Structural and dielectric properties of Li2O-doped TiO2
Source abstract
Abstract
Abstract The dielectric properties of the system Li–Ti–O have been exploited in the frequency range 20 Hz–1 MHz in order to obtain permittivity data of materials having high- κ ′ and low loss. Doping of titanium dioxide with lithium oxide acts as a strong promoter of the anatase to rutile phase transition and it may reduce the phase transition temperature (915 °C) by more than 100 °C, possibly due to induced oxygen concentration disorders in the ternary Li–Ti–O system. For TiO 2 :Li 2 O molar ratios of 98.92:1.08 and calcination temperature of 950 °C the resulting material exhibits high- κ ′ and low-loss permittivity properties with lack of interfacial polarization effects. Its dielectric response is superior compared to pure (undoped) rutile as obtained by calcination at much higher temperatures (1180 °C).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Dielectric properties of ceramics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. The identification of naturally occurring TiO2 (B) by structure determination using high-resolution electron microscopy, image simulation, and distance-least-squares refinement
2. TiO2 (B) a new form of titanium dioxide and the potassium octatitanate K2Ti8O1710.1016/0025-5408(80)90076-8 ↗
3. New hollandite oxides: TiO2(H) and K0.06TiO210.1016/0022-4596(89)90204-1 ↗
4. Topotactic oxidation of ramsdellite-type Li0.5TiO2, a new polymorph of titanium dioxide: TiO2(R)10.1006/jssc.1994.1337 ↗
5. Atomistic simulation of the crystal structures and bulk moduli of TiO2 polymorphs10.1016/S0022-3697(00)00246-8 ↗
6. Rutile: normal probability plot analysis and accurate measurement of crystal structure10.1063/1.1676569 ↗
7. Structural-electronic relationships in inorganic solids: powder neutron diffraction studies of the rutile and anatase polymorphs of titanium dioxide at 15 and 295 K10.1021/ja00246a021 ↗
8. Polyhedral thermal expansion in the TiO2 polymorphs; refinement of the crystal structures of rutile and brookite at high temperature
9. TiO2-II ambient pressure preparation and structure refinement10.1016/0025-5408(88)90040-2 ↗
10. Baddeleyite-type high-pressure phase of TiO210.1126/science.251.4995.786 ↗
11. Ultrastiff cubic TiO2 identified via first-principles calculations10.1103/PhysRevLett.98.035502 ↗
12. Permittivity properties of thermally treated TiO210.1016/j.matlet.2003.10.012 ↗
13. Kinetic model for TiO2 polymorphic transformation from anatase to rutile10.1111/j.1551-2916.2006.01369.x ↗
14. Experimental studies of oxide minerals
15. Particle size effects on transformation kinetics and phase stability in nanocrystalline TiO210.2138/am-1997-7-809 ↗
16. Thermodynamic analysis of phase stability of nanocrystalline titania10.1039/a802619j ↗
17. Kinetics study on phase transformation from titania polymorph brookite to rutile10.1016/j.jssc.2007.12.015 ↗
18. Grain size dependence of anatase-to-rutile structural transformation in gel-derived nanocrystalline titania powders10.1007/BF00275343 ↗
19. Phase transformation of nanocrystalline anatase-to-rutile via combined interface and surface nucleation10.1557/JMR.2000.0067 ↗
20. Understanding polymorphic phase transformation behavior during growth of nanocrystalline aggregates: insights from TiO210.1021/jp000499j ↗
21. On crystallite size dependence of phase stability of nanocrystalline TiO210.1063/1.1604966 ↗
22. Preparation and characterization of nanosized anatase TiO2 cuboids for photocatalysis10.1016/j.apcatb.2005.02.001 ↗
23. Polymorphic transformations and particle coarsening in nanocrystalline titania ceramic powders and membranes10.1021/jp067665t ↗
24. Rao CNR. Mechanism of crystal structure transformations Part 3 — factors affecting the anatase–rutile transformation10.1039/TF9625801579 ↗
25. The calcination of titania Part IV: the effect of additives on the anatase–rutile transformation
26. Anatase-to-rutile transition of titania thin films prepared by MOCVD10.1016/S0025-5408(96)00203-6 ↗
27. Low-temperature synthesis and microstructural control of titania nano-particles10.1016/j.jssc.2003.11.016 ↗
