Mechanical properties degradation of Sn 37Pb solder joints caused by interfacial microstructure evolution under cryogenic temperature storage
Source abstract
Abstract
The interfacial microstructure, shear property and fracture behaviors of Sn 37Pb joints after cryogenic temperature storage for different durations were investigated in this study, storage test at room temperature (298 K) and thermal aging test at 423 K were also carried out as comparison. The morphology of interfacial Cu 6Sn 5 IMCs for the joints stored under 77 K and 173 K transformed from scallop-like to column-like, moreover, the IMC layer thickness slowly increased with prolonged storage time. The growth rate of Cu 6Sn 5 layer in Sn 37Pb joint stored at 77 K was slightly faster as compared with that stored at 173 K. However, the morphology and thickness of Cu 6Sn 5 IMC layer still remained roughly unchanged after storage at 298 K for up to 40 days. The Cu 6Sn 5 IMC growth of Sn 37Pb joint stored at 77 K and 173 K was expected to be caused by Cu atom diffusion from Cu pad towards Sn 37Pb solder, which was induced by the stress gradient. Additionally, the shear force declined and fracture position changed from in Sn 37Pb solder to primarily in Sn 37Pb solder and partly along the interface with the prolonging of storage time at 77 K and 173 K, which were induced by IMC layer growth.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Microstructure and grain orientation evolution in SnPb/SnAgCu interconnects under electrical current stressing at cryogenic temperature10.3390/ma12101593 ↗
2. Fracture pattern evolution of SnAgCu-SnPb mixed solder joints at cryogenic temperature10.1016/S1003-6326(21)65691-1 ↗
3. Influence of stress on the creep behavior of Cu particle enhancement SnPb based composite solder joints10.1016/S1001-0521(07)60027-8 ↗
4. Effect of Ag and Cu co-addition on the microstructure evolution, interface behavior and mechanical properties of Sn-5Sb based solder joints subjected to different thermal aging conditions10.1016/j.microrel.2022.114797 ↗
5. Interfacial intermetallic compound growth in Sn-3Ag-0.5 Cu/Cu solder joints induced by stress gradient at cryogenic temperatures10.1016/j.jallcom.2019.05.295 ↗
6. Shear performance of BGA structure Cu/Sn-3.0Ag-0.5 Cu/Cu solder joints after deep cryogenic treatment with different time
7. Solid state interfacial reaction of Sn-37Pb and Sn-3.5Ag solders with Ni-P under bump metallization10.1016/j.actamat.2003.12.042 ↗
8. Tensile fracture behaviors of solid-state-annealed eutectic SnPb and lead-free solder flip chip bumps10.1557/JMR.2004.0235 ↗
9. Interfacial stability of eutectic SnPb solder and composite 60Pb40Sn solder on Cu/Ni(V)/Ti under-bump metallization10.1557/jmr.2007.0083 ↗
10. Microstructure, orientation and damage evolution in SnPb, SnAgCu, and mixed solder interconnects under thermomechanical stress10.1016/j.mee.2012.03.005 ↗
11. Effect of aging on fatigue crack growth at Sn-Pb/Cu interfaces10.1007/BF02669424 ↗
12. Kirkendall void formation in eutectic SnPb solder joints on bare Cu and its effect on joint reliability10.1063/1.1839637 ↗
13. Isothermal aging characteristics of Sn-Pb micro solder bumps10.1016/S0026-2714(03)00060-X ↗
14. Microstructure, joint strength and failure mechanisms of SnPb and Pb-free solders in BGA packages10.1109/TEPM.2002.801649 ↗
15. The superstructure of domain-twinned η'-Cu6Sn510.1107/S0108768194004052 ↗
16. Cu/Sn interfacial reactions: thin-film case versus bulk case10.1016/S0254-0584(97)80016-8 ↗
17. Effects of aging time, strain rate and solder thickness on interfacial fracture behaviors of Sn-3Cu/Cu single crystal joints10.1016/j.mee.2009.08.021 ↗
18. Effect of isothermal aging and thermal cycling on interfacial IMC growth and fracture behavior of SnAgCu/Cu joints10.1007/s11664-010-1401-3 ↗
19. Effects of Ni layer thickness of thin-ENEPIG surface finishes on the interfacial reactions and shear strength of Sn-3.0Ag-0.5Cu solder joints during aging10.1007/s10854-019-01653-x ↗
20. Residual stresses in metal/ceramic bonded strips10.1111/j.1151-2916.1985.tb15316.x ↗
21. Modeling of elastic deformation of multilayers due to residual stresses and external bending10.1063/1.1478137 ↗
22. Stress distribution and curvature in graded semiconductor layers10.1016/S0022-0248(03)01563-X ↗
23. In situ measurement of biaxial modulus of Si anode for Li-ion batteries10.1016/j.elecom.2010.09.008 ↗
24. Fracture behaviors of Sn-Cu intermetallic compound layer in ball grid array induced by thermal shock10.1007/s11664-013-2845-z ↗
25. Characterization of IMC layer and its effect on thermomechanical fatigue life of Sn-3.8Ag-0.7Cu solder joints10.1016/j.jallcom.2012.06.104 ↗
26. Thermal and electrical properties of copper-tin and nickel-tin intermetallics10.1063/1.351487 ↗
27. FEA evaluation on solder joint reliability of CCGA
28. Size and constraint effects on interfacial fracture behavior of microscale solder interconnects10.1016/j.microrel.2012.07.033 ↗
29. Study of the thermal stress in a Pb-free half-bump solder joint under current stressing10.1063/1.2747183 ↗
30. Anisotropic grain growth and crack propagation in eutectic microstructure under cyclic temperature annealing in flip-chip SnPb composite solder joints10.1016/j.scriptamat.2013.03.018 ↗
31. In situ SEM study on tensile fractured behavior of Al/steel laser welding-brazing interface10.1016/j.matdes.2022.111320 ↗
32. Effect of substrates on the formation of Kirkendall voids in Sn/Cu joints10.1007/s40194-019-00704-5 ↗
33. Shear strength and interfacial microstructure of Sn-Ag-xNi/Cu single shear lap solder joints10.1016/j.msea.2006.08.065 ↗
34. Influence of reflow and thermal aging on the shear strength and fracture behavior of Sn-3.5 Ag solder/Cu joints10.1007/s11661-005-0138-8 ↗