Effect of solution-aging treatment on microstructure and high temperature fracture toughness of Ti60 alloy rolled sheet

Zhen Gong, Shulin Dong, Zhiyong Chen, Yingdong Qu, Ruirun Chen, Guanglong Li, Wei Zhang, Rongyi Na

Publisher page

Abstract

In this study, the Ti60 alloy rolled sheet was solution-aging treatment at different temperatures, and then the high temperature fracture toughness test was carried out on the samples after solution-aging treatment. The microstructure morphology and crack propagation behavior were studied. The original microstructure of the Ti60 alloy rolled sheet is composed of primary α phase and flocculated α phase. The microstructure of Ti60 alloy rolled sheet after solution-aging treatment is a typical bimodal structure. It is mainly composed of acicular α s phase, equiaxed α phase and lamellar α phase. The proportion of equiaxed α phase gradually increases from 46 % to 82 % with the increase of solution treatment temperature. After 1080 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment and 1090 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment, lamellar α appears inside the equiaxed α grains. After 1100 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment, the lamellar α will be transformed into acicular α s. The average K IC value of the original Ti60 alloy rolled sheet is 46.35 MPa·m 1/2. The K IC values of the samples after 1070 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment, 1080 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment and 1100 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment is approximately in the range of 44.15 MPa·m 1/2–51.33 MPa·m 1/2. But the average K IC value after 1090 °C/2 h/AC + 700 °C/2 h/AC solution-aging treatment is increased to 74.56 MPa·m 1/2. This may be due to the appearance of lamellar α, which makes the fracture toughness of Ti60 alloy rolled sheet increase significantly.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Material Properties and Applications · Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Rolling texture and its effect on tensile property of a near-α titanium alloy Ti60 plate10.1016/j.jmst.2018.10.032 ↗
2. Fracture toughness characteristics of additively manufactured Ti–6Al–4V lattices10.1016/j.euromechsol.2020.104170 ↗
3. Analysis of local crystallographic orientation in an annealed Ti60 billet10.1016/j.jmst.2018.10.014 ↗
4. Effect of texture on anisotropy at 600 °C in a near-α titanium alloy Ti60 plate10.1016/j.msea.2017.01.098 ↗
5. Effect of aging on the tensile properties and microstructures of a near-alpha titanium alloy10.1016/j.matdes.2014.01.063 ↗
6. The analysis of fracture toughness and fracture mechanism of Ti60 alloy under different temperatures10.1016/j.jallcom.2019.151899 ↗
7. A novel TWIP/TRIP near-α Ti alloy with multi-scale α-phase: the superior combination of strength and fracture toughness10.1016/j.jmrt.2023.07.247 ↗
8. Influence of thermomechanical processing and heat treatment on microstructure, tensile properties and fracture toughness of Ti-1100-0.1B alloy10.1016/j.jallcom.2013.11.014 ↗
9. Growth mechanism of αp and interface relationships between αp and αs during cooling of a near α titanium alloy10.1016/j.matdes.2022.111191 ↗
10. Effect of the initial microstructure on the deformation behavior of Ti60 titanium alloy at high temperature processing10.1016/j.jallcom.2014.08.092 ↗
11. Controlling the microstructure and fracture toughness of the Ti–5Al–5Mo–5V–1Cr–1Fe alloy by multiple heat treatments10.1016/j.jmrt.2022.02.020 ↗
12. The effects of lamellar features on the fracture toughness of Ti-17 titanium alloy10.1016/j.msea.2015.04.021 ↗
13. Fracture toughness of Ti–22Al–25Nb alloy at room and high temperatures10.1016/j.msea.2020.140009 ↗
14. Effect of solution treatments on microstructure and mechanical properties of Ti–6Al–4V alloy hot rolled sheet10.1016/j.jmrt.2023.02.192 ↗
15. Anomalous increase of fracture toughness of TiAl-based alloys at high temperature10.1016/j.matchar.2024.114215 ↗
16. Hot processing performance and fracture toughness control of Al CrFeNiCu1.5 (x = 0, 0.2, 0.4, 0.6, 0.8) high entropy alloys10.1016/j.mtcomm.2024.108566 ↗
17. Improved fracture toughness by microalloying of Fe in Ti-6Al-4V10.1016/j.matdes.2019.108251 ↗
18. The use of compact specimens to determine fracture toughness anisotropy of Ti–6Al–4V additively manufactured for repair10.1016/j.msea.2021.141779 ↗
19. Time-temperature effects in dual scale crack growth of titanium alloys10.1016/j.tafmec.2017.06.016 ↗
20. The interrelationship of fracture toughness and microstructure in a new near β titanium alloy Ti–7Mo–3Nb–3Cr–3Al10.1016/j.matchar.2014.07.018 ↗
21. Effect of microstructure on the creep properties of Ti–6Al–4V alloys: an analysis10.1007/s12666-018-1292-1 ↗
22. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
23. Effect of microstructure on creep crack growth behavior of a near-α titanium alloy IMI-83410.1007/s11661-008-9684-1 ↗
24. The fracture toughness and its prediction model for Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy with basket-weave microstructure10.1016/j.jallcom.2015.01.217 ↗
25. The interdependence of microstructure, strength and fracture toughness in a novel β titanium alloy Ti–5Al–4Zr–8Mo–7V10.1016/j.msea.2020.139248 ↗
26. Influence of phase morphology, static recrystallization, and crystallographic texture on room temperature tensile properties of Ti–6Al–4V alloy: Comparison between post-tested equiaxed, bimodal, and lamellar microstructures10.1016/j.msea.2023.144990 ↗
27. The effect of surface oxidation behavior on the fracture toughness of Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy10.1016/j.jallcom.2015.05.211 ↗