journal article·2009-12

Metallurgical investigation of the aging process on tensile fracture welded joints in pipeline steel

B. Vargas-Arista, C. Angeles-Chavez, A. Albiter, J.M. Hallen

Materials Characterization· Volume 60· Issue 12
Publisher page

Abstract

The effects of aging in the tensile fracture behavior of welded joints of API5L-X52 pipe steel were studied by accelerating aging at 250 °C for different periods of time. The weld metal, heat affected zone and base metal, showed an increase in yield strength while the strain-hardening exponent decreased at early stages of aging. A maximum strength and minimum hardening exponent was found at 500 h due to peak-aging. Subsequently, both properties exhibited an opposite behavior due to over-aging. Tensile fractured specimens for the three different zones exhibited ductile failure, presenting microvoid morphology associated with the coalescence of microcavities. An increase in void density and a reduction in diameter during short periods in the fractured specimens were observed. The maximum density and minimum diameter of voids were obtained at 500 h and were linked to the improvement of strength and precipitation of nanoparticles. Afterward, the fractured surfaces exhibited a reduction in density and the diameters of voids were larger, having been induced by the deterioration of strength and coarsening of particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Sharma U, Ivey GD. Microstructure of microalloyed line pipe steels. Proc Int Conf on Pipeline ASME. Calgary, Alberta, Canada, October 1–5; 2000;1:193–201.
2. Leslie · 1982 · 79
3. Investigation of the age hardening behaviour of 6063 aluminium alloys refined with Ti, RE and B10.1016/j.jmatprotec.2008.02.007 ↗
4. Effect of the artificial aging on the microstructure of weldment on API 5L X-52 steel pipe10.1016/j.matchar.2006.11.004 ↗
5. Effect of long-term service on the tensile properties and capability of pipeline steel 17GS to resist cleavage fracture10.1016/j.ijpvp.2004.02.015 ↗
6. Effect of stress on microstructural change due to aging at 823K in multi-layer welded joint of 2.25Cr-1mo steel10.1016/j.ijpvp.2003.12.017 ↗
7. Effect of pre-deformation on the age hardening of a niobium-microalloyed steel10.1016/j.matlet.2005.02.014 ↗
8. Fracture toughness of cold worked and simulated heat affected structural steel10.1016/S0013-7944(97)00100-8 ↗
9. API Standard 1104 · 2007 · 2
10. API Specification 5L · 2008 · 23
11. ASTM Standard E-8M · 2008 · 7
12. ASTM Standard E-646 · 2007 · 2
13. Evans · 1997 · 148
14. Effect of TiO2-containing fluxes on the mechanical properties and microstructure in submerged-arc weld steels10.1016/j.matchar.2008.06.003 ↗
15. Ju JB, Jang JI, Kim SW, Kwon D. The effect of microstructural change on fracture behavior in heat-affected zone of API-5L X65 pipeline steel. Proc Int Conf on Pipeline ASME. Calgary, Alberta, Canada, October 1–5; 2000;1: 169–75.
16. Plastic strain distribution underneath a Vickers indenter: role of yield strength and work hardening exponent10.1016/j.actamat.2006.06.032 ↗
17. Dieter · 1988 · 286
18. Garcés CY, Sáenz AL. Evaluación de la tenacidad a fractura del acero microaleado X-60 sometido a un tratamiento térmico de envejecimiento. VIII Congreso Iberoamericano en Metalurgia y Materiales. Quito, Ecuador, May 24–28; 2004: 478–86.
19. 1992 · 97
20. Effect of alternative aging process on the fracture and interfacial properties of particulate Al2O3-reinforced Al (6061) metal matrix composite10.1007/s11661-002-0179-1 ↗
21. Aplicación del ensayo miniatura de embutido para la evaluación de la tenacidad a temperaturas criogenicas de aceros inoxidables austeniticos envejecidos isotermicamente10.3989/revmetalm.2003.v39.i5.350 ↗
22. Effect of the artificial aging time on the mechanical properties of weldment on API 5L X-52 line pipe steel10.1007/BF02586102 ↗
23. Coarsening kinetics of TiN particle in a low alloyed steel in weld HAZ: considering critical particle size10.1016/j.actamat.2005.10.037 ↗