journal article·2008-11

Effect of Sn on the microstructure and compressive deformation behavior of the AZ91D aging alloy

R.G. Li, Y. Xu, W. Qi, J. An, Y. Lu, Z.Y. Cao, Y.B. Liu

Materials Characterization· Volume 59· Issue 11
Publisher page

Abstract

Abstract The effect of Sn on the microstructure and compressive deformation behavior of aging AZ91D magnesium alloy was investigated. The results show that the discontinuous precipitation occurs near the grain boundary in the form of lamellar precipitates of the Mg17Al12 phase. These precipitates alternatively lie in the α-Mg matrix perpendicular to the grain boundaries. With an increase in the Sn content, the cellular discontinuous precipitation can be efficiently suppressed, such that no discontinuous precipitation is observed when the Sn content is increased to 2 wt.%. The AZ91D aging alloy has a higher ultimate fracture strength than the base 2%Sn alloy due to the large numbers of grains containing the cellular discontinuous precipitation forming nearby the grain boundaries. In these regions the β phase can effectively hinder the dislocation movement. Conversely, the soft behavior induced by a high fraction of twins is the main reason that the strength of 2%Sn alloy is lower than that of the AZ91D alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Development of the as-cast microstructure in magnesium–aluminum alloys10.1016/S1471-5317(00)00007-9 ↗
2. Microstructure and mechanical properties of a thixocast Mg–Cu–Y alloy10.1016/S1359-6462(03)00392-0 ↗
3. TEM STUDY OF CONTINUOUS PRECIPITATION IN Mg-9 Wt%Al-1 Wt%Zn ALLOY10.1016/S1359-6454(00)00004-5 ↗
4. Macroscopic kinetics of discontinuous precipitation in a Mg-8.5 wt% Al alloy10.1016/0956-7151(92)90147-7 ↗
5. Crystallography of Mg17Al12 precipitates in AZ91D alloy10.1016/S1359-6462(02)00555-9 ↗
6. The effect of gold additions on the aging behaviour and creep properties of the magnesium alloy AZ91E10.1016/S0921-5093(02)00731-1 ↗
7. Age hardening in a Mg-9 wt.% Al alloy10.1016/0001-6160(68)90109-0 ↗
8. Effect of Pb and Sb additions on the precipitation kinetics of AZ91 magnesium alloy10.1016/j.msea.2006.12.132 ↗
9. Effect of Pb addition on aging behavior of AZ91 magnesium alloy10.1016/j.msea.2006.10.119 ↗
10. Enhanced age hardening response by the addition of Zn in Mg–Sn alloys.Scripta Materialia10.1016/j.scriptamat.2006.04.005 ↗
11. Morphology and chemical nanoanalysis of discontinuous precipitation in Mg-Al alloys—I. Regular growth10.1016/0956-7151(94)90450-2 ↗
12. On the competition between continuous and discontinuous precipitations in binary Mg-Al alloys
13. Twinning-induced softening in polycrystalline AM30 Mg alloy at moderate temperatures10.1016/j.scriptamat.2005.11.029 ↗