journal article·2026-02

Creep deformation and failure mechanisms of powder metallurgy processed FeCrAl alloy at 700 °C

Chenwei Zhang, Fanhao Yue, Kun Zhang, Hongchang Wang, Ling Li, Shiyi Bao, Lijia Luo, Yibin Tang, Xujia Wang, Wei Qin

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Nuclear Materials and Properties · High Temperature Alloys and Creep · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. Current status of materials development of nuclear fuel cladding tubes for light water reactors10.1016/j.nucengdes.2017.02.031 ↗
2. Using tube specimen to investigate the creep behavior of FeCrAl fuel cladding tubes10.1016/j.engfracmech.2023.109253 ↗
3. Terrani · 2016
4. Accident tolerant nuclear fuels and cladding materials10.1007/s11837-017-2701-3 ↗
5. High-temperature burst creep properties of nuclear-grade FeCrAl fuel cladding
6. Advanced oxidation-resistant iron-based alloys for LWR fuel cladding10.1016/j.jnucmat.2013.06.041 ↗
7. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
8. An investigation of FeCrAl cladding behavior under normal operating and loss of coolant conditions10.1016/j.jnucmat.2017.04.039 ↗
9. Recent studies on potential accident-tolerant fuel-cladding systems in light water reactors10.1007/s41365-020-0741-9 ↗
10. Characterization of stress-rupture behavior of nuclear-grade C26M2 FeCrAl alloy for accident-tolerant fuel cladding via burst testing10.1016/j.msea.2020.139753 ↗
11. High temperature oxidation of fuel cladding candidate materials in steam–hydrogen environments10.1016/j.jnucmat.2013.05.047 ↗
12. Performance of FeCrAl for accident-tolerant fuel cladding in high-temperature steam
13. Hydrothermal corrosion of 2nd generation FeCrAl alloys for accident tolerant fuel cladding10.1016/j.jnucmat.2020.152221 ↗
14. Microstructural stability and mechanical properties of advanced FeCrAl alloy cladding after thermal exposure at 800 °C ∼1200 °C10.1016/j.jnucmat.2025.155653 ↗
15. Study on high temperature creep behavior of the accident-resistant cladding Fe–13Cr–4Al-1.85Mo-0.85Nb alloy10.1016/j.msea.2020.140688 ↗
16. The microstructure and mechanical properties of micro-scale Y2O3 strengthened 9Cr steel fabricated by vacuum casting10.1016/j.matdes.2014.10.075 ↗
17. Designing ultrastrong and thermally stable FeCrAl alloys with the fine-grained structure10.1016/j.jmst.2023.06.053 ↗
18. Microstructure and tensile properties of Zr-containing ODS-FeCrAl alloy fabricated by laser additive manufacturing10.1016/j.msea.2020.138937 ↗
19. Additive manufacturing of FeCrAl alloys for nuclear applications - a focused review
20. Corrosion behavior of additively manufactured FeCrAl in out-of-pile light water reactor environments10.1038/s41529-024-00499-x ↗
21. Achieving columnar to equiaxed grain transformation in additively manufactured ODS-FeCrAl alloy via inhomogeneous composition distribution in melt pool10.1016/j.jallcom.2025.178557 ↗
22. Characterization of oxide dispersoids and mechanical properties of 14Cr-ODS FeCrAl alloys10.1016/j.jallcom.2019.152282 ↗
23. Evolution of microstructure and surface characteristics of FeCrAl alloys when subjected to flow boiling testing10.1016/j.jnucmat.2021.153269 ↗
24. Microstructure and tensile behavior of powder metallurgy FeCrAl accident tolerant fuel cladding10.1016/j.jnucmat.2022.153524 ↗
25. Influence of mechanical alloying and extrusion conditions on the microstructure and tensile properties of low-Cr ODS FeCrAl alloys10.1016/j.jnucmat.2018.10.017 ↗
26. Microstructural stability and intermetallic embrittlement in high Al containing FeCrAl-ODS alloys10.1016/j.msea.2021.140858 ↗
27. Effect of hot isostatic pressing on the microstructure and mechanical properties of selective laser melting FeCrAl ODS alloys10.1016/j.jallcom.2025.179691 ↗
28. Temperature dependence of the strength of fine- and ultrafine-grained materials10.1016/j.actamat.2010.10.062 ↗
29. Temperature dependence of strengthening mechanisms in the nanostructured ferritic alloy 14YWT: part II—mechanistic models and predictions10.1016/j.msea.2012.08.041 ↗
30. Effect of annealing temperature on the microstructure and mechanical properties of laves phase reinforced FeCrAl alloy thin-walled tubes10.1016/j.jnucmat.2022.153561 ↗
31. Cooperative grain boundary sliding in creep deformation of FeCrAl-ODS steels at high temperature and low strain rate10.1016/j.jnucmat.2018.04.050 ↗
32. High-temperature creep deformation in FeCrAl-oxide dispersion strengthened alloy cladding10.1016/j.msea.2020.139863 ↗
33. Deformation mechanism in nanolaminate FeCrAl alloys by in situ micromechanical strain rate jump tests at elevated temperatures10.1016/j.scriptamat.2022.114698 ↗
