Mechanism of crack formation of the butt joint between UMCo50A and Inconel 600

Haitao Xue, Wenjie Mu, Yang Jia, Zheng Wan, Weibing Guo, Cuixin Chen, Wenzhao Li, Yaojie Li

Abstract

The burner nozzle serves as the core component in pressurized coal-water slurry gasification systems . During the butt welding process between the nozzle and a nickel-based alloy cooling water coil, cracks were observed in the Heat Affected Zone (HAZ) of the welded joint. To address technical and safety concerns in industrial applications, this study systematically investigated the crack formation mechanism through microstructural characterization. Results indicate that liquation cracks originate from partial liquefaction of M 23 C 6 carbides along grain boundaries during the welding thermal cycle. The liquefied carbides combine with low-melting eutectic phases to form discontinuous liquid films at grain boundaries. As the material approaches its solidification temperature, these viscous liquid films exhibit limited fluidity. Subsequent welding tensile stresses induce liquid film decohesion from grain boundaries, ultimately generating microvoids that coalesce into macroscopic cracks.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal Forming Simulation Techniques · Metallurgy and Material Forming · Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Pilot-scale investigation on slurrying, combustion, and slagging characteristics of coal slurry fuel prepared using industrial wasteliquid[J]10.1016/j.apenergy.2013.11.026 ↗
2. Preparing coal slurry from coking wastewater to achieve resource utilization: Slurrying mechanism of coking wastewater–coal slurry[J]10.1016/j.scitotenv.2018.09.329 ↗
3. Microstructure and properties of TIG surfacing co-based alloy in UMCo50 process burner[J]
4. Thermo-economic optimization of gasification process with coal water slurry preheating technology[J]10.1016/j.energy.2020.117354 ↗
5. The weld heat-affected zone of the 18-Ni maraging steel[J]
6. Effects of constitutional liquation in 18-Ni maraging steel weldments[J]
7. Microstructural evolution of a Ni-based superalloy (617B) at 700°C studied by electron microscopy and atom probe tomography[J]10.1016/j.actamat.2011.11.020 ↗
8. Formation mechanisms for (Cr,Co)7C3/(Cr,Co)23C6 heterogeneous precipitates and stacking faults around carbides in surfacing welding of stellite alloy on stainless steel[J]10.1007/s12540-021-01049-9 ↗
9. Failure analysis of the end surface of the burner nozzle made of UMCo50 material in long-term high temperature oxygen-enriched sulfur-chlorine environment[J]10.1016/j.engfailanal.2024.107958 ↗
10. The mechanism for HAZ liquation of nickel-based alloy 617B during gas tungsten arc welding[J]10.3390/met10010094 ↗
11. Liquation cracking in fiber laser welded joints of Inconel 617[J]10.1016/j.jmatprotec.2015.07.004 ↗
12. The effect of pre-heating and pre-cold treatment on the formation of liquation and solidification cracks of nickel-based superalloy welded by laser beam[J]10.1016/j.jmrt.2020.07.053 ↗
13. Evolution of dislocations and twins in a strong and ductile nanotwinned steel[J]10.1016/j.actamat.2016.03.057 ↗
14. Evolution of microstructures and properties of a new γ/γ’ co-based superalloy via forging process[J]10.1007/s11837-019-03621-6 ↗
15. The effect of δ phase on the microplasticity evolution of a heat-treated nickel base superalloy[J]10.1016/j.mechmat.2020.103520 ↗
16. Transformation of carbides and mechanisms for cracking in co-based alloy surfacing layer during thermal fatigue[J]10.1016/j.matchar.2023.112971 ↗
17. Effect of Cr addition on microstructure and welding solidification cracking susceptibility of co-Al-W based superalloys[J]10.1016/j.jmapro.2020.03.049 ↗
18. The investigation of carbides evolution in a cobalt-base superalloy at elevated temperature[J]10.1016/j.jallcom.2016.10.256 ↗
19. Characterization of the as-cast microstructure and selected properties of the X-40 co-based superalloy produced via lost-wax casting[J]10.1007/s43452-022-00466-w ↗
20. Evolution behavior of liquid film in the heat-affected zone of laser cladding non-weldable nickel-based superalloy[J]10.1016/j.jallcom.2020.158463 ↗
21. The crack initiation and strengthening mechanism in FGH96 solid-state diffusion bonding joint by quasi-in-situ SEM-DIC and EBSD[J]
22. Cracking mechanism and susceptibility of laser melting deposited Inconel 738 superalloy[J]10.1016/j.matdes.2019.108105 ↗
23. Grain orientation, deformation microstructure and flow stress[J]10.1016/j.msea.2007.10.086 ↗
24. Microstructure analysis and cracking mechanism of aero-engine hot-end component K4169 superalloy based on in-situ EBSD test[J]
25. Effect of local carbide formation behavior on repair weld liquation cracking susceptibility for long-term-serviced 247LC superalloy[J]10.1016/j.jmrt.2023.12.003 ↗
26. Investigation on remelting solution heat treatment for nickel-based single crystal superalloys[J]10.1016/j.scriptamat.2017.04.016 ↗
27. Investigation on solution heat treatment response and γ’ solvus temperature of a Mo-rich second generation Ni based single crystal superalloy[J]10.1016/j.intermet.2020.106896 ↗
28. The behaviour and kinematic model for evolution and grain growth during solution treatment of a powdered metallurgical Ni-based superalloy[J]10.1016/j.matchar.2023.112820 ↗
29. Controlling hot cracking in Ni-based Inconel-718 superalloy cast sheets during tungsten inert gas welding[J]10.1016/j.jmatprotec.2015.03.031 ↗
30. Recrystallization behavior of selective laser melted co-Cr-Mo alloys with several heat treatment times[J]10.1016/j.msea.2022.143998 ↗
31. Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy[J]10.1016/j.matchar.2011.09.006 ↗