Influence of Fe addition on the formation of a quasicrystalline phase in bulk Al-rich Al Mn base alloys
Source abstract
Abstract
Abstract This work evaluates the effect of Fe addition on the formation of a quasicrystalline phase in the 94Al 6Mn base alloys obtained by wedge casting. Different Mn to Fe ratios (1, 1.4, 2, 5) were used to estimate Fe content that leads to formation of a quasicrystalline icosahedral phase (I-phase) at the selected Al concentration (94 at.%). Based on the obtained results, Fe enhances I-phase nucleation in the studied ternary alloys compared to the non-modified binary composition. Although the maximum thickness of the cast wedge at which the I-phase was formed in the prepared alloys varied with Fe content, its nucleation was always limited to a certain range of cooling rates above 103 K/s. Hardness increased significantly for areas composed of Al matrix and I-phase particles. The highest HV values were obtained for parts of castings where the microstructure consisted of very fine I-phase/Al eutectic.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Quasicrystal Structures and Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. High mechanical strength of Al-(V, Cr, Mn)-(Fe, Co-Ni) quasicrystalline alloys prepared by rapid solidification10.2320/matertrans1989.37.1287 ↗
2. Production and mechanical properties of aluminum alloys with dispersed nanoscale quasicrystalline and amorphous particles10.1007/BF03027251 ↗
3. Nanoquasicrystalline Al–Fe–Cr-based alloys. Part II. Mechanical properties10.1016/j.actamat.2009.07.009 ↗
4. Structure and mechanical properties in a powder-processed icosahedral-phase-strengthened aluminum alloy10.1016/j.scriptamat.2016.05.037 ↗
5. Strengthening mechanisms in an Al-Fe-Cr-Ti nano-quasicrystalline alloy and composites10.1016/j.msea.2016.07.007 ↗
6. Effect of trace additions of Ag on precipitation in Al–Mg alloys10.2320/matertrans.46.2968 ↗
7. Characterisation of quasicrystalline particles in an isothermally aged Al–10Mg–0.5Ag (mass%) alloy10.2320/matertrans.46.1278 ↗
8. Synthesis of stable quasicrystalline particle-dispersed Al base composite alloys10.1557/JMR.1993.0005 ↗
9. Structure and mechanical properties of mechanically alloyed Al/Al-Cu-Fe composites10.1023/B:JMSC.0000039253.28721.3f ↗
10. Microstructure and mechanical properties of aluminium matrix composites reinforced by Al 62 Cu 25.5 Fe 12.5 melt spun ribbon10.1016/j.matchar.2016.04.025 ↗
11. Orientation relation between icosahedral and crystalline phases in Al-Mn alloys10.1080/13642818808211231 ↗
12. Crystallization and precipitation structures of quasicrystalline phase in rapidly solidified Al-Mn-X ternary alloys10.1007/BF02385762 ↗
13. Inhibition of Al grain coarsening by quasicrystalline icosahedral phase in the rapidly solidified powder metallurgy Al-Fe-Ti-Cr10.1016/j.scriptamat.2007.01.012 ↗
14. Microstructure modification and quasicrystalline phase formation in Al–Mn–Si–Be cast alloys10.1016/j.msea.2003.10.004 ↗
15. Formation of quasicrystalline phases in Al-rich Al–Mn–Be alloys10.1016/j.jnoncrysol.2003.11.005 ↗
16. Characterization of cast Al86Mn3Be11 alloy10.1111/j.1365-2818.2009.03135.x ↗
17. Enhancement of the quasicrystal-forming ability in Al-based alloys by Be-addition10.1016/S0925-8388(02)00186-X ↗
18. Crystal–quasicrystal transition depending on cooling rates in directionally solidified Al–3Mn–7Be (at.%) alloy10.1016/j.intermet.2013.09.004 ↗
19. Beryllium
20. High mechanical strength of qua-sicrystalline phase surrounded by fcc-Al phase in rapidly solidified Al–Mn–Ce alloys10.2320/matertrans1989.33.723 ↗
21. Synthesis and 672 mechanical properties of cast quasicrystal-reinforced Al-alloys10.1016/S1359-6454(01)00045-3 ↗
22. Reassessment of the effects of Ce on quasicrystal formation and microstructural evolution in rapidly solidified Al–Mn alloys10.1016/j.actamat.2015.07.046 ↗
23. K. Stan-Głowińska, L. Rogal, A. Góral, A. Wierzbicka-Miernik, J. Wojewoda-Budka, N. Schell, L. Lityńska-Dobrzyńska, Formation of a quasicrystalline phase in Al-Mn base alloys cast at intermediate cooling rates, J. Mater. Sci. in press: DOI 10.1007/s10853-017-1011-z10.1007/s10853-017-1011-z ↗
24. Selection and application of aluminum alloys
25. Rational approximants to the decagonal phase in Al-Mn-M (M=Ni, Cu, Zn) systems10.1016/0921-5093(94)90732-3 ↗
26. The structure and stability of some intermetallic phases in rapidly solidified Al-Fe10.1016/S0036-9748(88)80052-8 ↗