Effects of pre-stretching on mechanical properties and corrosion behavior of superplastic formed 2A97 Al Li alloy
Source abstract
Abstract
Effects of pre-stretching on mechanical properties and corrosion behavior of superplastic formed 2A97 Al Li alloy were investigated by using tensile test, intergranular corrosion test, electrochemical analysis, electron backscattering diffraction analysis and transmission electron microscopy. The results show that compared with T6 heat treatment, the T8 heat treatment effectively improves the strength by introducing more finer and more homogeneous T 1 precipitations. And the pre-stretching strain has significant influence on the microstructure and properties of superplastic formed alloy. When the pre-stretching strain reaches 4 %, the cavities formed during superplastic forming are obviously elongated along the pre-stretching direction. During 4 %–8 % pre-stretching strain, the increment of strength gradually decreases, but the elongation drops sharply. When the pre-stretching strain reaches 8 %, the elongated cavities and cracked coarse second phases result in a slight decrease in strength. The corrosion behavior of samples after heat treatment with different pre-stretching strain are obviously different. The corrosion microscopy of T6 and T82 sample is pitting with intergranular corrosion (IGC) by the grain boundary precipitation free zones (PFZ) dissolving preferentially. After 4 %–8 % pre-stretching treatments, the corrosion microscopy is only pitting by the dissolution of the matrix around T 1 precipitations. What`s more, strength and corrosion resistance are both at a high level by 4 % pre-stretching treatment.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. A review of manufacturing processes, mechanical properties and precipitations for aluminum lithium alloys used in aeronautic applications10.1016/j.heliyon.2022.e12565 ↗
2. Seventy-five years of superplasticity: historic developments and new opportunities10.1007/s10853-009-3780-5 ↗
3. Alloys for aeronautic applications: state of the art and perspectives10.3390/met9060662 ↗
4. The evolution of Al-Li base products for aerospace and space applications10.1007/s11661-012-1155-z ↗
5. Superplastic forming technology of aircraft structures for Al-Li alloy and high-strength Al alloy10.1016/S0924-0136(97)00148-9 ↗
6. G.T. Zou, S.J. Chen, Y.Q. Xu, et al, Microstructural evolution and deformation mechanisms of superplastic aluminium alloys: a review, Trans. Nonferrous Met. Soc. China. 34(10) (2024) 3069–3092.https://doi.org/10.1016/s1003-6326(24)66596-9.10.1016/S1003-6326(24)66596-9 ↗
7. Superplastic formability of Al-cu-Li alloy
8. Microstructure and properties of 2A97 aluminum-lithium alloy after different aging process
9. Study on microstructure and properties of a novel high strength aluminum lithium alloy 2A97
10. H.Y. Li, X.F. Wang, J. Bin, et al, Effect of two aging processes on microstructure and properties of alloy 2A97, J. Cent. South Univ. (Sci. Technol.). 42(5) (2011) 1261–1269. CNKI:SUN:ZNGD.0.2011–05-016.
11. Effect of thermo-mechanical treatment process on microstructure and mechanical properties of 2A97 Al-Li alloy10.1016/S1003-6326(14)63332-X ↗
12. Effect of pre-stretching processing on the corrosion behavior of 2A97 Al-Li alloy
13. Electrochemical behavior of the T1 (Al2CuLi) intermetallic compound and its role in localized corrosion of Al-2%Li-3%Cu alloys10.5006/1.3293500 ↗
14. Influence of aging at 200°C on the corrosion resistance of Al-Li and Al-Li-Cu alloys10.5006/1.3577857 ↗
15. Effect of aging on mechanical properties and localized corrosion behaviors of Al-cu-Li alloy
16. Wanhill · 2014 · 503
17. Grain-stored energy and the propagation of intergranular corrosion in AA2xxx aluminium alloys10.1002/sia.5218 ↗
18. The propagation of localized corrosion in Al-cu-Li alloy10.1002/sia.5890 ↗
19. The influence of grain structure on the corrosion behaviour of 2A97-T3 Al-Cu-Li alloy10.1016/j.corsci.2016.12.005 ↗
20. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
21. Cavitation and cavity-induced fracture during superplastic deformation10.1007/BF00349941 ↗
