The morphological evolution of primary austenite during isothermal coarsening
Source abstract
Abstract
The morphological evolution of primary austenite in an industrial hypoeutectic lamellar cast iron was studied under isothermal conditions for coarsening times varying from 0 min to 96 h. The dendritic austenite structure formed during the primary solidification suffered major morphological changes during the isothermal coarsening process. After a sufficient coarsening time, dendrite fragmentation, globularization, and coalescence of austenite were studied using electron backscatter diffraction (EBSD) technique. This study confirmed that the secondary dendrite arm spacing (SDAS) is an inappropriate length scale to describe the primary austenite coarsening process for longer times. The application of shape independent quantitative parameters confirmed the reduction of the total interfacial area during microstructural coarsening. The modulus of the primary austenite, M γ, which represents the volume-surface ratio for the austenite phase, and the spatial distribution of the austenite particles, measured as the nearest distance between the center of gravity of neighboring particles, D γ, followed a linear relation with the cube root of coarsening time during the whole coarsening process. The mean curvature of the austenite interface, characterized through stereological relations, showed a linear relation to M γ and D γ, allowing the quantitative characterization and modeling of the complete coarsening process of primary austenite.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. The morphological evolution of dendritic microstructures during coarsening10.1016/j.actamat.2005.11.031 ↗
2. Coarsening mechanisms in a dendritic Al–10% Cu alloy10.1016/j.actamat.2009.08.052 ↗
3. The Theory of Ostwald Ripening10.1007/BF01017860 ↗
4. The morphological evolution of equiaxed dendritic microstructures during coarsening10.1016/j.actamat.2009.01.036 ↗
5. The kinetics of precipitation from supersaturated solid solutions10.1016/0022-3697(61)90054-3 ↗
6. Theorie der Alterung von Niederschlägen Durch Umlösen
7. Dendrite arm spacing in aluminiun alloys
8. Dendrite coarsening during directional solidification of Al–Cu–Mn alloys10.1016/S0921-5093(97)00720-X ↗
9. The dendrite arm spacings of aluminum-copper alloys solidified under steady-state conditions10.1007/BF02673688 ↗
10. Effect of fraction solid on coarsening of secondary dendrite arms10.1179/136404609X367911 ↗
11. On the rate of dendrite arm coarsening10.1007/BF02656824 ↗
12. Overview of geometric effects on coarsening of mushy zones10.1007/BF02648946 ↗
13. Influence of coarsening on dendrite arm spacing of aluminum-copper alloys
14. Coarsening in solidification processing10.2320/matertrans.46.895 ↗
15. Three-dimensional characterization of dendritic microstructures10.1016/S1359-6454(00)00355-4 ↗
16. The morphological evolution of dendritic microstructures during coarsening10.1007/s11661-003-0084-2 ↗
17. The evolution of dendrites during coarsening: fragmentation and morphology10.1016/j.actamat.2017.01.029 ↗
18. Relation between SDAS and eutectic cell size in grey iron10.1179/136404610X12693537269895 ↗
19. Austenite dendrite morphology in lamellar graphite iron10.1179/1743133615Y.0000000018 ↗
20. Dynamic coarsening of 3.3C–1.9Si gray cast iron10.1007/s11661-012-1244-z ↗
21. Weibel · 1979 · 1 · 26
22. Theory of the solidification of castings
23. A generic model to predict the ultimate tensile strength in pearlitic lamellar graphite iron10.1016/j.msea.2014.08.061 ↗
24. The significance of average mean curvature and its determination by quantitative metallography
25. The quantitative estimation of mean surface curvature
26. Underwood · 1970 · 225
27. Weibel · 1980 · 2 · 101
28. Dendrite coherency of Al-Si-Cu alloys10.1007/s11661-001-0110-1 ↗
29. Microstructural changes during quenching10.1016/S0022-0248(98)00451-5 ↗
30. Evolution of specific surface area with solid fraction during solidification10.1016/j.actamat.2010.04.012 ↗