journal article·2022-02

A new insight on evolution of texture and cellular structure of P/M processed Sm2Co17 permanent magnets and their effect on magnetic properties

D.M. RajKumar, Mithun Palit, D.V. Sridhara Rao, N.V. Rama Rao, Vajinder Singh, C.V.S. Kiran, A.K. Singh, S.V. Kamat

Publisher page

Abstract

Sm 2Co 17 type permanent magnets were prepared by a novel processing technique involving pulsed magnetization followed by cold isostatic pressing (CIP). The magnetic properties and microstructure of the CIPed magnetswere compared with those of the magnets processed through conventional uniaxial compaction in a transverse field press (TP)and heat treated under identical conditions. Enhanced values of remanence (B r ~ 10.7 kG) and energy product [(BH) max ~ 29 MGOe] were obtained in the CIPed magnetsas compared to those of the TP magnets[B r ~ 10 kG and (BH) max ~ 25 MGOe]. However, the values of intrinsic coercivity ( iH c ) and knee field (H k) of CIPed magnet were found to be lower than those of the TP magnet.The results were explained on the basis of the difference in texture, microtexture and microstructure obtained in these magnets due to different processing methods adopted.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. High temperature 2:17 magnets: relationship of magnetic properties to microstructure and processing10.1109/20.908808 ↗
2. RETM5 and RE2TM17 permanent-magnets development10.1063/1.341084 ↗
3. Hard-magnetic properties and microstructure of Sm(Co,Cu)zcompounds10.1063/1.322987 ↗
4. Magnetic properties of Sm-Co-Fe-Cu alloys for permanent magnet materials10.1143/JJAP.14.1619 ↗
5. Sm–Co–Cu–Fe–Ti magnets10.1143/JJAP.17.1993 ↗
6. Rare earth-cobalt permanent magnets near the 2-17 composition10.1109/TMAG.1976.1059138 ↗
7. Sintered Ce-Co-Cu-Fe-Ti magnets10.1063/1.89280 ↗
8. A study of magnetic hardening in Sm(Co0.69Fe0.22Cu0.07Zr0.02)7.2210.1063/1.330866 ↗
9. Metallurgical behavior of Sm(Co,Fe,Cu,Zr)z alloys10.1063/1.333575 ↗
10. The development of high energy product permanent magnets from 2:17 RE-TM alloys10.1109/TMAG.1984.1063180 ↗
11. Recent progress in 2:17-type permanent magnets10.1007/BF02648616 ↗
12. Microstructures of precipitation-hardened SmCo permanent magnets10.1063/1.330867 ↗
13. Microstructure and high temperature magnetic properties of Sm(Co,Cu,Fe,Zr)z(z= 6.7–9.1) permanent magnets10.1063/1.369597 ↗
14. Sm(Co,Fe,Cu,Zr)zmagnets for high temperature applications: microstructuraland magnetic analysis10.1109/TMAG.2002.803313 ↗
15. Coercivity of precipitation hardened cobalt rare earth 17:2 permanent magnets10.1016/0304-8853(82)90010-5 ↗
16. Effects of Zr content on phasetransformation and magnetic properties of Sm(Co Cu Fe)7-9magnetalloys10.2320/jinstmet1952.52.2_243 ↗
17. Evolution of magnetic domain structures and coercivity in high-performance SmCo 2:17-type permanent magnets10.1016/j.actamat.2005.10.026 ↗
18. Microstructure of aged (Co,Cu,Fe)7Sm magnets10.1063/1.323729 ↗
19. Genesis of the cell microstructure in the Sm(Co, Fe, Cu, Zr) permanent magnets with 2:17 type10.1002/pssa.2211400104 ↗
20. Rare earth Iron permanent magnets
21. Microstructure and properties of step aged rare earth alloy magnets10.1063/1.328987 ↗
22. Direct evidence for Cu concentration variation and its correlation to coercivity in Sm(Co0.74Fe0.1Cu0.12Zr.04)7.4 ribbons10.1016/j.scriptamat.2009.01.006 ↗
23. Analysis of the temperature dependence of the coercive field of Sm2Co17 based magnets10.1016/S1359-6462(02)00619-X ↗
24. Micromagnetism and the microstructure of high-temperature permanent magnets10.1063/1.1809250 ↗
25. Permanent magnet alloys based on Sm2Co17; phase evolution in the quinary system Sm–Zr–Fe–Co–Cu10.3139/146.018078 ↗
26. Samarium–cobalt 2:17 magnets: analysis of the coercive field of Sm2(CoFeCuZr)17 high-temperature permanent magnets10.1016/j.scriptamat.2010.03.066 ↗
27. Magnetic properties and coercivity mechanism of melt-spun Sm(Co1−xFex)6.8Zr0.2C0.06 ribbons with TbCu7 structure10.1016/j.jmmm.2004.04.111 ↗
28. Effect of grain size on microstructure and magnetic properties of Sm2(Co,Cu,Fe,Zr)17 permanent magnets10.1016/j.matchemphys.2016.05.033 ↗
29. A direct method of determining preferred orientation of a flat reflection sample using a Geiger counter X-Ray spectrometer10.1063/1.1698268 ↗
30. Magnetic properties of cobalt-samarium with a 24-MG Oe energy product10.1063/1.1654011 ↗
31. Correlation of microchemistry of cell boundary phase and interface structure to the coercivity of Sm(Co0.784Fe0.100Cu0.088Zr0.028)7.19 sintered magnets10.1016/j.actamat.2016.12.050 ↗