The effect of hydrogen on the crack initiation site of TRIP-assisted steels during in-situ hydrogen plasma micro-tensile testing: Leading to an improved ductility?
Source abstract
Abstract
Abstract The hydrogen induced damage and crack initiation in transformation induced plasticity (TRIP) steel is considered in the present work by micro tensile testing and subsequent microstructural assessment. Hydrogen characteristics are studied for two material conditions for this purpose, i.e. TRIP 0% and TRIP 15%. To increase, on the one hand, microstructural defects such as dislocations, and on the other hand, to provoke the strain induced phase transformation of retained austenite to fresh martensite, cold deformation of 15% is applied (TRIP 15%) and compared to the as-received material (TRIP 0%). Both electrochemical charging and hydrogen plasma charging is done compared to uncharged tensile specimens, as reference. A hydrogen induced ductility loss is found when the samples are hydrogen charged electrochemically, whereas plasma charging remarkably induces a ductility increase. A comprehensive hydrogen assisted crack analysis by environmental scanning electron microscopy reveals that the uncharged and electrochemically charged specimens show crack initiation in the martensitic regions, whereas plasma charging results into crack initiation in the soft, crack arresting ferritic matrix. Furthermore, the hydrogen effect is for both charging methods more pronounced after cold deformation, which is correlated to hydrogen trapping ability of the deformation induced defects, as verified by thermal desorption spectroscopy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
2. HE understood10.1007/s11663-015-0325-y ↗
3. Effect of in-situ hydrogen charging on the mechanical properties of advanced high strength steels10.1016/j.ijhydene.2013.12.190 ↗
4. Hydrogen embrittlement of the equi-molar FeNiCoCr alloy10.1016/j.actamat.2018.07.032 ↗
5. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
6. Clean energy and the hydrogen economy10.1098/rsta.2016.0400 ↗
7. van Wijk · 2017
8. Hydrogen embrittlement in HSSs limits use in lightweight body
9. Fractographic analysis of the role of hydrogen diffusion on the hydrogen embrittlement susceptibilty of DP steel10.1016/j.msea.2015.09.124 ↗
10. Characterization of hydrogen induced cracking in TRIP-assisted steels10.1016/j.ijhydene.2015.06.017 ↗
11. Microstructural characterization of hydrogen induced cracking in TRIP-assisted steel by EBSD10.1016/j.matchar.2015.12.017 ↗
12. EBSD characterization of hydrogen induced blisters and internal cracks in
13. Structure–properties relationship in TRIP steels containing carbide-free bainite10.1016/j.cossms.2004.10.002 ↗
14. The solubility and diffusivity of hydrogen in well-annealed and deformed iron10.1016/0001-6160(83)90192-X ↗
15. Modelling of hydrogen diffusion and hydrogen induced cracking in supermartensitic and duplex stainless steels10.1016/j.matdes.2008.04.026 ↗
16. The effect of a constant tensile load on the hydrogen diffusivity in dual phase steel by electrochemical permeation experiments
17. Combined thermal desorption spectroscopy, differential scanning calorimetry, scanning electron microscopy and X-ray diffraction study of hydrogen trapping in cold deformed TRIP steel10.1016/j.actamat.2012.01.026 ↗
18. First observation by EBSD of martensitic transformations due to hydrogen presence during straining of duplex stainless steel10.1016/j.matchar.2019.109843 ↗
19. In-situ observation of martensitic transformation in an interstitial metastable high-entropy alloy during cathodic hydrogen charging10.1016/j.scriptamat.2019.07.042 ↗
20. Hydrogen embrittlement studies of a TRIP steel10.1007/BF02648707 ↗
21. Hydrogen trapping ability of steelswith differentmicrostructures10.1080/02533839.1999.9670440 ↗
22. The detrimental effect of mobile hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism
23. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
24. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
25. Multiscale modeling of hydrogen enhanced homogeneous dislocation nucleation10.1016/j.actamat.2016.01.036 ↗
26. Determination of the equivalent hydrogen fugacity during electrochemical charging of 3.5NiCrMoV steel10.1016/j.corsci.2017.12.018 ↗
27. Electrochemical and mechanical aspects of hydrogen embrittlement evaluation of martensitic steels
28. Recent developments in the study of hydrogen embrittlement: hydrogen effect on dislocation nucleation10.1016/j.actamat.2010.05.057 ↗
