journal article·2008-11

Effects of deformation and Mo, Nb, V, Ti on continuous cooling transformation in Cu–P–Cr–Ni–Mo weathering steels

Chunling Zhang, Dayong Cai, Yuhui Wang, Mingqing Liu, Bo Liao, Yunchang Fan

Materials Characterization· Volume 59· Issue 11
Publisher page

Abstract

Abstract The continuous cooling transformation (CCT) diagrams of the weathering steels Cu–P–Cr–Ni–Mo were investigated by means of a combined method of dilatometry and metallography. For five of the steels (B, C, D, E and F), since there is a metastable austenite gap completely open or half-open between the ferrite and the bainite transformation regions, it is possible to obtain dual-phase microstructure directly by hot-rolling and appropriate cooling. Hot deformation increased the transformation start temperature Ar3 significantly, enlarged the polygonal ferrite transformation temperature range, and shortened the gestation period of pearlite and polygonal ferrite transformation. Mo effectively retards the bainite and the pearlite transformations, elevates the pearlite-finish temperature, and induces the metastable austenite gap formed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Magnetic Properties and Applications · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Design of process parameters for dual phase steel production with strip rolling using the finite-element method10.1016/S0924-0136(99)00241-1 ↗
2. Microstructural evolution and its relation to mechanical properties in a drawn dual-phase steel10.1023/A:1004705705208 ↗
3. Influence of deformation induced ferrite transformation on grain refinement of dual phase steel10.1016/S0921-5093(01)01359-4 ↗
4. The effect of SO2, NO2, NO and O3 on the corrosion of unalloyed carbon steel and weathering steel — the results of laboratory exposures10.1016/0010-938X(96)00025-X ↗
5. Premature corrosion failure of structural highway components made from weathering steel10.1016/S1350-6307(01)00038-3 ↗
6. Study on the dual-phase treatment of weathering steel 09CuPCrNi10.1016/j.matlet.2003.10.018 ↗
7. Microstructure and mechanical properties of dual-phase weathering steel 09CuPTiRe10.1023/B:JMSC.0000033436.06575.aa ↗
8. Dual-phase treatment of weathering steel: dual-phase weathering steel
9. A study of the effect of the thermomechanical history on the mechanical properties of a high niobium steel10.1016/0921-5093(95)10050-4 ↗
10. Continuous cooling transformation of undeformed and deformed low carbon pipeline steels10.1016/S0921-5093(03)00074-1 ↗