Research on crack regulation in laser deposition manufacturing of Inconel718 superalloy through interlayer temperature control with air knife cooling
Source abstract
Abstract
This study aims to address the issue of crack formation in Inconel718 superalloy during the laser deposition manufacturing process. By using an air knife cooling device to regulate the interlayer temperature during the manufacturing process, the study investigates the impact of interlayer temperature on the microstructure, grain boundaries, and crack formation in Inconel718 superalloy components, and explores methods to reduce crack sensitivity by controlling interlayer temperature. The research findings reveal that cracks in the Inconel718 alloy during laser deposition manufacturing are mainly caused by element segregation and concentration of residual stress, with cracks typically propagating along long-chain Laves phases, especially at large angle grain boundaries where the effect is more pronounced. These areas provide a stable liquid film environment for crack growth, making internal stress concentration the main factor driving crack initiation. When the interlayer temperature is controlled at 20 °C, it can accelerate the cooling rate of the molten pool, increase the temperature gradient, and reduce the duration of high temperature in the molten pool, thereby promoting the formation of discrete fine Laves phases, refining the grain size, and reducing the proportion of large angle grain boundaries, effectively suppressing the occurrence of cracks. This study provides an effective crack control strategy for the laser deposition manufacturing of Inconel718 superalloy.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Advanced Machining and Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Microstructure and mechanical behavior of bright crescent areas in Inconel 718 sample fabricated by selective laser melting10.1016/j.matdes.2020.109259 ↗
2. Boundary liquation and interface cracking characterization in laser deposition of Inconel 738 on directionally solidified Ni-based superalloy10.1016/j.scriptamat.2005.03.047 ↗
3. Avoiding cracks in additively manufactured non-weldable directionally solidified Ni-based superalloys
4. Development and characterization of multilayer laser cladded high speed steels
5. Investigation of grain boundary segregation evolution and corrosion behavior in 7050 aluminum alloy under oscillating laser melting10.1016/j.jallcom.2024.177524 ↗
6. Causes analysis on cracks in nickel-based single crystal superalloy fabricated by laser powder deposition additive manufacturing10.1016/j.matdes.2018.10.042 ↗
7. Cracks and process control in laser powder bed fusion of Al-Zn-Mg alloy10.1016/j.jmapro.2022.06.066 ↗
8. Laser cladding of Inconel 718 powder on a non-weldable substrate: clad bead geometry-solidification cracking relationship10.1016/j.jmapro.2020.04.045 ↗
9. Welding Metallurgy and Weldability of Nickel-Base Alloys
10. Hot cracking during the fabrication of Inconel 625/stainless steel 308 L functionally graded material by dual-wire arc additive manufacturing10.1016/j.jmapro.2022.08.018 ↗
11. Laser Powder Bed Fabrication of Nickel-Base Superalloys: Influence of Parameters; Characterisation, Quantification and Mitigation of Cracking
12. Combining alloy and process modification for micro-crack mitigation in an additively manufactured Ni-base superalloy
13. Alloys-by-design: application to new superalloys for additive manufacturing10.1016/j.actamat.2020.09.023 ↗
14. Laser Powder Bed Fabrication of Nickel-Base Superalloys: Influence of Parameters; Characterisation, Quantification and Mitigation of Cracking
15. Combining alloy and process modification for Micro-crack mitigation in an additively manufactured Ni-base Superalloy
16. Sun · 2021
17. Enhanced wear resistance of Ti reinforced Inconel 718 superalloy manufactured by laser directed energy deposition10.1016/j.matchar.2024.113736 ↗
18. Micro-cracking, microstructure and mechanical properties of Hastelloy-X alloy printed by laser powder bed fusion: as-built, annealed and hot-isostatic pressed
19. Influence of post heat treatments on anisotropy of mechanical behaviour and microstructure of Hastelloy-X parts produced by selective laser melting10.1016/j.msea.2016.04.086 ↗
20. Liquid-induced healing of cracks in nickel-based superalloy fabricated by laser powder bed fusion10.1016/j.actamat.2024.119731 ↗
21. Avoiding cracks in additively manufactured non-weldable directionally solidified Ni-based superalloys
