Effects of Cu content on microstructure and mechanical properties of Al–14.5Si–0.5Mg alloy
Source abstract
Abstract
This study elucidates how Mg content affects the microstructure and mechanical properties of Al-14.5Si-4.5Cu alloy by adding 0.45 and 0.90 wt pct Mg. Primary silicon, eutectic silicon, acicular β-Al5FeSi, Al2Cu, and Al5Cu2Mg8Si6 phases were observed under the as-cast condition in low-Mg alloy. In high-Mg alloy, a large proportion of the acicular β-Al5FeSi phase was converted to Chinese script Al8Mg3FeSi6 phase. Neither the acicular β-Al5FeSi phase nor the Chinese script Al8Mg3FeSi6 phase dissolved in the Al matrix during solution heat treatment. Tensile testing indicates that T6-treated high-Mg alloy containing the Chinese script Al8Mg3FeSi6 phase is better than the T6-treated low-Mg alloy that contains the acicular β-Al5FeSi phase. The morphologies of Chinese script Al8Mg3FeSi6 and acicular β-Al5FeSi phases affect the tensile properties of Mg-containing Al-14.5Si-4.5Cu alloys. Additionally, high-Mg alloy contains a higher concentration of Mg solute atoms in the Al matrix than low-Mg alloy, and so the former contains more λ′ precipitates (Al5Cu2Mg8Si6) after T6-tempering treatment. The large amount of λ′ that precipitates in T6-treated high-Mg alloy may also enhance its tensile strength. The ultimate tensile strength (UTS) and elongation of the high-Mg alloy are superior to those of the low-Mg alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Influence of grain refinement and modification on microstructure and mechanical properties of Al–7Si and Al–7Si–2.5Cu cast alloys10.1016/j.matchar.2007.01.011 ↗
2. Characterization of the dissolution of the Al2Cu phase in two Al–Si–Cu–Mg casting alloys using calorimetry10.1016/S1044-5803(02)00283-8 ↗
3. Effect of Mg and Sr additions on the formation of intermetallics in Al–6wt pct Si–3.5wt pct Cu–(0.45) to (0.8) wt pct Fe 319-type alloy10.1007/s11661-998-0194-y ↗
4. Observations on the formation of β-Al5FeSi phase in 319 type Al–Si alloys10.1007/BF01159327 ↗
5. Modification of iron intermetallics by magnesium and strontium in Al–Si alloys10.1080/13640461.1997.11819229 ↗
6. Effects of solution temperature on mechanical properties of 319.0 aluminum casting alloys containing trace beryllium10.1557/JMR.2000.0291 ↗
7. Effects of Be and nonequilibrium heat treatment on mechanical properties of 319.0 alloys with 1.0% Fe10.1179/026708304225012107 ↗
8. Mechanical properties of Al–11%Si casting alloys containing trace Be and Sr10.2320/matertrans1989.40.294 ↗
9. Effects of Be and Fe content on plane strain fracture toughness in A357 alloys10.1007/BF02669650 ↗
10. Effects of beryllium on fatigue crack propagation of A357 alloys containing iron10.1016/0142-1123(95)00034-8 ↗
11. Effects of Be and Fe additions on the microstructure and mechanical properties of A357.0 alloys10.1007/BF02670615 ↗
12. Effect of iron in Al–Si casting alloys: a critical review
13. Age-hardening characteristics of Al–Si–Cu-base cast alloys
14. Influence of Cu on the mechanical properties and precipitation behavior of AlSi7Mg0.5 alloy during aging treatment10.1016/j.scriptamat.2005.08.044 ↗
15. Influence of Cu content on ageing behavior of AlSiMgCu cast alloys10.1016/j.matdes.2005.11.015 ↗
16. Effect of processing on the microstructural variation and heat-treatment response of a hypereutectic Al–Si alloy10.1016/0924-0136(95)01797-6 ↗
17. Hodgson · 1992 · 273
18. ASTM B557M-81, ASTM; 1991, Philadelphia, PA.
19. The effect of iron and manganese on the recrystallization behavior of hot-rolled and solution heat treated aluminum alloy 601310.1007/BF02647743 ↗
20. An approach for the aging process optimization of Al–Zn–Mg–Cu series alloys10.1016/j.matdes.2008.10.008 ↗
21. The effects of Mn additions on the microstructure and mechanical properties of Al–Si–Cu casting alloys10.1016/j.msea.2007.12.026 ↗