journal article·2025-11

Effect of post-weld heat treatment on microstructure and mechanical properties of linear friction welded Ti60/Ti17 dissimilar titanium alloy joint

Tian Xu, Wentao Huang, Danling Luo, Chao He, Hong Zhang, Chong Wang, Qingyuan Wang, Fulin Liu, Yongjie Liu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Effect of solution and aging treatment on the microstructure and properties of LAZ931 Mg-Li alloy by friction stir processing10.3390/met15030314 ↗
2. Heterogeneous microstructure and associated mechanical properties of thick electron beam welded Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy joint10.1016/j.msea.2021.141850 ↗
3. Theoretical and experimental studies of structural integrity of dovetail joints in aeroengine discs10.1016/0924-0136(95)01880-8 ↗
4. Comprehensive investigation on linear friction welding a dissimilar material joint between Ti17(α+β) and Ti17(β): microstructure evolution, failure mechanisms, with simultaneous optimization of tensile and fatigue properties10.1016/j.msea.2024.146818 ↗
5. Effects of annealing on microstructure and properties of linear friction welded dissimilar titanium joints10.1179/1362171814Y.0000000243 ↗
6. BLISK fabrication by linear friction welding
7. High strength beta titanium alloys: new design approach10.1016/j.msea.2015.01.073 ↗
8. Effect of strain rate and temperature on strain hardening behavior of a dissimilar joint between Ti–6Al–4V and Ti17 alloys10.1016/j.matdes.2013.11.003 ↗
9. Enhancing the high-temperature oxidation resistance of TiAl alloy via a novel Al2O3/Ti5Si3 composite coating prepared through a modified pack cementation technique
10. Strain-controlled fatigue properties of dissimilar welded joints between Ti–6Al–4V and Ti17 alloys10.1016/j.matdes.2013.02.034 ↗
11. Influence of environment on fatigue mechanisms in high-temperature titanium alloy IMI83410.1016/j.ijfatigue.2005.06.009 ↗
12. Influence of welded pores on fatigue behavior of TC17 titanium alloy welded joints subjected to gigacycle regime at room and high temperatures10.1016/j.jmst.2023.09.006 ↗
13. The novel high-entropy alloy filler realized the efficient inhibition of the violent reaction and brittle phase formation in the SiCf/SiC heterogeneous brazed joint
14. Low cycle fatigue properties of linear friction welded joint of TC11 and TC17 titanium alloys10.1016/j.jallcom.2016.03.113 ↗
15. Microstructure and mechanical properties of a high nitrogen titanium alloy10.1016/j.msea.2007.08.074 ↗
16. Optimizing microstructure and mechanical properties of Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy electron beam welded joint through post-weld heat treatment10.1016/j.jmrt.2023.09.052 ↗
17. Strain hardening behavior of linear friction welded joints between TC11 and TC17 dissimilar titanium alloys10.1016/j.msea.2014.10.044 ↗
18. Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint10.1179/1362171811Y.0000000079 ↗
19. Microstructural evolution and mechanical properties of a linear friction welded two-phase Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy joint10.1016/j.msea.2018.11.059 ↗
20. Effect of post-weld heat treatment on microstructure and property of linear friction welded TC17/TA15 titanium alloy joint
21. Influence of parent metal microstructure and post-weld heat treatment on microstructure and mechanical properties of linear friction welded Ti-6Al-4V joint10.1002/adem.201100203 ↗
22. Effect of heat treatment on the microstructure, microhardness and impact toughness of TC11 and TC17 linear friction welded joint10.1016/j.msea.2020.140496 ↗
23. Measuring residual stresses in linear friction welded joints composed by dissimilar titanium10.1080/13621718.2015.1115158 ↗
24. Heat reflux in flash and its effect on joint temperature history during linear friction welding of steel10.1016/j.ijthermalsci.2012.12.004 ↗
25. Tensile and fatigue behavior of electron beam welded TC17 titanium alloy joint10.1016/j.ijfatigue.2019.105210 ↗
26. Linear friction welding of Ti-6Al-4V: processing, microstructure, and mechanical-property inter-relationships10.1007/s11661-005-0335-5 ↗
27. In situ characterizations of phase transformations kinetics in the Ti17 titanium alloy by electrical resistivity and high temperature synchrotron X-ray diffraction10.1016/j.msea.2007.04.072 ↗
28. Enhancing the mechanical properties of electron beam welded TC17 titanium alloy joint by post-weld heat treatment10.1016/j.jallcom.2019.151937 ↗
