Effects of d.c. current on the phase transformation in 7050 alloy during homogenization
Source abstract
Abstract
Evolutions of properties and morphologies of secondary phases in 7050 alloy homogenized with direct electric current were studied in detail by conductivity measurement, tensile test and energy dispersive X-ray microanalysis. With increasing temperature, the conductivity decreases, and while the ultimate tensile strength, yield strength and elongation of 7050 alloy increase in alloy homogenized with direct electric current, and reaches the saturation values at 440 °C/2 h. During homogenization, the brighter white AlZnMgCu phase having (weight ratio %) 12.1–15.2Mg, 27.2–32.1Al, 20.9–26.2Cu and 31.4–34.4Zn gradually transforms to the gray phase having (weight ratio %) 10.3–15.1Mg, 41.4–53.7Al, 22.9–35.2Cu and 5.8–13.1Zn and then to the dark gray phase having (weight ratio %) 10.6–14.2 Mg, 38.2–54.9Al, 23.3–44Cu, and 3.6–9.2Zn. With the application of direct electric current, the elemental diffusion network becomes profuse, the amount of gray phase increases, the diffusion of Zn accelerates, the apparent activation of the transformation from AlZnMgCu to Al 2MgCu decreases from 125.52 kJ/mol for the alloy homogenized without direct electric current to 118.82 kJ/mol, and the area fraction of secondary phase decreases by 38% at 450 °C.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Electromagnetic Effects on Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. New aspects of development of high strength Al alloys for aerospace applications10.1016/S0921-5093(00)00667-5 ↗
2. Microstructure and tensile properties of large-size 7055 aluminum billets fabricated by spray forming rapid solidification technology10.1016/j.jallcom.2013.05.117 ↗
3. On the nature of T(Al2Mg3Zn3) and S(Al2CuMg) phases present in as-cast and annealed 7055 aluminum alloy10.1016/j.msea.2004.09.013 ↗
4. Investigation of phase equilibria in alloys of the Al–Zn–Mg–Cu–Zr–Sc system10.1016/j.jallcom.2003.08.003 ↗
5. Microstructural evolution in aluminium alloy 7050 during processing10.1016/j.msea.2004.05.006 ↗
6. Study on inhomogeneous characteristics and optimize homogenization treatment parameter for large size DC ingots of Al–Zn–Mg–Cu alloys10.1016/j.jallcom.2013.09.139 ↗
7. Effects of high magnetic field on the evolutions of constituent phases in 7085 aluminum alloy during homogenization10.1016/j.matchar.2012.05.014 ↗
8. Effect of high magnetic field on phase transformation of 7055 alloy during homogenization10.4028/www.scientific.net/AMR.189-193.4472 ↗
9. Evolution of eutectic structures in Al–Zn–Mg–Cu alloys during heat treatment10.1016/S1003-6326(06)60101-5 ↗
10. The improvement of constituent dissolution and mechanical properties of 7055 aluminum alloy by stepped heat treatments10.1016/S0924-0136(03)00597-1 ↗
11. Effect of compositional variations on characteristics of coarse intermetallic particles in overaged 7000 aluminium alloys10.1179/026708301101509449 ↗
12. In situ evidence of enhanced transformation kinetics in a medium carbon steel due to a high magnetic field10.1016/j.scriptamat.2004.03.029 ↗
13. Grain boundary characteristics and texture formation in a medium carbon steel during its austenitic decomposition in a high magnetic field10.1016/j.actamat.2005.08.007 ↗
14. Aligned two-phase structures in Fe–C alloys10.1016/S1359-6462(99)00381-4 ↗
15. Grain boundary and grain structure control through application of a high magnetic field10.1016/j.scriptamat.2005.11.038 ↗
16. Effect of stable magnetic field on grain refinement of low carbon Mn–Nb steel
17. Electric current effects on Sn/Ag interfacial reactions10.1007/s11664-999-0217-5 ↗
18. Electric current effects upon the Sn/Cu and Sn/Ni interfacial reactions10.1007/s11664-998-0068-5 ↗
19. Effect of an alternating magnetic field on the phase formation in Al–Cu couple10.1023/B:JMSC.0000021485.17417.3b ↗
20. Effects of electric field on recrystallization texture evolution in cold-rolled high-purity aluminum sheet during annealing10.1016/S1003-6326(07)60063-6 ↗
21. Magnetically enhanced recrystallization in an aluminum alloy10.1016/j.scriptamat.2006.08.018 ↗
22. Annealing behavior of cold rolled aluminum alloy in a high magnetic field10.1016/j.scriptamat.2006.02.033 ↗
23. Influences of magnetic annealing on the grain growth in a cryoECAPed 1050 aluminum alloy10.1016/j.matchar.2013.07.020 ↗
24. Effect of prior cold work on the influence of electric current pulses on the recrystallization of copper10.1016/0036-9748(84)90522-2 ↗
25. Effect of an electric field on the recovery and recrystallization of Al and Cu10.1016/0036-9748(89)90252-4 ↗
26. Effects of electropulse duration and frequency on grain growth in Cu10.1016/0956-716X(90)90270-Q ↗
27. Effect of electric field on kinetics of formation of S phase in 2E12 aluminum alloy
28. Influence of homogenization treatment in an electric field on the workability of 1420 Al–Li alloy during hot rolling10.1007/BF00264096 ↗
29. Texture and microstructure development in cold-rolled interstitial free (IF) steel sheet during electric field annealing10.1016/S1359-6462(02)00552-3 ↗
30. A study on the ageing treatment of 2091 Al–Li alloy with an electric field10.1023/A:1018513411517 ↗
31. Effects of an electric field applied during the solution heat treatment of the Al–Mg–Si–Cu alloy AA 6111 on the subsequent natural aging kinetics and tensile properties10.3139/146.101216 ↗
32. Enhanced phase transformation and variant selection by electric current pulses in a Cu–Zn alloy10.1557/jmr.2014.76 ↗
33. Studies on the microstructures and properties in phase transformation of homogenized 7050 alloy10.1016/j.msea.2014.06.027 ↗
34. Microstructural evolution of high strength 7B04 ingot during homogenization treatment10.1016/S1003-6326(08)60132-6 ↗
35. The constituents in Al–10Zn–2.5Mg–2.5Cu aluminum alloy10.1016/j.msea.2005.02.013 ↗
36. Intermetallic phase evolution of 7050 aluminum alloy during homogenization10.1016/j.intermet.2012.03.006 ↗
37. The tensile response and fracture behavior of an Al–Zn–Mg–Cu alloy: influence of temperature10.1007/s11665-997-0100-6 ↗
38. Cahn · 1996
39. Effect of small alloying additions on behaviour of rapidly solidified Cu–Cr alloys10.1179/mst.1990.6.9.892 ↗
40. Determination of kinetic parameters from calorimetric study of solid state reactions in 7150 Al–Zn–Mg alloy10.1016/S1003-6326(11)60843-1 ↗
41. A differential technique for the determination of the activation energy of precipitation reactions from differential scanning calorimetric data10.1016/S0036-9748(88)80207-2 ↗