journal article·2012-06

Microstructural evolution of P92 ferritic/martensitic steel under Ar+ ion irradiation at elevated temperature

Shuoxue Jin, Liping Guo, Tiecheng Li, Jihong Chen, Zheng Yang, Fengfeng Luo, Rui Tang, Yanxin Qiao, Feihua Liu

Publisher page

Abstract

Irradiation damage in P92 ferritic/martensitic steel irradiated by Ar{sup +} ion beams to 7 and 12 dpa at elevated temperatures of 290 Degree-Sign C, 390 Degree-Sign C and 550 Degree-Sign C has been investigated by transmission electron microscopy, scanning electron microscopy and atomic force microscopy. The precipitate periphery (the matrix/carbide interface) was amorphized only at 290 Degree-Sign C, while higher irradiation temperature could prevent the amorphization. The formation of the small re-precipitates occurred at 290 Degree-Sign C after irradiation to 12 dpa. With the increase of irradiation temperature and dose, the phenomenon of re-precipitation became more severe. The voids induced by irradiation were observed after irradiation to 7 dpa at 550 Degree-Sign C, showing that high irradiation temperature ({>=} 550 Degree-Sign C) was a crucial factor which promoted the irradiation swelling. Energy dispersive X-ray analysis revealed that segregation of Cr and W in the voids occurred under irradiation, which may influence mechanical properties of P92 F/M steel. - Graphical Abstract: High density of small voids, about 2.5 nm in diameter, was observed after irradiation to 12 dpa at 550 Degree-Sign C, which was shown in panel a (TEM micrograph). As shown in panel b (SEM image), a large number ofmore » nanometer-sized hillocks were formed in the surface irradiated at 550 Degree-Sign C, and the mean size was {approx} 30 nm. The formation of the nanometer-sized hillocks might be due to the voids that appeared as shown in TEM images (panel a). High irradiation temperature ({>=} 550 Degree-Sign C) was a crucial factor for the formation of void swelling. Highlights: Black-Right-Pointing-Pointer Small carbides re-precipitated in P92 matrix irradiated to 12 dpa at 290 Degree-Sign C. Black-Right-Pointing-Pointer High density of voids was observed at 550 Degree-Sign C. Black-Right-Pointing-Pointer Segregation of Cr and W in voids occurred under irradiation.« less
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Serrated flow behavior in AL6XN austenitic stainless steel10.1016/j.jnucmat.2009.08.002 ↗
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. Tensile and stress corrosion cracking behavior of ferritic–martensitic steels in supercritical water10.1016/j.jnucmat.2009.09.012 ↗
4. Irradiation-assisted stress corrosion cracking of austenitic alloys in supercritical water10.1016/j.jnucmat.2009.09.010 ↗
5. Influence of strain rate on P92 microstructural stability during fatigue tests at high temperature10.1016/j.proeng.2010.03.230 ↗
6. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
7. Microstructural evolution of P92 ferritic/martensitic steel under argon ion irradiation10.1016/j.matchar.2010.11.015 ↗
8. Mechanical and microstructural stability of P92 steel under uniaxial tension at high temperature10.1016/j.msea.2010.03.001 ↗
9. Creep rupture behaviour of P92 steel weldment10.1016/j.engfailanal.2010.08.020 ↗
10. High temperature low cycle fatigue behaviour of P92 tungsten added 9Cr steel10.1007/s12666-010-0084-z ↗
11. Microstructural stability and creep rupture strength of the martensitic steel P92 for advanced power plant10.1016/S1359-6454(97)00176-6 ↗
12. Void swelling in a 9Cr ferritic/martensitic steel irradiated with energetic Ne-ions at elevated temperatures10.1016/j.jnucmat.2007.11.009 ↗
13. Structural characterization of TiN coatings on Si substrates irradiated with Ar ions10.1016/j.matchar.2009.07.002 ↗
14. Microstructural changes in a low-activation Fe–Cr–Mn alloy irradiated with 92MeV Ar ions at 450degrees C10.1016/S0022-3115(00)00207-5 ↗
15. Standard practice for neutron radiation damage simulation by charged-particle irradiation, ASTM designation E 521-89
16. Phase evolution in P92 and E911 weld metals during ageing10.1016/j.msea.2007.07.036 ↗
17. Substructure stability of highly alloyed martensitic steels for power industry10.1016/S0254-0584(03)00047-6 ↗
18. Structural evolution in modified 9Cr–1Mo ferritic/martensitic steel irradiated with mixed high-energy proton and neutron spectra at low temperatures10.1016/S0022-3115(02)01198-4 ↗
19. Radiation induced phase instability of precipitates in reduced-activation ferritic/martensitic steels10.1016/j.jnucmat.2007.03.155 ↗
20. Microstructure in martensitic steels T91 and F82H after irradiation in SINQ target-310.1016/S0022-3115(03)00101-6 ↗
21. The impact of irradiation temperature on the microstructure of F82H martensitic/ferritic steel irradiated in a proton and neutron mixed spectrum10.1016/S0022-3115(02)00916-9 ↗
22. Irradiation-induced precipitates in a neutron irradiated 304 stainless steel studied by three-dimensional atom probe10.1016/j.jnucmat.2011.07.027 ↗
23. Influence of boron on radiation enhanced diffusion of antimony in delta-doped silicon10.1063/1.1448896 ↗
24. Hydrogenation of platinum introduced in silicon by radiation enhanced diffusion10.1016/j.mseb.2008.11.038 ↗
25. Effect of triple ion beams in ferritic/martensitic steel on swelling behavior10.1016/S0022-3115(02)01076-0 ↗
26. Effect of irradiation temperature on void swelling of China Low Activation Martensitic steel (CLAM)10.1016/j.matchar.2007.01.014 ↗
27. Effect of gas atoms and displacement damage on mechanical properties and microstructures of F82H10.1016/j.jnucmat.2006.05.032 ↗
28. irradiation damage behavior of aging precipitated carbide in Fe–Cr–Mn steel
29. Microstructural evolution of the China Low Activation Martensitic (CLAM) steel irradiated by H and He ion beams10.1016/j.nimb.2009.06.073 ↗
30. Irradiation-induced grain boundary chromium microchemistry in high alloy ferritic steels10.1016/j.scriptamat.2008.01.004 ↗
31. Efficient annealing of radiation damage near grain boundaries via interstitial emission10.1126/science.1183723 ↗
32. Jin S, Guo L, Yang Z, Zhou Z, Fu D, Liu C, et al. Structural Characterization of Nickel-base Alloy C-276 irradiated with Ar ions. Plasma Sci Technol in press.