journal article·2023-06

Investigation of diffusion reaction mechanism between W20Ta solid solution and Ni

Yao Wang, Yufeng Huang, Wensheng Liu, Baishan Chen, Jiayi Liu, Lei Zhang, Wenyang Liu, Yunzhu Ma

Publisher page

Abstract

The tantalum (Ta) solution into tungsten (W) can effectively reduce the intrinsic brittleness of W, it is likely to further enhance the toughness of tungsten alloys by using W Ta solid solution particles. However, the solid solution promotes the diffusion reaction between W Ta particles and nickel (Ni) based matrix phase and generates massive intermetallics (IMCs), deteriorating the structure of the tungsten alloy. Hence, the diffusion reaction mechanism between W Ta solid solution and Ni can be the key to guide the development of tungsten alloys. This study determined that the diffusion layer generated the tetragonal Ni 3Ta phase through W-20(wt%)Ta/Ni solid phase diffusion reaction below 1350 °C, which has the highest hardness (10.06GPa) and a good interface orientation with W Ta particles. As the temperature reached 1400 °C, the liquid phase appeared, and a eutectic reaction occurred: Liq. → fcc Ni + orthogonal Ni 3Ta. The tetragonal Ni 3Ta phase transformed into a more stable orthogonal Ni 3Ta and formed a coherent interface. At the same time, a small amount of unstable Ni(Ta, W) 2 phase appeared at the edge of W Ta solid solution particles. Its structure and properties were similar to NiTa 2. This study is significant in guiding the strengthening and toughening of tungsten alloys with W Ta solid solution particles.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. The effect of hot rolling on the strength and fracture toughness of 90W–7Ni3Fe tungsten heavy metal alloys10.1016/j.msea.2021.141738 ↗
2. Elevated temperature tensile behavior and microstructure evolution of liquid phase sintered 90W–7Ni–3Fe alloy10.1016/j.jallcom.2019.06.222 ↗
3. Review: liquid phase sintering10.1007/s10853-008-3008-0 ↗
4. The effect of tantalum (ta) doping on mechanical properties of tungsten (W): a first-principles study10.1557/jmr.2016.358 ↗
5. Effect of tantalum concentration on the microstructure and mechanical properties of novel W–Ta-Re alloy10.1016/j.vacuum.2022.111627 ↗
6. Short-range ordering governs brittleness and ductility in W-ta solid solution: insights from Pugh’s shear-to-bulk modulus ratio10.1016/j.scriptamat.2021.114136 ↗
7. Effect of tungsten tantalum pre-alloying on the sintering structure of 90(W-ta)-Ni-Fe alloy
8. Effect of tantalum addition method on microstructure and mechanical properties of the 90(W20Ta)–Ni–Fe alloy10.1016/j.ijrmhm.2022.105848 ↗
9. The effect of tungsten content on the rolling texture and microstructure of ta-W alloys10.1016/j.matchar.2019.110067 ↗
10. Revealing impact failure behavior of tungsten composite using instrumented Charpy impact testing10.1016/j.matchar.2022.112181 ↗
11. K.B. Gajanan Balaji Kale, Sheo Parakash Garg, M. Materials Science International Team, Assessed phase diagram of the Ni-Ta binary system: Datasheet from MSI Eureka in SpringerMaterials https://materials.springer.com/msi/phase-diagram/docs/sm_msi_r_20_014057_01_full_LnkDia0, G. Effenberg MSI, Materials Science International Services GmbH, Stuttgart.
12. Microstructure and properties of intermetallic compounds of W/Ni/ta diffusion couple10.1016/j.intermet.2022.107732 ↗
13. First-principles studies of Ni–ta intermetallic compounds10.1016/j.jssc.2012.01.001 ↗
14. Thermodynamic optimization of the Ni–ta system supported by the key experiments10.1016/j.tca.2018.06.011 ↗
15. Hardness and tensile properties of tungsten based heavy alloys prepared by liquid phase sintering technique10.1016/j.ijrmhm.2008.08.003 ↗
16. Liquid-phase sintering of tungsten heavy alloys, defect and diffusion
17. Low temperature sintering of 90W–7Ni–3Fe alloy with cu additive: microstructure evolution and mechanical properties10.1016/j.jmrt.2021.01.079 ↗
18. C.L. Haixia Tian, Chenying Shi, Liya Dreval, M. Materials Science International Team, Assessed Phase Diagram of the Ni-W system: Datasheet from MSI Eureka in SpringerMaterials https://materials.springer.com/msi/phase-diagram/docs/sm_msi_r_10_016224_01_full_LnkDia0 G. Effenberg MSI, materials science international, Stuttgart.
19. Experimental investigation and thermodynamic description of the Ni–ta–W system10.1016/j.calphad.2021.102381 ↗
20. Radiation-induced void formation and ordering in ta-W alloys10.1016/j.jnucmat.2017.08.029 ↗
21. Kinetics of solute-enhanced diffusion in dilute face-centered-cubic alloys10.1103/PhysRev.154.561 ↗
22. The influence of solutes on self-diffusion in metals10.1080/14786436008238325 ↗
23. Effect of transmutation elements re and ta on the vacancy formation and dissociation behaviors in W bulk10.1016/j.commatsci.2020.109624 ↗
24. 1 - classical and quantum theory of diffusion in solids
25. Frequency factors and isotope effects in solid state rate processes10.1016/0022-3697(57)90059-8 ↗
26. Interfacial plasticity governs strain rate sensitivity and ductility in nanostructured metals10.1073/pnas.0611097104 ↗
27. On the stability and mobility of di-vacancies in tungsten10.1088/1741-4326/aa99ee ↗
28. Gravitational effects during liquid phase sintering10.1016/S0254-0584(00)00415-6 ↗
29. On the existence and the crystal structure of Ni4W, NiW and NiW2 compounds10.1016/j.intermet.2008.11.001 ↗
30. Local decomposition induced by dislocation motions inside tetragonal Al(2)cu compound: slip system-dependent dynamics10.1038/srep03157 ↗
31. Wallace · 1972
32. Phonon anomalies and elastic constants of cubic NiAl from first principles