29. Effect of hydrogen on nanomechanical properties in Fe22Mn-0.6C TWIP steel revealed by in-situ electrochemical nanoindentation
30. Critical assessment of the evaluation of thermal desorption spectroscopydata for duplex stainless steels: a combined experimental and numerical approach10.1016/j.actamat.2019.12.055 ↗
31. Hydrogen diffusivity and tensile-ductility loss of solution-treated austenitic stainless steels with external and internal hydrogen10.1016/j.ijhydene.2017.04.055 ↗
32. Comparative study of hydrogen embrittlement in stable and metastable high-entropy alloys10.1016/j.scriptamat.2018.03.003 ↗
33. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗
34. On the environmental similitude for fracture in the SENT specimen and a cracked hydrogen gas pipeline10.1016/j.engfracmech.2011.06.002 ↗
35. Hydrogen embrittlement effect observed by in-situ hydrogen plasma charging on a ferritic alloy10.1016/j.scriptamat.2018.03.038 ↗
36. Assessment of the potential of hydrogen plasma charging as compared to conventional electrochemical hydrogen charging on dual phase steel10.1016/j.msea.2019.03.097 ↗
37. Hydrogen embrittlement of commercially produced advanced high strength sheet steels10.4271/2010-01-0447 ↗
38. In situ small-scale hydrogen embrittlement testing made easy: an electrolyte for preserving surface integrity at nano-scale during hydrogen charging10.1016/j.ijhydene.2018.04.168 ↗
39. Hydrogen trapping phenomena in metals with bcc and fcc crystal structures by the desorption thermal-analysis technique10.1016/0257-8972(86)90087-3 ↗
40. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
41. On the synergy of diffusible hydrogen content and hydrogen diffusivity in the mechanical degradation of laboratory cast Fe-C alloys10.1016/j.msea.2016.03.107 ↗
42. Evaluation of the hydrogen embrittlement susceptibility in DP steel under static and dynamic tensile conditions10.1016/j.ijimpeng.2018.10.002 ↗
43. Discerning enhanced dislocation plasticity in hydrogen-charged α-iron nano-crystals10.1080/21663831.2015.1052889 ↗
44. Hydrogen effects against hydrogen embrittlement10.1007/s11661-010-0275-6 ↗
45. Solid solution softening and hardening by mobile solute atoms with special focus on hydrogen10.1016/j.scriptamat.2012.07.022 ↗
46. Hydrogen embrittlement of an interstitial equimolar high-entropy alloy10.1016/j.corsci.2018.03.040 ↗
47. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
48. Classification of hydrogen trapping in steel10.1007/BF02812023 ↗
49. Trap-governed hydrogen diffusivity and uptake capacity in ultrahigh strength aermet 100 steel10.1007/s11661-002-0032-6 ↗
50. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
51. Evaluation of the role of Mo2C in hydrogen induced ductility loss in Q&T Fe-C-Mo alloys10.1016/j.ijhydene.2016.05.176 ↗
52. Hydrogen effects in prestrained transformation induced plasticity steel10.1007/s11661-011-1075-3 ↗
53. Characterization of hydrogen embrittlement in automotive advanced high strength steels
54. Comparison of damage development depending on the local microstructure in low alloyed Al-TRIP-steels, IF steel and a DP steel10.3139/146.110062 ↗
55. Effects of cryogenic and tempered treatment on the hydrogen embrittlement susceptibility of TRIP-780 steels10.1016/j.ijhydene.2013.05.113 ↗
56. Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel10.1016/j.actamat.2012.04.010 ↗
57. Effects of deformation induced phase transformation and twinning on the mechanical properties of austenitic Fe-Mn-Al alloys10.2355/isijinternational.29.868 ↗
58. The influence of hydrogen on the stacking fault energy of an austenitic stainless steel10.1002/pssb.19640070241 ↗
59. Stacking fault energy decrease in austenitic stainless steels induced by hydrogen pairs formation10.1016/S1359-6462(98)00285-1 ↗
60. X-ray diffraction measurement of the stacking fault energy reduction induced by hydrogen in an AISI 304 steel10.1016/S1359-6462(97)00332-1 ↗
61. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(99)00094-6 ↗
62. Direct observations of martensite nuclei in stainless steel10.1016/0001-6160(79)90074-9 ↗
63. A review of the influence of hydrogen on the mechanical properties of DP, TRIP, and TWIP advanced high-strength steels for auto construction10.1515/corrrev-2015-0083 ↗
64. High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development - properties - application10.1016/S0749-6419(00)00015-2 ↗