Abstract
In single-step metal Additive Manufacturing (AM) processes, thermal cycling resulting from inappropriate scanning length and deposition height will eventually cause the cracking and deformation of the deposits, which will significantly damage object performance and intended applications. In this work, a unique altering thermal cycling pathway is proposed to efficiently control the cracking and deformation of AMed CuSi3Mn alloys without either using any auxiliary equipment or adjusting the alloy composition. With the help of the Intrinsic Heat Treatment (IHT) caused by secondary or multiple heating and cooling between the subsequent layers and the previous layers, a crack-free cylindric part fabricated by the Gas Metal Arc assisted Directed Energy Deposition (GMA-DED) based on Surface Tension Transfer (STT) is finally obtained, at the same time, the experimental results were verified by the numerical simulation. This further contributes to a superior deposition strategy to control the crack and deformation behavior on the metal AM.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Study on the interfacial characteristics and crack propagation of 630 stainless steel fabricated by hybrid additive manufacturing (additional DED building on L-PBFed substrate)10.1016/j.msea.2022.142657 ↗
2. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
3. Additive manufacturing of structural materials10.1016/j.mser.2020.100596 ↗
4. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
5. Chain-Tsuan Liu, in situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
6. In-situ grain structure control in directed energy deposition of Ti6Al4V
7. Epitaxy and microstructure evolution in metal additive manufacturing10.1146/annurev-matsci-070115-031728 ↗
8. Machine learning customized novel material for energy-efficient 4D printing10.1002/advs.202206607 ↗
9. Effect of intrinsic heat treatment on microstructure and hardness of additively manufactured Inconel 625 alloy by directed energy deposition10.1016/j.matdes.2022.111279 ↗
10. Towards controlling intrinsic heat treatment of maraging steel during laser directed energy deposition10.1016/j.scriptamat.2021.113973 ↗
11. Peritectic titanium alloys for 3D printing10.1038/s41467-018-05819-9 ↗
12. Inducing stable alpha plus beta microstructures during selective laser melting of Ti-6Al-4V using intensified intrinsic heat treatments10.3390/ma10030268 ↗
13. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
14. Atmospheric corrosion of Cu-Si-Mn bronze for contemporary art under simulated runoff and continuous immersion conditions10.1016/j.corsci.2022.110442 ↗
15. Corrosion evaluation of traditional and new bronzes for artistic castings10.1016/j.matchemphys.2005.06.034 ↗
16. Material properties of gradient copper-nickel alloy fabricated by wire arc additive manufacturing based on bypass-current PAW10.1016/j.jmapro.2022.09.037 ↗
17. Investigations on the weld metal composition and associated weld metal cracking in laser beam welded steel copper dissimilar joints10.1016/j.jmatprotec.2021.117178 ↗
18. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
19. Design strategies for bi-metallic additive manufacturing in the context of wire and arc directed energy deposition10.1016/j.matdes.2022.110496 ↗
20. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
21. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
22. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
23. Rapid surface defects detection in wire and arc additive manufacturing based on laser profilometer10.1016/j.measurement.2021.110503 ↗
24. Invited review article: strategies and processes for high quality wire arc additive manufacturing
25. Laser powder bed fusion (L-PBF) of Cu and CuCrZr parts: influence of an absorptive physical vapor deposition (PVD) coating on the printing process
26. Nanoparticle-enhanced absorptivity of copper during laser powder bed fusion
27. Additive manufacturing of Ni-based superalloys: residual stress, mechanisms of crack formation and strategies for crack inhibition
28. Multi-scale defects in powder-based additively manufactured metals and alloys10.1016/j.jmst.2022.02.015 ↗
29. Direct laser deposition of crack-free CM247LC thin walls: mechanical properties and microstructural effects of heat treatment10.1016/j.matdes.2021.110123 ↗
30. Microstructure and mechanical properties of laser DED produced crack-free Al 7075 alloy: effect of process parameters and heat treatment10.1016/j.msea.2022.144075 ↗
31. Effect of laser pulse power on solidification cracking susceptibility in surface processing of a high carbon high chromium tool steel10.1016/j.cirpj.2022.06.005 ↗
32. Grain refinement and crack inhibition of hard-to-weld Inconel 738 alloy by altering the scanning strategy during selective laser melting10.1016/j.matdes.2021.109940 ↗
33. Niobium nanoparticle-enabled grain refinement of a crack-free high strength Al-Zn-Mg-Cu alloy manufactured by selective laser melting10.1016/j.jallcom.2021.163427 ↗
34. Review on field assisted metal additive manufacturing10.1016/j.ijmachtools.2023.104032 ↗
35. Scanning strategy induced cracking and anisotropic weakening in grain texture of additively manufactured superalloys
36. A study of the influence of novel scan strategies on residual stress and microstructure of L-shaped LPBF IN718 samples10.1016/j.matdes.2022.110386 ↗
37. Effects of scanning strategies on residual stress and deformation by high-power direct energy deposition: island size and laser jump strategy between islands10.1016/j.jmapro.2021.12.054 ↗
38. Study of the behavior of the electric arc in pulsed GMAW influenced by magnetic oscillation using shielding gas mixtures with different CO2 content10.1007/s40430-021-03033-1 ↗
39. The GMAW-STT, an advanced welding process for root pipe and sheet welding