journal article·2007-08

Electrochemical deposition and characterization of Ni–P alloy thin films

T. Mahalingam, M. Raja, S. Thanikaikarasan, C. Sanjeeviraja, S. Velumani, Hosun Moon, Yong Deak Kim

Materials Characterization· Volume 58· Issue 8-9
Publisher page

Abstract

Nickel phosphorus (Ni-P) alloy thin films were prepared by electrodeposition on pre-cleaned copper substrates using a potentiostatic cathodic electrodeposition method from sulfate electrolyte baths at various sodium hypophosphite (NaH{sub 2}PO{sub 2}) concentrations. X-ray diffraction studies reveal polycrystalline cubic alloys at low concentrations of phosphorus (< 13.5 at.%) and these transformed into amorphous alloys at higher concentrations. X-ray photoelectron spectra show the presence of Ni{sub 2}p and P{sub 2}p lines corresponding to their binding energies. Scanning electron microscopic studies reveal spherical shaped grains at low phosphorus contents and modules of cauliflower type morphology at higher phosphorus concentrations. The effects of phosphorus concentration on the crystal structure, composition and morphology are studied and discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Semiconductor materials and interfaces · Chalcogenide Semiconductor Thin Films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Electrodeposition of amorphous alloys based on the iron group of metals10.1149/1.1391850 ↗
2. Nanocrystallization studies of an electroless plated Ni–P amorphous alloy10.1149/1.1405518 ↗
3. Effect of ammonium on low temperature electrodeposition of Ni–P alloys10.1016/S0167-577X(03)00097-1 ↗
4. Electrochemical production and corrosion testing of amorphous Ni–P10.1149/1.2095468 ↗
5. Electrodeposition of Ni–P alloys from Ni-citrate bath10.1016/0013-4686(96)00173-9 ↗
6. Surface morphology and electronic state characterization of Ni–P amorphous alloy films10.1016/S0022-3093(00)00430-0 ↗
7. Corrosion resistance of ternary Ni–P based alloys in sulfuric acid solutions10.1016/S0013-4686(02)00198-6 ↗
8. Characteristics of Ni–P alloy electrodeposited from a sulfamate bath10.1016/S0257-8972(03)00661-3 ↗
9. Brenner · 1963 · vol. I
10. Electrodeposition and corrosion performance of nickel–phosphorus amorphous alloys
11. Dini · 1993
12. Structural transition in electroplated Ni–P alloys10.1007/BF01730163 ↗
13. Microstructure of electroplated Ni–P alloy films10.2320/jinstmet1952.58.2_138 ↗
14. Wagner · 1983
15. 2000 · 47