Effect of iron content on the structure and properties of Al4Ca0.8Mn(0.5, 1.3)Fe (wt%) alloy after high-pressure torsion
Source abstract
Abstract
The advantages of the Al–Ca–Mn–Fe alloys are their lightness, good ductility, high corrosion resistance, and excellent casting properties, but the main disadvantage is their low strength. Therefore interest in current work lies in improving the strength properties of these alloys though the severe plastic deformation method. The Al–4Ca–0.8Mn–(Fe) eutectic-type alloys with an iron content 0.5 and 1.3 wt% were processed by severe plastic deformation using the high-pressure torsion technique (HPT). HPT of the 20-mm diameter samples was carried out at room temperature through three revolutions. To characterize the samples we used the microstructural studies by an optical microscope, scanning microscope, and transmission microscope, the microhardness measurements, the hardening`s thermal stability analysis, the tensile tests, and the electrical conductivity measurements. It was found that as a result of HPT, a bimodal, but predominantly nanocrystalline microstructure was formed in the alloys and a simultaneous improvement in strength (4–6.5 times) and relative elongation (1.1–1.7 times) was achieved while maintaining a moderately low electrical resistance. Increasing the iron content from 0.5 to 1.3 wt% in the alloy provides a smaller grain size and a higher level of strength after HPT. The microstructural mechanisms of increasing strength and ductility in the alloys with different iron content are discussed. The effect of post-processing annealing on the mechanical properties of the alloys was studied.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Ultrafine-grained aluminium alloys: processes, structural features and properties
2. Equal-channel angular pressing of commercial aluminum alloys: grain refinement, thermal stability and tensile properties10.1007/s11661-000-0011-8 ↗
3. Plastic flow, structure and mechanical properties in pure Al deformed by twist extrusion10.1016/j.msea.2009.06.005 ↗
4. Continuous processing of ultrafine grained Al by ECAP-conform10.1016/j.msea.2004.04.021 ↗
5. Properties and deformation behaviour of severe plastic deformed aluminium alloys10.1016/j.jmatprotec.2006.07.038 ↗
6. Improving the combination of electrical conductivity and tensile strength of Al 1070 by rotary swaging deformation10.1016/j.rinp.2019.102236 ↗
7. Microstructure, hardness evolution and thermal stability of binary Al−7Mg alloy processed by ECAP with intermediate annealing10.1016/S1003-6326(14)63348-3 ↗
8. Effect of ECAP temperature on microstructure and mechanical properties of Al–Zn–Mg–Cu alloy10.1016/j.pnsc.2016.03.003 ↗
9. Microstructure evolution and aging kinetics of Al–Mg–Si and Al–Mg–Si–Sc alloys processed by ECAP10.4028/www.scientific.net/MSF.503-504.493 ↗
10. Effect of ECAP on microstructure and mechanical properties of a commercial 6061 Al alloy produced by powder metallurgy10.1016/S0925-8388(03)00008-2 ↗
11. Effect of severe plastic deformation on the structure and mechanical properties of Al-Cu-Mg alloy10.1088/1757-899X/63/1/012081 ↗
12. Characterisation of high pressure torsion processed 7150 Al–Zn–Mg–Cu alloy10.1016/j.msea.2012.05.026 ↗
13. Significance of grain refinement on microstructure and mechanical properties of an Al-3% Mg alloy processed by high-pressure torsion10.1016/j.jallcom.2016.06.194 ↗
14. Damage and strengthening mechanisms in severely deformed commercially pure aluminum: experiments and modeling10.1016/j.msea.2020.140224 ↗
15. Effect of post-aging on microstructure and mechanical properties of an ultrafine-grained 6061 aluminum alloy
16. Mechanical alloying and phase transition of the immiscible Al/Zn system during high-pressure torsion10.1016/S1003-6326(23)66358-7 ↗
17. Review: overcoming the paradox of strength and ductility in ultrafine-grained materials at low temperatures10.1007/s10853-015-9143-5 ↗
18. Simultaneously improving the strength and ductility of an Al-5.5Mg-1.6Li-0.1Zr alloy via warm multi-pass ECAP10.1016/j.matchar.2019.03.043 ↗