22. Effect of aging on microstructure and performance after superplastic deformation of fine grained 1420 Al-Li alloy10.4028/www.scientific.net/AMR.936.1647 ↗
23. Investigation of post-superplastic forming properties of AZ31 magnesium alloy10.1016/j.cirp.2007.05.067 ↗
24. The effect of superplastic deformation on subsequent service properties of fine grained 7475 Al10.1115/1.3225619 ↗
25. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al-Li-cu-X alloy10.1016/S1471-5317(00)00002-X ↗
26. Effects of coarse Al2CuLi phase on the hot deformation behavior of Al-Li alloy10.1016/j.jallcom.2019.152469 ↗
27. The cavitation and fracture characteristics of a superplastic Al-cu-Li-Zr alloy10.1016/0921-5093(89)90156-1 ↗
28. Nanocrystalline Al-mg alloy with ultrahigh strength and good ductility10.1016/j.scriptamat.2005.09.028 ↗
29. Evaluation of Dislocation Density for 1100 Aluminum with Different Grain Size during Tensile Deformation by Using In-Situ X-ray Diffraction Technique10.2320/matertrans.L-M2015803 ↗
30. Corrosion resistance of a two-stage stress-aged Al-Cu-Mg alloy: Effects of stress-aging temperature10.1016/j.jallcom.2015.10.114 ↗
31. Corrosion protection of aluminium alloy 2024-T3 in 0.05M NaCl by cerium cinnamate10.1016/j.corsci.2011.03.012 ↗
32. Effect of aging treatment on microstructure and corrosion behavior of Al-Zn-mg aluminum alloy in aqueous solutions with different aggressive ions10.1016/j.jmst.2019.09.030 ↗
33. Defect engineering and characterization of active sites for efficient electrocatalysis10.1039/D0NR08976A ↗
34. Effects of non-isothermal aging on mechanical properties, corrosion behavior and microstructures of Al-cu-mg-Si alloy10.1016/j.jallcom.2019.152960 ↗
35. Effect of cu content on quenching sensitivity relative to exfoliation corrosion susceptibility of Al-Zn-mg-(cu) alloys10.1016/j.matchar.2022.112476 ↗
36. Effect of cu content on local corrosion behavior of Al-Li alloy
37. D.A. Harringtona, P.V.D. Driessche, Mechanism and equivalent circuits in electrochemical impedance spectroscopy, Electrochim. Acta 56(23) (2011) 8005–8013.https://doi.org/10.1016/j.electacta.2011.01.067.10.1016/j.electacta.2011.01.067 ↗
38. Quantitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing cl−10.1016/j.corsci.2020.109076 ↗
39. Quantification of the influence of increased pre-stretching on microstructure-strength relationships in the Al-cu-Li alloy AA219510.1016/j.actamat.2016.02.017 ↗
40. Effect of annealing on microstructure and mechanical properties of an Al-mg-Sc-Zr alloy10.1016/j.msea.2022.142821 ↗
41. Strengthening mechanisms of an Al-mg-Sc-Zr alloy10.1016/S1359-6454(02)00258-6 ↗
42. Ageing response of a Al-cu-Li 2198 alloy10.1016/j.matdes.2014.04.063 ↗
43. Effect of superplastic deformation on microstructures, texture, and mechanical properties of 2A97 Al-cu-Li alloy10.1016/j.msea.2023.145972 ↗
44. Quantification and modelling of the microstructure/strength relationship by tailoring the morphological parameters of the T1 phase in an Al-cu-Li alloy10.1016/j.actamat.2014.04.046 ↗
45. Size distribution and volume fraction of T1 phase precipitates from TEM images: direct measurements and related correction10.1016/j.micron.2015.06.002 ↗
46. Microstructure evolution and strengthening mechanism of Al-Li alloy during thermo-electromagnetic forming process10.1016/j.jmatprotec.2023.117922 ↗
47. Effects of heat treatment and pre-stretching on the mechanical properties and microstructure evolution of extruded 2050 Al-cu-Li alloy10.1016/j.msea.2022.143236 ↗
48. Microstructure evolution and deformation mechanisms of a banded-grained 2A97 Al-cu-Li alloy during superplastic deformation10.1016/j.msea.2023.145178 ↗
49. Corrosion behaviour of 2A97-T6 Al-cu-Li alloy: the influence of non-uniform precipitation10.1016/j.corsci.2017.12.010 ↗
50. Corrosion behaviour of 2A97-T8 Al-cu-Li alloy extrusion10.1016/j.jallcom.2021.162872 ↗
51. Effects of aging treatment on the intergranular corrosion behavior of Al-cu-mg-ag alloy10.1016/j.jallcom.2015.03.174 ↗
52. Electrochemical characteristics of intermetallic phases in aluminum alloys: an experimental survey and discussion10.1149/1.1869984 ↗
53. Corrosion behavior of anodized Al-cu-Li alloy: the role of intermetallic particle-introduced film defects10.1016/j.corsci.2019.108110 ↗