Microstructure evolution and corrosion behavior of TC11 laser melt deposition additive components after post-heat treatment

Wenshan Guo, Hui Zhang, Qingjun Zhou, Guangchun Xiao, Ning Guo, Wei Zhao, Gang Wang

Publisher page

Abstract

The TC11 components were produced using a high-power, high-speed laser metal deposition (LMD) process. Subsequent post-heat treatment significantly improved the microstructures and corrosion resistance of the components. The results showed that the microstructure of the as-deposited component primarily comprised α Widmanstatten microstructure and mesh basket-weave microstructure. After post-heat treatment, the original interlayer zone disappeared in the deposition direction, and the microstructures were transformed from α’ to α phase. The aspect ratio of the α phase decreased, and the α grain boundary (α GB ) became spheroidized. The tensile strength decreased but plasticity increased significantly. Overall, the corrosion resistance was improved in both directions, with greater improvements observed in the deposition direction. Phase ratio, grain size and KAM value are all factors affecting the corrosion resistance, but for the deposited direction, the significant improvement of the corrosion resistance is mainly due to the weakening of the charged galvanic corrosion effect between the non-interlayer zone and interlayer zone.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Laser-induced spectroscopy and plasma · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. The effect of hydrogen on the grain refinement and mechanisms for Ti6Al4V alloys during laser melting deposition10.1016/j.jallcom.2021.160122 ↗
2. Microstructure and mechanical properties of LMD-SLM hybrid forming Ti6Al4V alloy10.1016/j.msea.2016.02.069 ↗
3. Additive manufacturing of Ti-6Al-4V parts through laser metal deposition (LMD): process, microstructure, and mechanical properties10.1016/j.jallcom.2019.04.255 ↗
4. Fatigue crack growth behavior of Ti-6Al-4V alloy fabricated via laser metal deposition: effects of building orientation and heat treatment10.1016/j.jallcom.2021.159023 ↗
5. Characterization of microstructure and mechanical properties of laser melting deposited Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.matdes.2013.11.044 ↗
6. Microstructure evolution and layer bands of laser melting deposition Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.jallcom.2014.07.161 ↗
7. Microstructure and mechanical properties of as-deposited and heat treated Ti-5Al-5Mo-5V-3Cr-1Zr (Ti-55531) alloy fabricated by laser melting deposition10.1016/j.jallcom.2019.151792 ↗
8. The anisotropy of laser melting deposition additive manufacturing Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.matdes.2014.11.001 ↗
9. Research on the microstructure and mechanical properties of doubled annealed laser melting deposition TC11 titanium alloy10.1016/j.optlastec.2022.107983 ↗
10. Distinction in corrosion resistance of selective laser melted Ti-6Al-4V alloy on different planes10.1016/j.corsci.2016.06.009 ↗
11. Hot working of Ti-6Al-3Mo-2Zr-0.3Si alloy with lamellar α+β starting structure using processing map10.1016/j.matdes.2008.07.031 ↗
12. Flow softening and microstructural evolution of TC11 titanium alloy during hot deformation10.1016/j.jmatprotec.2008.04.063 ↗
13. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
14. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: part I10.1007/s11661-004-0094-8 ↗
15. Microstructure and tensile properties of additive manufactured Ti-6Al-4V with refined prior-β grain structure obtained by rapid heat treatment10.1016/j.msea.2021.141271 ↗
16. Variant selection during α precipitation in Ti–6Al–4V under the influence of local stress – a simulation study10.1016/j.actamat.2013.06.042 ↗
17. Intensification of preferred orientation in the additive manufactured Ti-6Al-4V alloy after heat treatment10.1016/j.matlet.2020.129198 ↗
18. Effects of heat treatment on microstructures and mechanical properties of GH4169/K418 functionally graded material fabricated by laser melting deposition10.1016/j.msea.2021.141601 ↗
19. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗
20. Impact of microstructure evolution on the corrosion behaviour of the Ti-6Al-4V alloy welded joint using high-frequency pulse wave laser10.1016/j.jmrt.2023.04.077 ↗
21. Effect of Y2O3 on microstructure and properties of CoCrFeNiTiNb high entropy alloy coating on Ti–6Al–4V surface by laser cladding
22. Oxidation behavior of low-cost CP-Ti powders for additive manufacturing via fluidization10.1016/j.corsci.2020.109080 ↗
23. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
24. Influence of inter-layer rotation in parallel deposition strategies on the microstructure, texture, and mechanical behaviour of Inconel-625 during directed energy deposition10.1016/j.matchar.2023.112711 ↗
25. Ductility improvement due to martensite α’ decomposition in porous Ti-6Al-4V parts produced by selective laser melting for orthopedic implants10.1016/j.jmbbm.2015.09.020 ↗
26. Building direction dependence of corrosion resistance property of Ti–6Al–4V alloy fabricated by electron beam melting10.1016/j.corsci.2017.08.008 ↗
27. In situ corrosion monitoring of Ti-6Al-4V alloy in H2SO4/HCl mixed solution using electrochemical AFM10.1016/j.electacta.2010.10.024 ↗
28. The role of macrostructural morphology and grain size on the corrosion resistance of Zn and Al castings10.1016/j.msea.2005.02.094 ↗
29. Galvanic effect of magnetite on the corrosion behavior of carbon steel in deaerated alkaline solutions under flowing conditions10.1016/j.corsci.2017.10.017 ↗
30. Understanding the galvanic corrosion of the Q-phase/Al couple using SVET and SIET10.1016/j.jmst.2019.03.001 ↗