22. Cracking suppression in additive manufacturing of hard-to-weld nickel-based superalloy through layer-wise ultrasonic impact peening10.1016/j.jmapro.2022.05.041 ↗
23. The influence of columnar to equiaxed transition on deformation behavior of FeCoCrNiMn high entropy alloy fabricated by laser-based directed energy deposition
24. Combining alloy and process modification for micro-crack mitigation in an additively manufactured Ni-base superalloy
25. New alloy design approach to inhibiting hot cracking in laser additive manufactured nickel-based superalloys10.1016/j.actamat.2023.118736 ↗
26. A novel method to prevent cracking in directed energy deposition of Inconel 738 by in-situ doping Inconel 71810.1016/j.matdes.2020.109214 ↗
27. Cracking inhibition of nano-TiC reinforced René 104 superalloy fabricated by selective laser melting10.1016/j.jallcom.2021.160413 ↗
28. Additive manufacturing of nickel-based superalloy Inconel 718 by selective electron beam melting: processing window and microstructure10.1557/jmr.2014.192 ↗
29. As-built and post-treated microstructures of an Electron beam melting (EBM) produced nickel-based Superalloy10.1007/s11661-020-06037-z ↗
30. Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling10.1016/j.jallcom.2016.01.250 ↗
31. Healing cracks in selective laser melting by 3D laser shock peening
32. Two-step heat treatment for laser powder bed fusion of a nickel-based superalloy with simultaneously enhanced tensile strength and ductility
33. Laser powder bed fusion of Hastelloy X: effects of hot isostatic pressing and the hot cracking mechanism10.1016/j.msea.2018.07.008 ↗
34. Inhibiting of softening behavior in AA2219 laser welded joints10.1016/j.msea.2024.147742 ↗
35. Effect of double-pulse frequency and post-weld heat treatment on microstructure and mechanical properties of metal-inert gas welded Al–Mg–Si alloy joints10.1016/j.msea.2024.147029 ↗
36. Investigations on the microstructure and crack formation of IN738LC samples processed by selective laser melting using Gaussian and doughnut profiles10.1016/j.matdes.2015.10.027 ↗
37. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 71810.1016/j.matdes.2015.10.155 ↗
38. Effect of heat input on heat affected zone cracking in laser welded ATI Allvac 718Plus superalloy10.1016/j.msea.2006.11.054 ↗
39. Cracking behavior and control of Rene 104 superalloy produced by direct laser fabrication10.1016/j.jmatprotec.2015.06.002 ↗
40. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy10.1016/j.jallcom.2014.06.172 ↗
41. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
42. On the relationship between critical tensile stress and fracture toughness in mild steel10.1016/0022-5096(73)90008-2 ↗
43. A generalised hot cracking criterion for nickel-based superalloys additively manufactured by electron beam melting
44. Effects of heat input on microstructure of tungsten inert gas welding used hastelloy X
45. Effect of heat treatment on liquation cracking in continuous Fiber and pulsed Nd:YAG laser welding of HASTELLOY X alloy10.1007/s11661-017-4300-x ↗
46. Solidification cracking of superalloy single- and bi-crystals10.1016/j.actamat.2004.03.047 ↗
47. An improved prediction of residual stresses and distortion in additive manufacturing10.1016/j.commatsci.2016.10.003 ↗
48. Laser melting deposition of K403 superalloy: the influence of processing parameters on the microstructure and wear performance10.1016/j.jallcom.2019.07.102 ↗
49. Effect of weld cooling rate on laves phase formation in Inconel 718 fusion zone10.1016/j.jmatprotec.2013.09.006 ↗
50. Microstructures and stress rupture properties of pulse laser repaired Inconel 718 superalloy after different heat treatments10.1016/j.jallcom.2018.08.063 ↗
51. A new approach to improve strength and ductility of laser powder deposited Inconel 718 thin-wall structure10.1016/j.msea.2022.143871 ↗
52. The initiation and propagation mechanism of the overlapping zone cracking during laser solid forming of IN-738LC superalloy10.1016/j.jallcom.2018.03.366 ↗
53. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
54. Last-stage solidification of alloys: theoretical model of dendrite-arm and grain coalescence10.1007/s11661-003-0083-3 ↗
55. Hirth · 1982
56. Recent advances in hot tearing during casting of aluminium alloys10.1016/j.pmatsci.2020.100741 ↗
57. Solidification cracking of superalloy single- and bi-crystals10.1016/j.actamat.2004.03.047 ↗
58. Chauvet · 2018
59. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