19. Achieve high plasticity and strength in 6016 alloy by high-pressure torsion combined with post-aging treatments10.1016/j.jmrt.2022.12.150 ↗
20. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
21. On the relation between the strength and the plasticity of metallic materials10.1134/S0036029516100050 ↗
22. High strength Al-La, Al-Ce, and Al-Ni eutectic aluminum alloys obtained by high-pressure torsion10.3390/ma14216404 ↗
23. Mechanical and electrical properties of an ultrafine grained Al-8.5 wt.% RE (RE= 5.4 wt.% Ce, 3.1 wt.% La) alloy processed by severe plastic deformation10.1016/j.matdes.2015.10.163 ↗
24. Thermodynamic assessment of the Al–Ca binary system using random solution and associate models10.1016/S0925-8388(01)01713-3 ↗
25. Remarkable thermal stability of the Al-Ca-Ni-Mn alloy manufactured by laser-powder bed fusion10.1016/j.matlet.2020.129074 ↗
26. Structure and mechanical properties of Al – 6% Ca – 1% Fe alloy foundry goods, obtained by die casting10.17580/tsm.2017.03.11 ↗
27. Microstructure and phase composition of the eutectic Al – Ca alloy, additionally alloyed with small additives of zirconium, scandium and manganese10.17580/nfm.2017.02.09 ↗
28. Influence of the thermal treatment on the deformation-induced precipitation of a hypoeutectic Al–7 wt% Si casting alloy deformed by high-pressure torsion10.1016/j.jallcom.2010.09.122 ↗
29. Effect of the eutectic Al-(Ce,La) phase morphology on microstructure, mechanical properties, electrical conductivity and heat resistance of Al-4.5(Ce,La) alloy after SPD and subsequent annealing10.1016/j.jallcom.2019.05.006 ↗
30. Structure and mechanical properties of Al-Ca alloys processed by severe plastic deformation10.1016/j.msea.2019.138410 ↗
31. Improvement of strength–ductility balance of Al–Ca–Mn–Fe alloy by severe plastic deformation10.1016/j.matlet.2023.134797 ↗
32. A review on high-pressure torsion (HPT) from 1935 to 198810.1016/j.msea.2015.11.074 ↗
33. Formation and characterization of Al10CaFe2 compound in Al-Ca-Fe alloys10.1016/S1003-6326(23)66404-0 ↗
34. Phase transitions in Cu-based alloys under high pressure torsion10.1016/j.jallcom.2016.12.057 ↗
35. Physics of megaplastic (severe) deformation in solids10.1134/S1063783410060089 ↗
36. Understanding the role of Ca segregation on thermal stability, electrical resistivity and mechanical strength of nanostructured aluminum10.1016/j.msea.2020.140108 ↗
37. General view of severe plastic deformation in solid state10.1016/j.matlet.2014.10.052 ↗
38. Phase transitions induced by severe plastic deformation: steady-state and equifinality10.3139/146.111215 ↗
39. Dependence of electrical resistivity on temperature and composition of Al–Cu alloys10.1179/1433075X11Y.0000000041 ↗
40. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
41. The cause of high-angle boundaries formation at the severe plastic deformation of crystals: deformation fragmentation or dynamic recrystallization
42. A physical model for the initial stages of the fragmentation of polycrystals in the process of developed plastic deformation10.1134/S0031918X17120110 ↗
43. Disclinations in large-strain plastic deformation and work-hardening
44. Dynamic recrystallization and recovery during high-pressure torsion: experimental evidence by torque measurement using ring specimens10.1016/j.msea.2012.08.132 ↗
45. Self-organization of plastic shears in localized deformation macrobands in the neck of high-strength polycrystals, its role in material fracture under uniaxial tension10.1016/j.physme.2008.03.006 ↗
46. The Hall–Petch breakdown in nanocrystalline metals: a crossover to glass-like deformation10.1016/j.actamat.2007.07.020 ↗
47. Effect of the structural factor on the inverse Hall–Petch dependence in nanocrystals10.3103/S1062873814110288 ↗
48. The strength–grain size relationship in ultrafine-grained metals10.1007/s11661-016-3499-2 ↗
49. Thermal stability of Al-Ca and Al-Ce alloys obtained by high-pressure torsion10.1007/s11665-021-06105-4 ↗