29. Linear friction welding of Ti60 near-α titanium alloy: investigating phase transformations and dynamic recrystallization mechanisms10.1016/j.matchar.2022.112424 ↗
30. Comparative study on machinability and surface integrity of γ-TiAl alloy in laser assisted milling10.1016/j.jmrt.2024.10.028 ↗
31. Grain size and misorientation evolution in linear friction welding of additively manufactured IN718 to forged superalloy AD730™10.1016/j.matchar.2020.110766 ↗
32. Linear friction welding of equiaxed Ti17 titanium alloy: effects of microstructure evolution on tensile and impact properties10.1007/s10853-023-08666-2 ↗
33. Effects of welding parameters on material flow behavior during linear friction welding of Ti6Al4V titanium alloy by numerical investigation10.1007/s00170-015-7408-4 ↗
34. Linear friction welding of Ti60 near-α titanium alloy: investigating phase transformations and dynamic recrystallization mechanisms
35. Phase transformation during the continuous cooling in near α titanium alloy Ti6010.1016/S1875-5372(15)30061-8 ↗
36. Texture development in near-α Ti friction stir welds10.1016/j.actamat.2010.08.007 ↗
37. Martensitic transformations in Ti-Mo alloys10.1007/BF00772735 ↗
38. Texture development during the torsion testing of α-iron and two IF steels10.1016/1359-6454(96)00114-0 ↗
39. Texture formation during equal channel angular extrusion of fcc and bcc materials: comparison with simple shear10.1016/j.msea.2004.11.032 ↗
40. Interfacial bonding mechanism of linear friction welded dissimilar Ti2AlNb–Ti60 joint: grain intergrowth induced by combined effects of dynamic recrystallization, phase transformation and elemental diffusion10.1016/j.jmrt.2023.04.184 ↗
41. Interface evolution and bond strength when diffusion bonding materials with stable oxide films10.1002/sia.1088 ↗
42. Interfacial characteristics and cohesion mechanisms of linear friction welded dissimilar titanium alloys: Ti–5Al–2Sn–2Zr–4Mo–4Cr (Ti17) and Ti–6Al–2Sn–4Zr–2Mo (Ti6242)10.1016/j.matchar.2019.109942 ↗
43. Study on non-isothermal transformation of Ti-6Al-4V in solution heating stage
44. Joining of dissimilar alloys Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si using linear friction welding10.3390/ma13173664 ↗
45. Influence of matrix microstructure on aging response of near alpha titanium alloy (IMI834) parent metal and welds on toughness10.1179/174328409X439141 ↗
46. Resistance spot welded NiTi shape memory alloy to Ti6Al4V: correlation between joint microstructure, cracking and mechanical properties
47. Through analysis of the microstructure changes during linear friction welding of the near-α titanium alloy Ti-6Al-2Sn-4Zr-2Mo (Ti6242) towards microstructure optimization10.1016/j.matchar.2019.02.027 ↗
48. The effect of heat treatment on microstructure evolution and tensile properties of selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2018.12.051 ↗
49. Optimization for the process parameters of nickel–titanium nitride composites fabricated via jet pulse electrodeposition10.3390/nano14242034 ↗
50. Contributions of an innovative post-weld heat treatment to the micro-tensile behavior of two mono-material linear friction welded joints using: the β-metastable Ti–5Al–2Sn–2Zr–4Mo–4Cr (Ti17) and the near-α Ti–6Al–2Sn–4Zr–2Mo (Ti6242) Ti-alloys10.1016/j.msea.2019.138334 ↗
51. Strength, fatigue strength and toughness of dissimilar Ti17–Ti64 linear friction welded joints: effect of soft surface contamination and depletion of α precipitates10.1016/j.msea.2020.139989 ↗
52. Optimizing microstructure and mechanical properties of Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy electron beam welded joint through post-weld heat treatment10.1016/j.jmrt.2023.09.052 ↗
53. Mechanical properties and microstructure of a high-power laser-welded Ti6Al4V titanium alloy10.1007/s11665-020-04737-6 ↗
54. Cooperative effect of strength and ductility processed by thermomechanical treatment for Cu–Al–Ni alloy
55. Microstructure and mechanical properties of WC-12Co cemented carbide fabricated by laser powder bed fusion on a WC-20Co cemented carbide substrate10.1016/j.jmrt.2024.05.266 ↗
56. In-situ isothermal aging TEM analysis of a micro Cu/ENIG/Sn solder joint for flexible interconnects10.1016/j.jmst.2023.06.020 ↗
57. Dissimilar linear friction welding of Ni-based superalloys10.1016/j.ijmachtools.2023.104062 ↗