34. Control of laves precipitation in a FeCrAl-based alloy through severe thermomechanical processing10.3390/ma12182939 ↗
35. Recovery, recrystallization and precipitation behavior in an ATF FeCrAl alloy during annealing treatment10.1016/j.matchar.2022.112026 ↗
36. Interstitial precipitation in Fe-Cr-Al alloys10.1007/BF02652289 ↗
37. Field · 2018
38. Microstructure and high temperature mechanical properties of as-cast FeCrAl alloys10.1016/j.msea.2018.04.039 ↗
39. Structure and composition of oxides in FeCrAl ODS alloy with Zr addition10.1080/02670836.2017.1318245 ↗
40. High temperature creep and tensile properties of alumina formed on Fecralloy foils doped with yttrium10.1016/j.jeurceramsoc.2008.05.051 ↗
41. Development of Al added high-Cr ODS steels for fuel cladding of next generation nuclear systems10.1016/j.jnucmat.2010.12.300 ↗
42. High temperature deformation mechanism of 15CrODS ferritic steels at cold-rolled and recrystallized conditions10.1016/j.jnucmat.2015.07.049 ↗
43. Grain boundary sliding associated with low strain rate at 1000°C in recrystallized ODS ferritic steel10.1016/j.nme.2016.08.006 ↗
44. Viscoplastic behavior of a FeCrAl alloy for high temperature steam electrolysis (HTSE) sealing applications between 700°C and 900°C10.1016/j.msea.2011.01.050 ↗
45. Phase transformation and precipitation during solidification of FeCrAl alloy for automobile exhaust gas purifying systems10.1016/j.jallcom.2017.04.181 ↗
46. Influence of grain size, solute atoms and second-phase particles on creep behavior of polycrystalline solids10.1016/S0921-5093(01)01121-2 ↗
47. Creep behavior of discontinuous SiC Al composites10.1016/0921-5093(90)90004-M ↗
48. Creep behaviour of an oxide dispersion strengthened Al–5Mg alloy reinforced by silicon carbide particulates — an oxide dispersion strengthened Al–5Mg–30SiCp composite10.1016/S0921-5093(99)00452-9 ↗
49. Origin of threshold stresses in a P92-type steel10.1007/s12666-015-0757-8 ↗
50. Oxidation growth stresses in an alumina-forming ferritic steel measured by creep deflection10.1007/BF01670498 ↗
51. In-situ tube burst testing and high-temperature deformation behavior of candidate materials for accident tolerant fuel cladding10.1016/j.jnucmat.2015.08.030 ↗
52. The stress/creep rate behaviour of precipitation-hardened alloys10.1179/030634576790431462 ↗
53. A simple procedure for estimating threshold stresses in the creep of metal matrix composites
54. The Monkman-Grant relationship10.1016/0921-5093(89)90360-2 ↗
55. Creep rupture behavior of grade 91 steel10.1016/j.msea.2012.12.031 ↗
56. An assessment of creep deformation and rupture behaviour of 9Cr–1.8W–0.5Mo–VNb (ASME grade 92) steel10.1016/j.msea.2015.05.068 ↗
57. The relation between minimum creep rate and time to fracture10.1080/03063453.1976.11683560 ↗
58. Modified Monkman–Grant relationship for austenitic stainless steel foils10.1016/j.jnucmat.2012.08.048 ↗
59. Creep properties, microstructural evolution, and fracture mechanism of an Al added high Cr ODS steel during creep deformation at 600 °C10.1016/j.jnucmat.2021.153376 ↗
60. Creep deformation and cavitation in an additively manufactured Al-8.6Cu-0.4Mn-0.9Zr (wt%) alloy
61. Creep ductility limiting mechanisms in an additively manufactured Al-Ce-Ni-Mn-Zr alloy
62. On creep fracture by void growth10.1016/0079-6425(82)90001-9 ↗
63. Tertiary creep behaviour of 9Cr–1Mo ferritic steel10.1016/j.msea.2013.07.026 ↗
64. Creep damage mechanics and micromechanisms
65. Constitutive equations for creep rupture10.1016/0001-6160(77)90135-3 ↗
66. Deformation and damage processes during creep of Incoloy MA95710.1016/S0921-5093(04)00969-4 ↗
67. Coherent precipitation and strengthening in compositionally complex alloys: a review10.3390/e20110878 ↗
68. Hosford · 2005
69. On the attractive particle–dislocation interaction in dispersion-strengthened material10.1016/S1359-6454(97)00234-6 ↗
70. Effect of Zr content on microstructure and hardness of ODS-FeCrAl alloys10.1016/j.matchar.2022.112221 ↗
71. Effects of Zr addtion on recrystallization behaviors and mechanical properties of FeCrAl alloys10.1016/j.jmrt.2022.11.129 ↗
72. Atomic-scale insights into grain boundary-mediated plasticity mechanisms in a magnesium alloy subjected to cyclic deformation10.1016/j.actamat.2024.120210 ↗
73. In-situ study of creep in Sn-3Ag-0.5Cu solder10.1016/j.actamat.2020.06.013 ↗
74. Revealing hot tearing mechanism for an additively manufactured high-entropy alloy via selective laser melting
75. Reducing hot tearing by grain boundary segregation engineering in additive manufacturing: example of an AlxCoCrFeNi high-entropy alloy