journal article·2007-08

Effect of artificial aging on the microstructure of weldment on API 5L X-52 steel pipe

B. Vargas-Arista, J.M. Hallen, A. Albiter

Materials Characterization· Volume 58· Issue 8-9
Publisher page

Abstract

Abstract The effects of artificial aging on the microstructure in the weldment of an API 5L X-52 steel pipe were studied. Aging was performed at 250 °C over a period of 1000 h and values were recorded at every 100 h intervals. Transmission electron microscopy observations showed precipitation strengthening from nearly circular Nb–C containing nanoparticles for the base metal and heat affected zone, and cementite for the weld metal. The largest amount of precipitation in the weldment zone was obtained at 500 h, due to peak-aging, which showed the highest particle density. The weld metal was more susceptible to aging, exhibiting the highest increase in precipitation at 500 h, followed by the heat affected zone. After 500 h, the deterioration in the microstructure was caused by the coarsening of particles due to over-aging. The base metal showed the larger increment in particle size after 900 h of aging accompanied by a bigger decrease in fine particles than in the weld metal.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Gladman · 1997 · 185
2. High strength line pipe: current and future production
3. Microstructure of microalloyed line pipe steels
4. Microstructures of line pipe steels10.1179/cmq.1983.22.2.169 ↗
5. Microstructural characterization of precipitation in an isothermally aged Nb-containing microalloyed steel10.2355/isijinternational.41.1532 ↗
6. Leslie · 1982 · 79
7. Steel · 1992 · 97
8. Effect of stress on microstructural change due to aging at 823 K in multi-layer welded joint of 2.25Cr–1mo steel10.1016/j.ijpvp.2003.12.017 ↗
9. Sensitization behavior of type 308 stainless steel weld metals after postweld heat treatment and low-temperature aging and its relation to microstructure10.1007/s11661-002-0183-5 ↗
10. Efecto del envejecimiento artificial de ductos de acero grado API 5L X52 y X70 en la susceptibilidad a la corrosión
11. Aging behavior of the Ti–29Nb–13Ta–4.6Zr new beta alloy for medical implants10.1007/s11661-002-0110-9 ↗
12. Ni4Ti3-precipitation during aging of NiTi shape memory alloys and its influence on martensitic phase transformations10.1016/S1359-6454(02)00257-4 ↗
13. Fracture toughness of cold worked and simulated heat affected structural steel10.1016/S0013-7944(97)00100-8 ↗
14. API Standard 1104 · 2005 · 3
15. API Specification 5L · 2004 · 8
16. NRF-001-PEMEX · 2000 · 12
17. The effect of microstructural change on fracture behavior in heat-affected zone of API 5L X65 pipeline steel
18. 1976 · 224
19. Evans · 1997 · 148
20. The response of carbo-nitride particles in HSLA steels to weld thermal cycles10.1016/0001-6160(87)90242-2 ↗
21. Effect of the artificial aging time on the mechanical properties of weldment on API 5L X-52 line pipe steel10.1007/BF02586102 ↗