journal article·2017-03

Evolution of precipitates in a Cu-containing alumina-forming austenitic steel after short-term mechanical tests

Bingbing Zhao, Jifu Fan, Ze Chen, Xianping Dong, Feng Sun, Lanting Zhang

Publisher page

Abstract

Abstract Tensile tests at room temperature and 700 °C under different strain rates were performed on a Cu-containing alumina-forming austenitic (AFA) steel subject to 0–10% pre-strains after the same thermal-mechanical treatment. The sample with 3% pre-strain showed the longest equilibrium stage of strain hardening and dynamic recovery during testing at 700 °C and its creep/rupture life doubled compared to the unstrained condition. Both MC carbide precipitates and L1 2 -ordered precipitates were refined after creep/rupture at 700 °C for 50 h when dislocations introduced by pre-strain acted as nucleation sites. Precipitation kinetics showed that both L1 2 -ordered phase and MC carbides almost completed during the first 50 h of creep/rupture. The evolution of MC and L1 2 -ordered precipitates during tensile tests at sufficiently low strain rate makes it possible to correlate the strain hardening plateau length at dσ / de p ≈ 0 with the creep/rupture life. Thus, tensile tests at low strain rate can act as a guide to set an appropriate pre-treatment in alloy development.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels10.1007/s11661-010-0295-2 ↗
2. Creep-resistant, Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
3. Alloying effects on creep and oxidation resistance of austenitic stainless steel alloys employing intermetallic precipitates10.1016/j.intermet.2007.12.005 ↗
4. Effects of silicon additions on the oxide scale formation of an alumina-forming austenitic alloy10.1016/j.corsci.2012.08.039 ↗
5. Plastic flow behaviour in an alumina-forming austenitic stainless steel at elevated temperatures10.1016/j.msea.2013.11.021 ↗
6. Orientation relationships of Laves phase and NiAl particles in an AFA stainless steel10.1080/14786435.2015.1111529 ↗
7. Austenite grain growth in alumina-forming austenitic steel10.1557/jmr.2016.178 ↗
8. Protection of zirconium by alumina- and chromia-forming iron alloys under high-temperature steam exposure10.1016/j.jnucmat.2013.03.006 ↗
9. The effects of water vapor on the oxidation behavior of alumina forming austenitic stainless steels10.1007/s11085-015-9581-0 ↗
10. Evolution of microstructure and tensile properties of Fe–18Ni–12Cr based AFA steel during aging at 700°C10.1016/j.msea.2016.06.060 ↗
11. Precipitation sequence and its effect on age hardening of alumina-forming austenitic stainless steel10.1016/j.msea.2015.08.005 ↗
12. Precipitation kinetics during aging of an alumina-forming austenitic stainless steel10.1016/j.msea.2016.04.081 ↗
13. Co-optimization of wrought alumina-forming austenitic stainless steel composition ranges for high-temperature creep and oxidation/corrosion resistance10.1016/j.msea.2013.10.014 ↗
14. The negative effect of Zr addition on the high temperature strength in alumina-forming austenitic stainless steels10.1016/j.matchar.2013.10.029 ↗
15. Effect of tungsten addition on high-temperature properties and microstructure of alumina-forming austenitic heat-resistant steels10.1016/j.msea.2015.09.018 ↗
16. Micro-alloying effects of yttrium on recrystallization behavior of an alumina-forming austenitic stainless steel10.1016/S1006-706X(16)30087-5 ↗
17. Development of L1(2)-ordered Ni-3(Al,Ti)-strengthened alumina-forming austenitic stainless steel alloys10.1016/j.scriptamat.2013.09.005 ↗
18. Formation of L12-ordered precipitation in an alumina-forming austenitic stainless steel via Cu addition and its contribution to creep/rupture resistance10.1016/j.scriptamat.2015.07.019 ↗
19. Annealing effects on precipitation and high-temperature properties of a Cu-containing alumina-forming austenitic steel10.1016/j.matlet.2016.04.110 ↗
20. Accelerated precipitation in the AFA stainless steel Fe–20Cr–30Ni–2Nb–5Al via cold working10.1016/j.intermet.2014.04.018 ↗
21. The effect of thermo-mechanical treatment on the high temperature tensile behavior of an alumina-forming austenitic steel10.1016/j.msea.2015.11.036 ↗
22. Alumina-forming austenitic stainless steels strengthened by Laves phase and MC carbide precipitates10.1007/s11661-007-9319-y ↗
23. Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels10.1007/s11661-009-9886-1 ↗
24. The influence of pre-compression on the creep deformation and failure behaviour of type 316H stainless steel10.1016/j.engfracmech.2013.08.006 ↗
25. Effect of prestrain on fracture toughness of HSLA steels10.1016/S0921-5093(00)00739-5 ↗
26. Effect of prestrain on the ductile fracture behavior of an interstitial-free steel10.1007/s11661-006-1049-z ↗
27. Schnellbestimmung des Krieverhaltens von Aluminium-Gusswerkstoffen durch Warm-Kriegzugversuche
28. Combined effect of Co and W on deformation resistance of 12Cr heat-resistant steel for USC steam turbines10.1007/s11665-010-9806-y ↗
29. Creep life assessment by low strain rate tensile testing10.1016/0308-0161(83)90015-7 ↗
30. Deformation mechanism diagrams with the strain rate as a coordinate10.1016/0025-5416(80)90148-2 ↗
31. Competition between work-hardening effect and dynamic-softening behavior for processing as-cast GH4720Li superalloys with original dendrite microstructure during moderate-speed hot compression10.1016/j.msea.2015.07.007 ↗
32. Plastic pre-compression and creep damage effects on the fracture toughness behaviour of type 316H stainless steel10.1016/j.engfracmech.2014.10.005 ↗