cr–1.7 W–0.4 Mo–Co ferritic heat-resistant steel after isothermal aging10.1038/s41598-017-06191-2 ↗
38. Coarsening behavior for M23C6 carbide in 12% Cr-reduced activation ferrite/martensite steel: experimental study combined with DICTRA simulation10.1007/s10853-013-7334-5 ↗
39. The crystallography of M23C6 carbides in a martensitic 9% Cr steel after tempering, aging and creep10.1080/14786435.2013.765995 ↗
40. Microstructural evolution and mechanical properties of ultrafine-grained ferritic-martensitic steel during thermal aging10.1007/s11661-020-05939-2 ↗
41. Tanigawa ferritic-martensitic steels for fission and fusion applications10.1016/j.jnucmat.2019.05.058 ↗
42. Evolution of microstructure and mechanical properties of 9Cr ferrite/martensite steels with different Si content after long-term aging at 550° C10.1016/j.jallcom.2021.159817 ↗
43. Hardening mechanisms of 12% chromium ferritic-martensitic steel EP-82310.3103/S0967091222120026 ↗
44. The study of the formation of comlexes of implementation and substitution atoms in EP-823 ferritic-martensitic steel at different heat treatment
45. ASM handbook volume 8: mechanical testing and evaluation
46. A plasticity model describing yield-point phenomena of steels and its application to FE simulation of temper rolling10.1016/j.ijplas.2008.05.004 ↗
47. Continuous and discontinuous yielding behaviors in ferrite-cementite steels10.1016/j.actamat.2020.07.017 ↗