Microstructure evolution and fracture behavior of Mg-9.5Gd-0.9Zn-0.5Zr alloy subjected to different heat treatments
Source abstract
Abstract
Abstract Microstructure evolution and fracture behavior of Mg-9.5Gd-0.9Zn-0.5Zr alloy subjected to different heat treatments were systematically investigated using SEM and TEM as well as tensile testing. It was found that the microstructure of the as-cast alloy consisted of α-Mg matrix, net-like eutectic compounds (α-Mg + Mg3 (Gd, Zn)), cubic GdH2 phases and lamellar 14H LPSO phases. After solution treated at 515 °C for 24 h, two different cooling processes were used to elucidate the effect of cooling rates on the precipitation microstructure. With a hot water quenching, those secondary phases were completely dissolved. Instead, grey-like patches were observed within the α-Mg matrix, which were proposed to be rod-like Zn2Zr3 phases around the α-Zr particle. In contrast, with a furnace cooling, the formation of 14H LPSO and several cubic Mg3 (Gd, Zn) phases was observed. Furthermore, after hot water quenching, the subsequent ageing treatment parameters were also optimized to be 225 °C for 48 h. In the peak-aged condition, a denser and uniform distribution of basal precipitates γ″ and several basal precipitates γ′ together with Zn2Zr3 and ZnZr2 phases were observed. The samples after the solution treatment (for both hot water quenching and furnace cooling) showed a much higher ductility than the as-cast alloy, while the tensile yield strength (TYS) and ultimate tensile strength (UTS) remained unchanged. After the peak-ageing, a significant increase in the TYS and UTS but a great loss in ductility was observed. In the as-cast alloy, the initiation of microcracks occurred from the net-like eutectic compounds, which was believed to be one of the most important reasons for the tensile fracture, and showed a co-existence of intergranular and transgranular fracture behavior. After the solution treatment, with a hot water quenching, the fracture can be mainly related with failures along contraction twins, and then showed a transgranular fracture behavior. While, with a furnace cooling, due to the presence of the kinked 14H LPSO phases, the fracture was caused by the broken of 14H LPSO phases, and then lead to a transgranular fracture. The peak-aged alloy exhibited a brittle intergranular fracture, which can be related with failures along soft precipitation free zones (PFZs).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Fabrication of extraordinary high-strength magnesium alloy by hot extrusion10.1016/j.scriptamat.2009.06.003 ↗
2. The relationship between microstructure and creep resistance in die-cast magnesium-rare earth alloys10.1016/j.scriptamat.2010.02.005 ↗
3. A simulation study of the shape of β’ precipitates in Mg-Y and Mg-Gd alloys10.1016/j.actamat.2012.09.044 ↗
4. Enhanced precipitation-hardening in Mg-Gd alloys containing Ag and Zn10.1016/j.scriptamat.2009.05.044 ↗
5. Enhanced age hardening response and creep resistance of Mg-Gd alloys containing Zn10.1016/j.scriptamat.2005.07.004 ↗
6. Effect of long-period stacking ordered phase on mechanical properties of Mg97Zn1Y2 extruded alloy10.1016/j.actamat.2010.07.050 ↗
7. The microstructure evolution with lamellar 14H-type LPSO structure in an Mg96.5Gd2.5Zn1 alloy during solid solution heat treatment at 773 K10.1016/j.jallcom.2008.10.126 ↗
8. Formation of long period stacking ordered phases in Mg-10Gd-1Zn-0.5Zr (wt.%) alloy10.1016/j.matchar.2018.10.022 ↗
9. Microstructure, tensile deformation and fracture behaviour of aluminium alloy 705510.1023/A:1018676501368 ↗
10. Constitutive characterization of a rare-earth magnesium alloy sheet (ZEK100-O) in shear loading: studies of anisotropy and rate sensitivity10.1016/j.ijmecsci.2017.04.013 ↗
11. Precipitation and its effect on the mechanical properties of a cast Mg-Gd-Nd-Zr alloy10.1016/j.msea.2007.11.080 ↗
12. Effect of aging treatment on fracture toughness in ZM61 magnesium alloy10.1179/1743284714Y.0000000633 ↗
13. Obtaining high strength and high plasticity in a Mg-3Al-1Zn plate using pre-tension and annealing treatments10.1016/j.jallcom.2017.02.087 ↗
14. Strain induced GdH2 precipitate in Mg-Gd based alloys10.1016/j.intermet.2010.11.001 ↗
