journal article·2006-06

Investigation of hydrogen induced cracking in 2205 duplex stainless steel in wet H2S environments after isothermal treatment at 675, 750 and 900°C

Maria Sozańska, Katarzyna Kłyk-Spyra

Materials Characterization· Volume 56· Issue 4-5
Publisher page

Abstract

The effect of isothermal treatment (at 675, 750 and 900 deg. C) on HIC (hydrogen induced cracking) in sour environments containing hydrogen sulphide of a 2205 duplex stainless steel has been investigated. The performance and microstructure of failed material were characterized by optical microscopy, scanning electron microscopy and also X-ray diffraction. Two kinds of Cr-, Mo-enriched intermetallic phases, {sigma} and {chi}, were found to precipitate preferentially at {alpha}/{gamma} interfaces and within {alpha} grains after different times of aging in the temperature range of 650-900 deg. C. After performing tests according to the NACE Standard TM 0284 (1987) the specimens were investigated by using quantitative metallography methods. The volume fraction of {sigma} phase was changed with the time of aging and {sigma} phase developed into coarse particles due to the high diffusibility of solute atoms at high temperatures. The variation of size and shape of {sigma} phase particles was obtained by applying different heat treatment conditions to 2205 steel specimens. The results showed that 2205 duplex stainless steel containing nearly 12 vol.% of {sigma} phase in dispersed conditions was resistant to step cracking in wet environments containing hydrogen sulphide. It was highly possible that a crack would propagate faster along themore » embrittled {sigma} phase. However, very small cracks were found at austenite-ferrite boundaries where o phase particles were also present.« less
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Materials to meet your needs
2. Effect of isothermal treatment of SAF 2205 duplex stainless steel on migration of δ/γ interface boundary and growth of austenite10.1016/S0925-8388(99)00014-6 ↗
3. Ravindranath K, Malhotram SN. The influence of aging on the intergranular corrosion of 22 chromium-5 nickel duplex stainless steel. Corros Sci 1995;37:12l–32.10.1016/0010-938X(94)00120-U ↗
4. Effects of solution treatment and continuous cooling on σ-phase precipitation in a 2205 duplex stainless steel10.1016/S0921-5093(01)00911-X ↗
5. Effect of 475°C embrittlement on fractal behavior and tensile properties of duplex stainless steel10.1361/105994999770347214 ↗
6. Corrosion resistance of super duplex stainless steels in chloride ion containing environments: investigations by means of a new microelectrochemical method: II. Influence of precipitates10.1016/S0010-938X(00)00088-3 ↗
7. Influence of σ-phase on mechanical properties and corrosion resistance of duplex stainless steels10.1016/S0010-938X(99)00009-8 ↗
8. Preferential precipitation site of sigma phase in duplex stainless steel weld metal10.1016/S1359-6462(98)00483-7 ↗
9. Thomas · 1994
10. Shek · Mater Sci Eng · 1999 · 231 · 4210.1016/S0921-5093(97)00077-4 ↗
11. Vander Voort GF. Metallography: Principles and Practice, ASM Inter., McGraw-Hill Inc; 1999.
12. Szala J, MetIlo, v 3.01 Authorized programs, Silesian University of Technology, Department of Materials Science; 2003.
13. Stereologia materiałów