28. Anatase–rutile transition of precipitated titanium oxide with alcohol rising10.1006/jcis.1999.6607 ↗
29. Grain growth enhanced by anatase-to-rutile transformation in gel-derived nanocrystalline titania powders10.1016/S0925-8388(96)02583-2 ↗
30. Effect of hydrolysis conditions on thermal transformation of alkoxide-derived titanium dioxide10.2109/jcersj.101.230 ↗
31. Effect of brookite phase on the anatase–rutile transition in titania nanoparticles10.1016/S0955-2219(02)00194-2 ↗
32. Textural evolution and phase transformation in titania membranes: part 2 — supported membranes10.1039/JM9930301151 ↗
33. Variation of structural and optical properties of sol–gel TiO2 thin films with catalyst concentration and calcination temperature10.1016/S0167-577X(03)00380-X ↗
34. Preparation and phase transformation of anatase–rutile crystals in metal doped TiO2/muscovite nanocomposites10.1016/j.tsf.2005.05.035 ↗
35. The role of counterions (Mo, Nb, Sb, W) in Cr-, Mn-, Ni- and V-doped rutile ceramic pigments Part 1 Crystal structure and phase transformations10.1016/j.ceramint.2005.03.014 ↗
36. Effect of CuO on the sintering behavior and dielectric characteristics of titanium dioxide10.1111/j.1744-7402.2006.02106.x ↗
37. Effect of silver doping on the phase transformation and grain growth of sol–gel titania powder10.1016/S0955-2219(02)00356-4 ↗
38. Influence of manganese ions on the anatase–rutile phase transition of TiO2 prepared by the sol–gel process10.1016/S0167-577X(01)00600-0 ↗
39. Quantum-sized PbS, CdS, Ag2S, Sb2S3, and Bi2S3 particles as sensitizers for various nanoporous wide-bandgap semiconductors10.1021/j100063a022 ↗
40. A study of mixtures of HfO2 and TiO2 as high-k gate dielectrics10.1016/j.mee.2004.01.001 ↗
41. High-k gate dielectrics: current status and materials properties considerations10.1063/1.1361065 ↗
42. The high-k solution10.1109/MSPEC.2007.4337663 ↗
43. Dielectric resonator antennas
44. Layered Al2O3–TiO2 composite dielectric resonators with tuneable temperature coefficient for microwave applications10.1049/ip-smt:20000699 ↗
45. Microwave pulse compression using a periodically dielectric loaded dispersive waveguide section10.1080/02726340600710791 ↗
46. Microwave dielectric loss of titanium oxide10.1111/j.1151-2916.2000.tb01154.x ↗
47. 1995
48. Phase equilibria of the system Li2O–TiO210.1016/0025-5408(80)90248-2 ↗
49. Synthesis and CO2 absorption property of Li4TiO4 as a novel CO2 absorbent10.2109/jcersj.115.324 ↗
50. Crystal structure refinement of Li4TiO4 containing tetrahedrally coordinated Ti4+ and tetragonally packed oxide ions10.1006/jssc.1994.1266 ↗
51. Mise en evidence et etude cristallographique d'une nouvelle solution solide de type spinelle Li1+xTi2−xO4 0≤x≤0,33310.1016/0025-5408(71)90103-6 ↗
52. Kleykamp H. Phase equilibria in the Li–Ti–O system and physical properties of Li2TiO3. Fusion Eng Des 2002;61-62:361–6.10.1016/S0920-3796(02)00120-5 ↗
53. Bridgman–Stockbarger crystal growth of Li2Ti3O710.1016/0022-0248(79)90009-5 ↗
54. Quantitative analysis of anatase–rutile mixtures with an X-ray diffractometer10.1021/ac60125a006 ↗
55. The critical size mechanism for the anatase to rutile transformation in TiO2 and doped-TiO2.10.1016/j.jeurceramsoc.2005.03.246 ↗
56. ASTM D150-98 · 2004
57. Application Note 1217-1 · 1992
58. Jonker · 1957 · 413
59. High temperature superconductivity in the Li–Ti–O ternary system10.1016/0025-5408(73)90183-9 ↗
60. The defect structure of oxygen deficient rutile10.1007/BF01690050 ↗
61. Dielectric loss caused by oxygen vacancies in titania ceramics10.1016/j.jeurceramsoc.2008.06.019 ↗
62. Infrared absorption of reduced rutile TiO2 single crystals10.1103/PhysRev.113.1222 ↗
63. The effects of O deficiency on the electronic structure of rutile TiO2.10.1016/j.jpcs.2006.09.023 ↗
64. Characterization of insulating particles by dielectric spectroscopy: case study for CaCO3 powders10.1016/j.matlet.2005.03.066 ↗
65. Interfaces are the dominant feature of dielectrics at the nanometric level10.1109/TDEI.2004.1349779 ↗
66. Dervos · 2008
67. Mergos · 2006 · 744