15. On the unexpected formation of rare earth hydrides in magnesium-rare earth casting alloys10.1016/j.scriptamat.2014.01.007 ↗
16. In vitro and in vivo comparison of binary Mg alloys and pure Mg10.1016/j.msec.2015.12.064 ↗
17. Effect of heat treatment on the microstructures and mechanical properties of the extruded Mg-11Gd-1Zn alloy10.1016/j.jallcom.2012.08.045 ↗
18. The relationship between (Mg,Zn)3RE phase and 14H-LPSO phase in Mg-Gd-Y-Zn-Zr alloys solidified at different cooling rates10.1016/j.jallcom.2010.12.136 ↗
19. Growth and transformation mechanisms of 18R and 14H in Mg-Y-Zn alloys10.1016/j.actamat.2012.08.022 ↗
20. Microstructural characterization of intermetallic phases in a solution-treated Mg-5.0Sm-0.6Zn-0.5Zr (wt%) alloy10.1016/j.matchar.2018.08.059 ↗
21. Transmission electron microscopy of Zr-Zn precipitate rods in magnesium alloys containing Zr and Zn10.1080/09500830802524096 ↗
22. Formation of 14H-type long period stacking ordered structure in the as-cast and solid solution treated Mg-Gd-Zn-Zr alloys10.1557/jmr.2009.0215 ↗
23. Substantial corrosion resistance improvement in heat-treated Mg-Gd-Zn alloys with a long period stacking ordered structure10.1016/j.matchemphys.2017.09.035 ↗
24. Formation of 14H long period stacking ordered structure and profuse stacking faults in Mg-Zn-Gd alloys during isothermal aging at high temperature10.1016/j.actamat.2007.08.033 ↗
25. Solute segregation and precipitation in a creep-resistant Mg-Gd-Zn alloy10.1016/j.actamat.2008.08.025 ↗
26. A super high-strength Mg-Gd-Y-Zn-Mn alloy fabricated by hot extrusion and strain aging10.1016/j.matdes.2019.107666 ↗
27. Precipitation sequence and kinetics in a Mg-4Sm-1Zn-0.4Zr (wt%) alloy10.1016/j.jallcom.2015.07.129 ↗
28. Heat treatment and mechanical properties of a high-strength cast Mg-Gd-Zn alloy
29. Thermodynamic modelling of the Zn-Zr system10.1016/j.calphad.2005.12.006 ↗
30. Analysis of anisotropic damage in forged Al-Cu-Mg-Si alloy based on creep tests, micrographs of fractured specimen and digital image correlations10.1016/j.msea.2015.11.090 ↗
31. Effect of segregation of secondary phase particles and “S” line on tensile fracture behavior of friction stir-welded 2024Al-T351 joints10.1007/s11661-013-1778-8 ↗
32. Fracture behavior of AZ91 magnesium alloy
33. Plastic strain-induced grain refinement in the nanometer scale in a Mg alloy10.1016/j.actamat.2006.09.018 ↗
34. The influence of microstructure on the Bauschinger effect in an Al-Si-Mg casting alloy10.1016/1359-6454(95)00171-6 ↗
35. The work-hardening of copper-silica10.1080/14786437108217405 ↗
36. Twinning-induced softening in polycrystalline AM30 Mg alloy at moderate temperatures10.1016/j.scriptamat.2005.11.029 ↗
37. Non-Schmid behaviour during secondary twinning in a polycrystalline magnesium alloy10.1016/j.actamat.2007.08.034 ↗
38. Contraction twinning dominated tensile deformation and subsequent fracture in extruded Mg-1Mn (Wt Pct) at ambient temperature10.1007/s11661-018-4557-8 ↗
39. Deformation twinning in AZ31: influence on strain hardening and texture evolution10.1016/j.actamat.2010.07.041 ↗
40. Twinning and the ductility of magnesium alloys Part II. “Contraction” twins10.1016/j.msea.2007.02.109 ↗
41. High-temperature compressive deformation behavior of Mg97Zn1Y2 extruded alloy containing a long-period stacking ordered (LPSO) phase10.1016/j.msea.2012.09.016 ↗
42. A two-step dynamic recrystallization induced by LPSO phases and its impact on mechanical property of severe plastic deformation processed Mg97Y2Zn1 alloy10.1016/j.jallcom.2017.02.107 ↗
43. Formation of lamellar phase with 18R-type LPSO structure in an as-cast Mg96Gd3Zn1(at%) alloy10.1016/j.matlet.2015.12.080 ↗
44. Strengthening and toughening mechanisms in Mg-Zn-Y alloy with a long period stacking ordered structure10.1016/j.actamat.2010.05.012 ↗
45. Room temperature deformation of LPSO structures by non-basal slip10.1016/j.msea.2016.11.056 ↗
46. Crystallographic classification of kink bands in an extruded Mg-Zn-Y alloy using intragranular misorientation axis analysis10.1016/j.actamat.2012.12.026 ↗
47. Ageing behavior of extruded Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr (wt.%) alloy containing LPSO phase and γ′ precipitates10.1038/srep43391 ↗