Solidification observations of vacuum arc melting processed Fe–Al–TiC composites: TiC precipitation mechanisms
Source abstract
Abstract
Abstract Fe22Al–5 wt.%TiC composite material has successfully synthesised by Vacuum Arc Melting (VAM) process. TiC crystals were formed by a dissolution–reprecipitation process of TiC powder added as precursor material. The solidification cooling rate alters the growth morphologies of the precipitated crystals. Jackson's classical crystal nucleation and growth theories were facilitated in order to explain the final TiC microstructure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Metallic Glasses and Amorphous Alloys · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Growth morphology and mechanism of primary TiC carbide in laser clad TiC/FeAl composite coating10.1016/S0167-577X(02)00964-3 ↗
2. Microstructure and wear resistance of laser clad TiC reinforced FeAl intermetallic matrix composite coatings10.1016/S0257-8972(02)00881-2 ↗
3. High temperature wear resistance of a laser clad TiC reinforced FeAl in situ composite coating10.1016/S0257-8972(03)00821-1 ↗
4. Eutectic MC carbide growth morphologies of a laser cald TiC/FeAl composite coating10.1016/j.matlet.2005.06.051 ↗
5. Growth morphologies and mechanisms of non-equilibrium solidified MC carbide10.1557/jmr.2006.0043 ↗
6. Growth morphology and mechanism of MC carbide under quasi-rapid solidification conditions10.1016/S1468-6996(01)00044-4 ↗
7. Growth morphologies and mechanism of TiC in a laser surface alloyed coating on the substrate of TiAl intermetallics10.1016/S0925-8388(02)01077-0 ↗
8. Rapidly solidified MC carbide morphologies of a pulsed laser surface alloyed γ-TiAl intermetallic with carbon10.1016/j.scriptamat.2003.10.028 ↗
9. Microstructure and wear resistance of laser-melted TiC reinforced nickel aluminide dual-phase matrix in situ composite10.1016/j.intermet.2005.06.011 ↗
10. Laser melted TiC reinforced nickel aluminide matrix in situ composites10.1016/j.jallcom.2004.08.066 ↗
11. Rapidly solidified MC carbide morphologies of a laser-glazed single-crystal nickel-base superalloy10.1016/0921-5093(92)90421-V ↗
12. Gradient microstructure in laser clad TiC-reinforced Ni-alloy composite coating10.1016/S0921-5093(97)00501-7 ↗
13. Effect of solidification conditions on MC carbides in a Nickel-base superalloy in 738 LC10.1016/0956-716X(94)90434-0 ↗
14. Transmission electron microscope studies of TiC crystals10.1002/1521-4079(200011)35:11/12<1295::AID-CRAT1295>3.0.CO;2-H ↗
15. Microstructure of TiC crystals obtained form high temperature nickel solution10.1016/S0925-8388(02)00955-6 ↗
16. Solidification processing and tribological behaviour of particulate TiC-ferrous matrix composites10.1016/0921-5093(90)90232-R ↗
17. Iron aluminides: present status and future prospects10.1016/S0921-5093(98)00909-5 ↗
18. Concepts derived form phase diagram studies for the strengthening of Fe–Al based alloys10.1016/j.intermet.2004.10.015 ↗
19. Effect of Ti substitution on the structure and properties of Fe3Al-based intermetallic alloys10.1007/BF00357866 ↗
20. Thermal distribution in electrical arc welding of tungsten inert gas (TIG) process
21. DO3-B2-α phase relations in Fe–Al–Ti alloys10.1007/BF02649468 ↗
22. Phase equilibria, phases and chemical compounds in the Ti–C system10.1070/RC2002v071n06ABEH000721 ↗
23. Order and disorder in transition metal carbides and nitrides: experimental and theoretical aspects10.1351/pac198557101391 ↗
24. Calculation of the Ti–C, W–C and Ti–W–C phase diagrams10.1016/0364-5916(84)90001-4 ↗
25. Crystal growth kinetics10.1016/0025-5416(84)90194-0 ↗
26. The interface kinetics of crystal growth processes10.1023/A:1015824230008 ↗
27. TiC particulate-reinforced Al–20Si–5Fe composite fabricated by melt in situ reaction spray forming10.1016/S0924-0136(02)01094-4 ↗
28. Effect of growth rate dependent partition coefficient on the dendritic growth of undercooled melts10.1016/0001-6160(87)90175-1 ↗
29. Rapid dendrite growth in undercooled melts10.1016/0001-6160(87)90174-X ↗