Abstract
Abstract An extruded AZ31B (Mg-3Al-1Zn-0.5Mn) magnesium alloy with a twin volume fraction of 60% was subjected to fully reversed strain-controlled tension-compression along the extrusion direction at strain amplitudes ranging from 0.23% to 0.45%. Dislocation slips were the dominant plastic deformation mechanisms without involving persistent twinning-detwinning. At an identical strain amplitude, the fatigue life of the pre-twinned alloy was much lower than that of the as-extruded alloy. Fatigue cracks were mainly initiated on the prismatic or prismatic-basal slip bands in the parent grains. The material volume reduction of the parent grains in the pre-twinned alloy enhanced fatigue damage. Twin cracks were not observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Fatigue of magnesium alloys10.1146/annurev.ms.20.080190.001041 ↗
2. Magnesium alloys and applications10.1179/mst.1994.10.1.1 ↗
3. Strain controlled cyclic deformation behavior of an extruded magnesium alloy10.1016/j.msea.2008.05.016 ↗
4. Multiaxial fatigue of extruded AZ31B magnesium alloy10.1016/j.msea.2012.03.039 ↗
5. Effect of forging on the low cycle fatigue behavior of cast AZ31B alloy10.1016/j.msea.2017.08.086 ↗
6. Dependence of the distribution of deformation twins on strain amplitudes in an extruded magnesium alloy after cyclic deformation10.1016/j.msea.2009.04.048 ↗
7. Fatigue deformation characteristic of as-extruded AM30 magnesium alloy10.1016/j.matdes.2009.08.042 ↗
8. Role of loading direction on cyclic behaviour characteristics of AM30 extrusion and its fatigue damage modelling10.1016/j.msea.2016.05.116 ↗
9. Twinning-detwinning behavior during the strain-controlled low-cycle fatigue testing of a wrought magnesium alloy, ZK60A10.1016/j.actamat.2007.10.030 ↗
10. Internal stress relaxation and load redistribution during the twinning-detwinning-dominated cyclic deformation of a wrought magnesium alloy, ZK60A10.1016/j.actamat.2008.04.006 ↗
11. An experimental study on cyclic deformation and fatigue of extruded ZK60 magnesium alloy10.1016/j.ijfatigue.2011.08.016 ↗
12. Anisotropy in the quasi-static and cyclic behavior of ZK60 extrusion: characterization and fatigue modeling10.1016/j.matdes.2018.10.026 ↗
13. Cyclic deformation and fatigue of extruded Mg-Gd-Y magnesium alloy10.1016/j.msea.2012.10.048 ↗
14. Analysis of fatigue damage process in magnesium alloy AZ3110.1016/j.msea.2008.10.034 ↗
15. Hardening evolution of AZ31B Mg sheet10.1016/j.ijplas.2006.03.005 ↗
16. Role of persistent slip bands in fatigue10.1080/14786430310001610339 ↗
17. Structure-property relations of cyclic damage in a wrought magnesium alloy10.1016/j.scriptamat.2010.05.048 ↗
18. In-situ observations of high cycle fatigue mechanisms in cast AM60B magnesium in vacuum and water vapor environments10.1016/S0142-1123(03)00079-3 ↗
19. A study of fatigue damage development in extruded Mg-Gd-Y magnesium alloy10.1016/j.msea.2013.09.089 ↗
20. Effects of pre-tension on fatigue behavior of rolled magnesium alloy10.1016/j.msea.2016.10.117 ↗
21. Crack initiation mechanism of extruded AZ31 magnesium alloy in the very high cycle fatigue regime10.1016/j.msea.2008.02.003 ↗
22. Effect of strain ratio on cyclic deformation and fatigue of extruded AZ61A magnesium alloy10.1016/j.ijfatigue.2012.04.013 ↗
23. Role of initial {1 0-1 2} twin in the fatigue behavior of rolled Mg-3Al-1Zn alloy10.1016/j.scriptamat.2010.01.021 ↗
24. Effect of initial twins on the stress-controlled fatigue behavior of rolled magnesium alloy10.1016/j.msea.2016.10.093 ↗
25. Fatigue damage development in extruded Mg-3Al-Zn magnesium alloy10.1016/j.msea.2016.05.009 ↗
26. Cyclic deformation and fatigue of extruded AZ31B magnesium alloy under different strain ratios10.1016/j.msea.2015.09.084 ↗
27. Twinning behaviors of a rolled AZ31 magnesium alloy under multidirectional loading10.1016/j.matchar.2016.11.046 ↗
28. Characteristic cyclic plastic deformation in ZK60 magnesium alloy10.1016/j.ijplas.2017.01.005 ↗
29. Cyclic deformation and fatigue damage in single-crystal magnesium under fully reversed strain-controlled tension-compression in the [100] direction10.1016/j.scriptamat.2014.10.020 ↗
30. Modeling inelastic behavior of magnesium alloys during cyclic loading-unloading10.1016/j.ijplas.2013.01.007 ↗
31. Study of slip mechanisms in a magnesium alloy by neutron diffraction and modeling10.1016/S1359-6462(02)00591-2 ↗
32. Cold rolling textures in AZ31 wrought magnesium alloy10.1016/j.scriptamat.2004.01.010 ↗
33. Cyclic deformation and fatigue of rolled AZ80 magnesium alloy along different material orientations10.1016/j.msea.2016.09.031 ↗
34. Reorientation and stress relaxation due to twinning: modeling and experimental characterization for Mg10.1016/j.actamat.2008.01.057 ↗
35. In situ neutron diffraction investigation of deformation twinning and pseudoelastic-like behaviour of extruded AZ31 magnesium alloy10.1016/j.ijplas.2008.08.002 ↗
36. Roles of deformation twinning and dislocation slip in the fatigue failure mechanism of AZ31 Mg alloys10.1016/j.scriptamat.2010.03.021 ↗
37. The crack initiation mechanism of the forged Mg-Zn-Y-Zr alloy in the super-long fatigue life regime10.1016/j.scriptamat.2006.09.006 ↗