Abstract

Abstract The effects of spark plasma sintering and conventional H2 atmosphere sintering on the microstructure and properties of W–15Cu alloy using ultrafine W–15Cu composite powder fabricated by spray drying and calcining-continuous reduction technology were investigated. Results showed that W–15Cu alloy, consolidated by spark plasma sintering for 10 min at 1200 °C under a pressure of 30 MPa, with 98% relative density, transverse rupture strength 1259 MPa, Vickers hardness 379, average grain size 0.8 µm and thermal conductivity 189 W/m K, was obtained. In comparison to the conventional H2 atmosphere sintering process, spark plasma sintering to W–15Cu alloy could be achieved at lower sintering temperature and shorter sintering time. Furthermore, better properties in spark plasma sintered compacts were obtained, moreover spark plasma sintering resulted in finer microstructure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Dilatometric analysis on the sintering behavior of nanocrystalline W–Cu prepared by mechanical alloying10.1016/S0925-8388(01)01805-9 ↗
2. Thermal conductivity of W–Cu composites at various temperatures10.1016/S0167-577X(01)00330-5 ↗
3. Fabrication of W–20 wt % Cu composite nanopowder and sintered alloy with high thermal conductivity10.1016/S0167-577X(03)00071-5 ↗
4. Preparation of W–Cu nanocomposite powder by hydrogen-reduction of ball-milled W and CuO powder mixture10.1016/j.matlet.2003.08.035 ↗
5. Microstructure and sintering behavior of W–Cu nanocomposite powder produced by thermo-chemical process10.1016/S0263-4368(02)00003-3 ↗
6. Apparent viscosity of W–Cu powder compacts during sintering10.1016/j.msea.2004.05.050 ↗
7. Characterization of W–20Cu ultrafine composite powder prepared by spray drying & calcining-continuous reduction technology10.1016/j.matchemphys.2007.03.032 ↗
8. Bending strength and microstructure of Al2O3 ceramics densified by spark plasma sintering10.1016/S0955-2219(00)00086-8 ↗
9. Rapid sintering of nanocrystalline ZrO2(3Y) by spark plasma sintering10.1016/S0955-2219(00)00152-7 ↗
10. Spark plasma sintering behavior of nanocrystalline WC–10Co cemented carbide powders10.1016/S0921-5093(02)00605-6 ↗
11. Granulation of a hardmetal powder for spark plasma sintering10.1016/S0032-5910(02)00266-8 ↗
12. Mechanical properties, phases and microstructure of ultrafine hardmetals prepared by WC–6.29Co nanocrystalline composite powder10.1016/j.msea.2004.09.043 ↗
13. The effect of tungsten buffer layer on the stability of diamond with tungsten carbide–cobalt nanocomposite powder during spark plasma sintering10.1016/j.diamond.2006.01.021 ↗
14. Enhanced sintering through second phase additions10.1179/pom.1985.28.1.7 ↗
15. Effect of Cu purity on thermal conductivity of W–Cu composites