Microstructures and mechanical properties of Fe3O4-reinforced glass matrix composite coatings fabricated using a novel hot-rolling deposition process
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Structural capacity and fatigue performance of ASTM A709 grade 50CR steel10.1016/j.conbuildmat.2020.121379 ↗
2. Instrumented indentation testing and FE analysis for investigation of mechanical properties in structural steel weld zone10.1016/j.ijmecsci.2015.09.015 ↗
3. Mechanical properties of weathering steels at elevated temperatures10.1016/j.jcsr.2020.105996 ↗
4. Mechanical performance of welds using ASTM A709 grade 50CR steel as base metal10.1016/j.jcsr.2020.106121 ↗
5. Influence of Al2O3 content on microstructure and oxidation resistance of glass-ceramic coatings for 06Ni9DR alloy steel10.1016/j.ceramint.2024.09.233 ↗
6. Corrosion resistance and microstructural evolution of Y-Al-Si-O glass-ceramics environmental barrier coating candidate in the presence of CMAS10.1016/j.matchar.2024.114685 ↗
7. Oxidation performance and interfacial reaction behavior of glass-ceramic coating on TiAl alloy with electrodeposited SiO2 interlayer10.1016/j.surfcoat.2021.127495 ↗
8. Damage resistant and tolerant glass-ceramics with low-thermal expansion crystals10.1016/j.jeurceramsoc.2025.117226 ↗
9. Interaction between Y-Al-Si-O glass-ceramics for environmental barrier coating materials and Ca-Mg-Al-Si-O melts10.1016/j.ceramint.2020.05.037 ↗
10. The erosive wear behavior of basalt based glass and glass–ceramic coatings10.1016/j.triboint.2012.03.005 ↗
11. Development of an oxidation resistant glass-ceramic composite coating on Ti-47Al-2Cr-2Nb alloy10.1016/j.apsusc.2013.12.012 ↗
12. Li2O-Al2O3-SiO2 glass-ceramic coating on a porous silica ceramic substrate10.1016/j.jallcom.2014.02.104 ↗
13. Influence of Ca/Al ratio on physical and dielectric properties of Al2O3/CaO-B2O3-SiO2 glass-ceramics composite coatings prepared by high enthalpy atmospheric plasma spraying10.1016/j.jeurceramsoc.2021.11.021 ↗
14. Crystallization, thermal expansion and hardness of Y2O3-Al2O3-SiO2 glasses10.1016/j.ceramint.2021.05.236 ↗
15. A multifunctional Mg2Si5Al4O18/Y2Si2O7 glass-ceramic coating for porous Si3N4 ceramic10.1016/j.surfcoat.2024.131409 ↗
16. Characteristics of heat-treated plasma-sprayed CaO-MgO-SiO2-based bioactive glass-ceramic coatings on Ti-6Al-4V alloy10.1016/j.surfcoat.2014.03.056 ↗
17. Pulsed laser deposited bioactive RKKP-Mn glass-ceramic coatings on titanium10.1016/j.surfcoat.2018.10.004 ↗
18. Laser deposition of wear-resistant titanium oxynitride/titanium composite coatings on Ti-6Al-4V alloy10.1016/j.apsusc.2020.147212 ↗
19. Temperature-dependent tribological behavior and interface evolution of plasma sprayed molybdenum coatings10.1016/j.matchar.2025.115294 ↗
20. Study on surface enhancement mechanism and fretting fatigue behavior of casting aluminum alloy under acousto-electropulsing-stress synergistic strengthening
21. Microstructures and mechanical properties of wear-resistant titanium oxide coatings deposited on Ti-6Al-4V alloy using laser cladding10.1016/j.jeurceramsoc.2019.10.037 ↗
22. Effect of WC content on microstructure, mechanical properties, and tribo-corrosion behavior of laser-cladded Ni40A/WC composite coatings on H13 steel10.1016/j.matchar.2025.115072 ↗
23. Interfacial and tribological properties of laser deposited TiOxNy/Ti composite coating on Ti alloy10.1016/j.triboint.2020.106758 ↗
24. Novel water-based nanolubricant with superior tribological performance in hot steel rolling
25. Analysis of TiO2 nano-additive water-based lubricants in hot rolling of microalloyed steel10.1016/j.jmapro.2017.03.011 ↗
26. Deformation and fracture behaviours of a YAG single crystal characterized using nanoindentation method10.1016/j.matchar.2020.110302 ↗
27. A new type of high flexural strength micro-nano-composite ceramic tool material Ti(C,N)/WC/ZrO2 for integrated micro milling cutter10.1016/j.ijrmhm.2024.106628 ↗
28. Wear of ceramic-based dental materials10.1016/j.jmbbm.2019.01.009 ↗
29. Science and art of ductile grinding of brittle solids10.1016/j.ijmachtools.2020.103675 ↗
30. High temperature oxide scale characteristics of low carbon steel in hot rolling10.1016/j.jmatprotec.2004.04.167 ↗
31. Deformation characteristics and surface generation modelling of crack-free grinding of GGG single crystals10.1016/j.jmatprotec.2019.116577 ↗
