journal article·2007-07

Influence of thermal exposure on γ′ precipitation and tensile properties of DZ951 alloy

P.C. Xia, J.J. Yu, X.F. Sun, H.R. Guan, Z.Q. Hu

Materials Characterization· Volume 58· Issue 7
Publisher page

Abstract

Abstract The effect of long-term exposure on the γ′ phase and the tensile behavior of a directionally solidified nickel-base superalloy DZ951 was investigated. Alloys after standard heat treatment (SHT) were isothermally aged at 900 °C up to 2000 h and tensile tests were performed in both SHT and aged conditions at various temperatures. The morphology of the γ′ phase changes from cuboid to rafting and the size increases from 300 nm at SHT to 930 nm, and the volume fraction of the γ′ phase decreases from 70% at SHT to 65% during aging at 900 °C for 2000 h. The changing trend of yield stress at different test temperatures is similar. The yield stress decreases slightly at 600 °C. This arises from few dislocations shearing the γ′ precipitates. There is a peak yield stress value at 760 °C, which is attributed to the high strength of the γ′ phase, the homogeneous deformation structure, and dislocation-γ′ precipitate and dislocation–dislocation interactions. The yield stress then decreases rapidly with increased temperature. The low strength of the γ′ phase and γ′ rafting at high temperature contribute to the drop of yield stress. The change of tensile elongation is inverse to that of yield stress. The yield stress continuously decreases with the increase of aging time at 900 °C. This arises from the coarsening of γ′ and a decrease in the γ′ volume fraction.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Sims · 1987 · vol. II
2. Heat treatment of UDIMET 720Li: the effect of microstructure on properties10.1016/S0921-5093(98)00867-3 ↗
3. Influence of grain size and heat treatment on the microstructure and mechanical properties of the nickel-base superalloy U 720 LI10.1016/S0921-5093(97)00161-5 ↗
4. Improvement of creep strength in a nickel-base single-crystal superalloy by heat treatment10.1016/0025-5416(83)90199-4 ↗
5. Factors which influence directional coarsening of γ′ during creep in nickel-base superalloy single crystals
6. Microstructural evolution of a single crystal nickel-base superalloy during thermal exposure10.1016/S0167-577X(03)00359-8 ↗
7. γ′ coarsening in high volume fraction nickel-base alloys
8. Long term coarsening of γ prime precipitates in a Ni-base superalloy10.1023/A:1018694716756 ↗
9. Microstructural changes which occur during isochronal heat treatment of the nickel-base superalloy in-73810.1007/BF00647782 ↗
10. The precipitation and growth kinitics of γ′ in Nimonic PE1610.1016/0025-5416(78)90167-2 ↗
11. The effect of long-term thermal exposures on the microstructure and properties of CMSX-10 single crystal Ni-base superalloys10.1016/j.msea.2004.04.001 ↗
12. The influence of thermal exposure on the γ′ precipitates characteristics and tensile behavior of superalloy IN-738LC10.1016/j.jmatprotec.2004.01.006 ↗
13. Tensile deformation mechanisms at different temperatures in the Ni-base superalloy GTD-11110.1016/j.jmatprotec.2004.04.273 ↗
14. Study of microstructure and mechanical properties of high performance Ni-base superalloy GTD-11110.1016/S0921-5093(01)01709-9 ↗
15. The dislocation microstructure of a nickel-base single-crystal superalloy after tensile fracture10.1016/S0921-5093(03)00039-X ↗