journal article·2022-07

Microstructure anomaly upon high temperature exposure and its influence on the mechanical properties of a modified 9Cr-1Mo steel weld

Ranjeet Kumar, Anand Varma, Y. Ravi Kumar, Jayant Jain, Suresh Neelakantan

Publisher page

Abstract

The present work evaluates the microstructure stability of modified 9Cr-1Mo steel welds when subjected to high temperature exposure (HTE) at 775 °C for different times (5, 100, 500, and 1000 h). Prior to HTE, a post weld heat treatment (PWHT) at 760 °C for 2 h was performed. Upon HTE, the individual weld zones viz., weld metal (WM), coarse-grain heat affected zone (CGHAZ) and fine-grain heat affected zone (FGHAZ) demonstrate distinct microstructural variations in terms of precipitate size, grain size and substructure (lath/block/packet boundaries) fractions. The least- and the highest-microstructure stability are respectively seen in FGHAZ and WM after HTE. A detailed investigation involving electron backscattered diffraction (EBSD) and high-resolution transmission electron microscopy (HR-TEM) confirm that a pronounced recovery of the substructure in FGHAZ happens due to enhanced diffusion along the higher fraction of prior-austenite grain boundaries (PAGBs), leading to M 23C 6 precipitate coarsening and substantial grain growth. The microstructure degradation upon HTE for 1000 h had eventually resulted in deterioration of mechanical properties, where the hardness reduced the most for FGHAZ (~34%), while the least for WM (~7%). Similarly, after HTE, the tensile strength and toughness had deteriorated by ~67% and ~57%, respectively, from the PWHT condition. Fractography further confirms the pronounced degradation after HTE as they result in failure from FGHAZ.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors10.1179/174328005X41140 ↗
2. Creep properties in similar weld joint of a thick-walled P92 steel pipe10.1016/j.matchar.2016.06.033 ↗
3. Microstructural stability and creep data assessment of Tenaris Grades 91 and 911
4. Abe · 2014
5. Abe · 2008
6. New insight into high-temperature creep deformation and fracture of T92 steel involving precipitates, dislocations and nanovoids10.1016/j.matchar.2017.01.025 ↗
7. The effect of tungsten on dislocation recovery and precipitation behavior of low-activation martensitic 9Cr steels10.1007/BF02664988 ↗
8. Alloy design of creep resistant 9Cr steel using a dispersion of nano-sized carbonitrides10.1016/j.ijpvp.2006.09.003 ↗
9. On the effect of long-term creep on the microstructure of a 12% chromium tempered martensite ferritic steel10.1016/j.actamat.2009.07.010 ↗
10. Theory of growth of spherical precipitates from solid solution10.1063/1.1698258 ↗
11. Five decades of the Zener equation10.2355/isijinternational.38.913 ↗
12. Effect of austenite grain boundary mobility on hardenabilityof steels containing vanadium10.1179/mst.1988.4.11.967 ↗
13. Effect of titanium additions on austenite grain growth kinetics of medium carbon V-Nb steels containing 0.008-0.018%N10.1179/mst.1991.7.2.176 ↗
14. Microstructure characterization of heat affected zone after welding in Mod.9Cr-1Mo steel10.1016/j.matchar.2015.01.013 ↗
15. Enhancement of mechanical properties through modified post-weld heat treatment processes of T91 and Super304H dissimilar welded joint10.1016/j.jmapro.2022.04.008 ↗
16. Effect of post-weld heat treatment on the microstructure and hardness of P92 steel in IN740H/P92 dissimilar weld joints10.1016/j.matchar.2019.110083 ↗
17. Optimization of post-weld heat treatment condition of arc-welded T91 steel tubes10.1016/j.ijpvp.2020.104213 ↗
18. Type IV creep damage behavior in Gr.91 steel welded joints10.1007/s11661-011-0967-6 ↗
19. Evaluation of creep damage in heat affected zone of thick welded joint for Mod.9Cr-1Mo steel10.1016/j.ijpvp.2009.04.008 ↗
20. Microstructural instability of a welded joint in P91 steel during creep at 600°C10.1179/174328405X43216 ↗
21. Role of microstructures on heterogeneous creep behaviour across P91 steel weld joint assessed by impression creep testing10.1016/j.matchar.2019.109988 ↗
22. Study on the creep deformation behavior and characterization of 9Cr-1Mo-V-Nb steel at elevated temperatures10.1016/j.matchar.2018.10.011 ↗
23. Failure investigation of radiant platen Superheater tube of thermal power plant boiler
24. Bulging rupture and caustic corrosion of a boiler tube in a thermal power plant10.1016/j.engfailanal.2019.06.022 ↗
25. Coarsening behaviour of M23C6 carbides in creep-resistant steel exposed to high temperatures10.1038/srep29734 ↗
26. Effects of precipitation on the scale and grain growth in 9% Cr tempered martensite steel upon steam oxidation10.1016/j.matchar.2020.110497 ↗
27. Handbook · 2004
28. Investigation of parent austenite grains from Martensite structure using EBSD in a Wear Resistant steel
29. Exploring performance limits of a new martensitic high strength steel by ausforming via equal channel angular pressing10.1016/j.scriptamat.2020.03.011 ↗
30. NIH image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
31. E8, ASTM E8/E8M standard test methods for tension testing of metallic materials 1
32. Factors affecting Type IV creep damage in Grade 91 steel welds10.1016/j.msea.2013.04.045 ↗
33. Role of grain boundary engineering in the SCC behavior of ferritic-martensitic alloy HT-910.1016/j.jnucmat.2006.12.006 ↗
34. Doherty · 1996 · 987
35. Evolution of dislocation density, size of subgrains and MX-type precipitates in a P91 steel during creep and during thermal ageing at 600°C for more than 100,000h10.1016/j.msea.2010.03.010 ↗
36. Static recovery of tempered lath martensite microstructures during long-term aging in 9-12% Cr heat resistant steels10.1016/j.matlet.2009.08.024 ↗
37. Creep behavior and degradation of subgrain structures pinned by nanoscale precipitates in strength-enhanced 5 to 12 Pct Cr ferritic steels10.1007/s11661-011-0726-8 ↗
38. Type IV cracking in ferritic power plant steels10.1179/174328406X148778 ↗
39. Evaluation of tension and creep rupture behaviors of long-term exposed P91 steel in a supercritical plant10.1016/j.engfailanal.2020.104736 ↗