32. X-ray photoelectron spectroscopy of sodium borosilicate glasses10.1016/S0022-3093(01)00720-7 ↗
33. Polishing performance and mechanism of a water-based nanosuspension using diamond particles and GO nanosheets as additives10.1016/j.triboint.2021.107241 ↗
34. Highlighting amorphous phase separation process on cooling borosilicate melts using impedance spectroscopy10.1016/j.jnoncrysol.2024.123155 ↗
35. Tribological performance of zeolite/sodium dodecylbenzenesulfonate hybrid water-based lubricants10.1016/j.apsusc.2022.153764 ↗
36. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗
37. Laser surface engineering of Ti-6Al-4V with TiO2/Al2O3 composite powder for improved wear resistance
38. Nanostructured Al2O3-YAG-ZrO2 ternary eutectic components prepared by laser engineered net shaping10.1016/j.actamat.2019.03.020 ↗
39. A distinctive material removal mechanism in the diamond grinding of (0001)-oriented single crystal gallium nitride and its implications in substrate manufacturing of brittle materials10.1016/j.ijmachtools.2024.104222 ↗
40. Understand anisotropy dependence of damage evolution and material removal during nanoscratch of MgF2 single crystals
41. Synergistic tribological performance of a water based lubricant using graphene oxide and alumina hybrid nanoparticles as additives10.1016/j.triboint.2019.02.031 ↗
42. Micromechanics of machining and wear in hard and brittle materials10.1111/jace.17502 ↗
43. Roughness-dependent tribological characteristics of water-based GO suspensions with ZrO2 and TiO2 nanoparticles as additives10.1016/j.triboint.2021.107073 ↗
44. Water-based nanosuspensions: formulation, tribological property, lubrication mechanism, and applications10.1016/j.jmapro.2021.10.002 ↗
45. Tribological properties of oscillatory pressure sintered SiC-based ceramics: influence of load and sliding speed10.1016/j.wear.2025.206074 ↗
46. Towards understanding the mechanisms of material removal and deformation in GaAs during nanomilling10.1016/j.jmatprotec.2025.118712 ↗
47. Surface micro-morphology model involved in grinding of GaN crystals driven by strain-rate and abrasive coupling effects10.1016/j.ijmachtools.2024.104197 ↗
48. Facile preparation of the dendritic Fe3O4 with a core-shell microstructure in SiO2-B2O3-Al2O3-CaO-Fe2O3 glass-ceramic system for enhanced microwave absorbing performance10.1016/j.jallcom.2021.160147 ↗
49. Effect of SiO2/B2O3 ratio on the thermophysical and wetting properties of borosilicate glass sealant for glass-metal joint10.1016/j.jmatprotec.2018.04.028 ↗
50. Effect of Na2CO3 content on thermal properties of foam-glass ceramics prepared from smelting slag10.1016/j.matchemphys.2020.123610 ↗
51. Comprehensive studies of activity of Ni in inorganic sodium borosilicate glasses doped with nickel oxide10.1016/j.apsusc.2021.149891 ↗
52. Mechanical properties and structural evolution of sodium borosilicate glasses during uniaxial tension: molecular dynamics simulation and experiments10.1016/j.ceramint.2024.09.413 ↗
53. A study on mechanical and tribological properties of eco-friendly synthesized ZrO2-doped borosilicate glasses10.1016/j.jmbbm.2023.106150 ↗
54. A review on ceramic coatings prepared by laser cladding technology10.1016/j.optlastec.2024.110993 ↗
55. Achieving dual strengthening in plasma-sprayed Mo coatings via acoustic-electro-stress synergistic processing: microstructural micro-forging and interfacial micro-metallurgy
56. Research on the microstructure and corrosion-wear resistance mechanism of Ti–6Al–4V alloy under cryogenic burnishing10.1016/j.jmrt.2025.02.189 ↗
57. Raman spectroscopic investigation of sodium borosilicate glass structure10.1007/BF02402831 ↗
58. Deformation and removal of semiconductor and laser single crystals at extremely small scales
59. Brittle-to-ductile transition in nanoscratching of silicon and gallium arsenide using Berkovich and conical tips10.1016/j.apsusc.2023.157934 ↗
60. Attaining exceptional wear resistance in an in-situ ceramic phase reinforced NbMoWTa refractory high entropy alloy composite by spark plasma sintering10.1016/j.wear.2024.205572 ↗
61. Microstructure and wear behavior of (ZrTaNb)C/N quaternary ceramic coatings prepared by double-cathode glow plasma surface alloying on titanium alloy10.1016/j.wear.2023.204789 ↗