In situ high-temperature transmission electron microscopy investigation of dynamic element migration for Sm-Co-Fe-Cu-Zr sintered magnets
Source abstract
Abstract
The investigation delved into the dynamic migration of elements and the evolution of interface structures within the Sm(Co balFe 0.09Cu 0.09Zr 0.03) 7.2 magnet as temperature increased, employing high-temperature transmission electron microscopy. Notably, the Cu distribution exhibited temperature susceptibility. Elevating the temperature from room temperature (RT) to 400 °C led to a notable expansion in the distribution width of Cu, ranging from 28.5 to 50.8 nm. Simultaneously, the average Cu content at the cell boundaries decreased from 14.4 to 11.6 at.%. According to the high-temperature in-situ experimental results of the transmission electron microscopy thin-film samples, the derived diffusion coefficients, D 300 °C and D 400 °C, were determined as 0.0525 nm 2/s and 1.414 nm 2/s, respectively. The significantly higher D 400°C compared to D 300 °C underscores the considerable influence of temperature on Cu element diffusion behavior. The simulation results demonstrate that the trend of magnetic properties variation at different temperatures closely aligns with the observed trend. Subsequent calculation of the temperature coefficient of intrinsic coercivity (β) reveals that |β 300 – 400 °C| is notably higher than |β RT-300 °C |. This suggests a substantial impact of Cu diffusion-induced deterioration on the β. Moreover, micromagnetic simulation results delineated the reverse magnetization process for magnets at varying temperatures, revealing that the presence of the Cu diffusion region diminished the pinning effect of the cell boundary phase. Furthermore, a wider Cu diffusion region facilitated easier magnetic moment reversal at the cell boundary phase, resulting in a marked deterioration of intrinsic coercivity. This elucidates that the formation of the Cu diffusion region stands as one of the primary reasons for the sharp decline in magnetic properties of Sm 2Co 17-type magnets under high-temperature conditions.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Magnetic Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. High temperature 2:17 magnets: relationship of magnetic properties to microstructure and processing10.1109/20.908808 ↗
2. Recent progress in high temperature permanent magnetic materials10.1007/s12598-013-0162-6 ↗
3. Sm-co high-temperature permanent magnet materials
4. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
5. New rare-earth permanent magnets with an intrinsic coercivity of 10 kOe at 500 °C10.1063/1.369832 ↗
6. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
7. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
8. Application of high temperature magnetic materials10.1109/20.908805 ↗
9. Liu · 2009
10. Overview of composition and technique process study on 2:17-type Sm–Co high-temperature permanent magnet10.1007/s12598-020-01514-1 ↗
11. Sm2(Co,Fe,Cu,Zr)17 magnets for use at temperature ≥400 °C10.1063/1.367937 ↗
12. Effect of iron on the high temperature magnetic properties and microstructure of Sm10.1063/1.369304 ↗
13. Sm(Co, Fe, Cu, Zr)z sintered magnets with a maximum operating temperature of 500°C10.1016/j.jmmm.2006.01.107 ↗
14. A new class of Sm-TM magnets for operating temperatures up to 550°C10.1109/20.908807 ↗
15. Effect of Zr on the microstructure and magnetic properties of Sm(CobalFe0.1Cu0.088Zrx)8.5 magnets10.1063/1.371874 ↗
16. Microstructure and high temperature magnetic properties of Sm(co, cu, Fe, Zr)z (z=6.7-9.1) permanent magnets10.1063/1.369597 ↗
17. Effect of Z value on high temperature performance of Sm(co, Fe, cu, Zr)z with z = 6.5-7.3
18. Effects of Sm content on thermal stability of Sm2Co17 sintered magnets10.3938/jkps.63.784 ↗
19. Cellular microstructure modification and high temperature performance enhancement for Sm2Co17-based magnets with different Zr contents10.1016/j.jmst.2021.12.037 ↗
20. Microstructural analysis during the step cooling annealing of iron rich Sm(Co0.65Fe0.26Cu0.07Zr0.02)7.8 anisotropic sintered magnets
21. Crystalline and magnetic microstructures of iron rich Sm(Co0.65Fe0.26Cu0.07Zr0.02)7.8 sintered magnets: isothermal aging effect10.1016/j.jmmm.2018.06.047 ↗
22. Investigation on microstructure and magnetic properties of Sm2Co17 magnets aged at high temperature10.1063/1.3563084 ↗
23. Dependence of macromagnetic properties on the microstructure in high-performance Sm2Co17-type permanent magnets10.1016/j.jmmm.2020.166942 ↗
24. Correlation of microchemistry of cell boundary phase and interface structure to the coercivity of Sm(Co0.784Fe0.100Cu0.088Zr0.028)7.19 sintered magnets10.1016/j.actamat.2016.12.050 ↗
25. Evolution of magnetic domain structures and coercivity in high-performance SmCo 2:17-type permanent magnets10.1016/j.actamat.2005.10.026 ↗
26. Direct evidence for cu concentration variation and its correlation to coercivity in Sm(Co0.74Fe0.1Cu0.12Zr.04)7.4 ribbons10.1016/j.scriptamat.2009.01.006 ↗
27. Development of high-coercivity state in high-energy and high-temperature Sm-co-Fe-cu-Zr magnets upon step cooling
28. Phase transformation in anisotropic Nanocrystalline SmCo5 magnets10.1016/j.jmmm.2018.08.041 ↗
29. Attractive-domain-wall-pinning controlled Sm-co magnets overcome the Coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
30. Saturation magnetization and anisotropy fields in the Sm(Co1-xCux)5 phases10.1063/1.355423 ↗
31. Micromagnetic theory of the pinning of domain walls at phase boundaries10.1016/S0921-4526(02)01113-4 ↗
32. Analysis of the temperature dependence of the coercive field of Sm2Co17 based magnets10.1016/S1359-6462(02)00619-X ↗