Microstructure evolution and tensile fracture behavior of AZ91/GWZ831K laminated heterostructured material fabricated via wire arc directed energy deposition
Source abstract
Abstract
In this study, the AZ91/GWZ831K laminated heterostructured material (LHM) were successfully fabricated using wire arc directed energy deposition (WA-DED) technology. The microstructure, mechanical properties, and tensile fracture behavior of the fabricated composite were systematically investigated. The results indicate that a transition zone, consisting of blocky Al 2 Gd and branched (Mg, Al) 3 Gd phases, formed at the heterogeneous interface. The grain structure exhibited alternating coarse and fine grain distributions. The tensile properties showed significant anisotropy, with the ultimate tensile strength (248.5 ± 2.7 MPa) and elongation (14.5 ± 0.42 %) along the traveling direction (TD) were 16 % and 63 % higher, respectively, than those along the building direction (BD). This improvement is primarily attributed to the effective heterogeneous deformation-induced strengthening effect. In-situ X-ray computed tomography (XCT) tensile tests were conducted to evaluate the damage evolution and failure mechanisms of the laminated heterostructured. The defects in the as-deposited specimens were mainly concentrated on the AZ91 alloy side near the interface. Damage evolution under tensile deformation primarily involved the coalescence of micro-voids and the merging of cracks with adjacent pores, while the brittle Al 2 Gd phase acted as the preferential nucleation site for cracks. This study elucidates the synergistic effect of interface characteristics and stress state on the damage behavior in laminated heterostructures, providing valuable insights for the fabrication of heterostructured Mg alloy components by WA-DED.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. On the excellent strength-ductility synergy of wire-arc directed energy deposited Mg-Gd-Y-Zn-Zr alloy via manipulating precipitates
2. The role and significance of magnesium in modern day research-a review10.1016/j.jma.2021.05.012 ↗
3. Achieving high strength-ductility of AZ91 magnesium alloy via wire-arc directed energy deposition assisted by interlayer friction stir processing
4. Microstructure evolution and its correlations with mechanical properties and corrosion behavior of Mg-9Gd-3Y-2Zn-0.5Zr alloy fabricated by wire-arc directed energy deposition10.1016/j.matchar.2025.115262 ↗
5. Coupling hot isostatic pressing and laser powder bed fusion: a new strategy to manufacture defect-free CuCrZr-316L steel multi-material structures10.1016/j.matdes.2024.112914 ↗
6. Improving mechanical properties of laminate heterogeneous GW103K/AZ31 alloys10.1016/j.jallcom.2023.169156 ↗
7. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
8. Strain hardening and ductility in a coarse-grain/nanostructure laminate material10.1016/j.scriptamat.2015.03.006 ↗
9. Research progress of heterogeneous structure magnesium alloys: a review10.1016/j.jma.2024.04.001 ↗
10. Improved impact toughness of laminate heterogeneous AZ31/GW103K alloys by interface delamination10.1016/j.msea.2023.144882 ↗
11. Microstructure and mechanical properties of Mg/Mg bimetal composites fabricated by hot-pressing diffusion and co-extrusion10.1016/j.msea.2019.138194 ↗
12. On the rule of mixtures for bimetal composites10.1016/j.msea.2017.08.005 ↗
13. Improving the tensile ductility of metal matrix composites by laminated structure: a coupled X-ray tomography and digital image correlation study10.1016/j.scriptamat.2017.03.030 ↗
14. Additive manufacturing of multi-scale heterostructured high-strength steels10.1080/21663831.2021.1904299 ↗
15. Fabrication and characterization of laminated heterostructured material with ER120 S-G and SS316L using wire and arc additive manufacturing10.1016/j.jallcom.2024.178293 ↗
16. Microstructure and mechanical properties of Al-Mg-Si/Al-Mg-Sc laminated composite fabricated by wire-arc directed energy deposition10.1016/j.msea.2024.146194 ↗
17. Wire and arc additive manufacturing of dissimilar 2319 and 5B06 aluminum alloys10.1016/j.jmst.2022.02.024 ↗
18. Heterogeneous interfaces of aluminum bronze/Inconel 718 dissimilar alloys under different wire arc directed energy deposition sequences
19. Tailoring interface properties in wire-arc directed energy deposited dissimilar aluminum alloys through interlayer laser shock peening10.1080/17452759.2025.2469155 ↗
20. Multi-wire arc additive manufacturing of TC4-Nb-NiTi bionic layered heterogeneous alloy: microstructure evolution and mechanical properties10.1016/j.matchar.2023.113001 ↗
21. Phase equilibria and solidification behavior of Mg-Al-Gd casting alloys10.1016/S1003-6326(23)66456-8 ↗
22. Excellent strength-ductility synergy property of wire-arc additively manufactured Mg-Gd-Y-Zr alloy investigated by heat treatment10.1016/j.jma.2025.03.026 ↗
23. Processing, microstructure, and mechanical properties of wire arc additively-manufactured AZ91 magnesium alloy using cold arc process10.1016/S1003-6326(24)66667-7 ↗
24. Exploration microstructural evolution and wear mechanisms of wire arc additive manufacturing NiTi/Nb bionic composite materials10.1016/j.triboint.2024.110154 ↗
25. Effect of deposition sequence on microstructure and mechanical properties of 18Ni300-Ni20 fabricated using laser-directed energy deposition10.1016/j.matchar.2025.115068 ↗
26. Recent advancements in thermal conductivity of magnesium alloys10.1016/j.jma.2024.02.007 ↗
27. Improved strength-ductility synergy of directed energy deposited AZ31 magnesium alloy with cryogenic cooling mode10.1080/17452759.2023.2170252 ↗
28. Microstructures and mechanical properties of a high pressure die-cast Mg–4Al−4Gd−0.3Mn alloy10.1016/j.msea.2019.138254 ↗
29. Excellent isotropic mechanical properties of directed energy deposited Mg-Gd-Y-Zr alloys via establishing homogeneous equiaxed grains embedded with dispersed nano-precipitation
30. P. Bai, J. Wang, Z. Zhao, Wenbo D., D. Tie, C. Cai, R. Zhang, F. Wang. Microstructure and mechanical properties of Mg-Gd-Y-Zn-Zr alloy fabricated by cold metal transfer wire arc additive manufacturing. J. Mater. Res. Technol. 27: 5805–5821. Doi: https://doi.org/10.1016/j.jmrt.2023.10.265.10.1016/j.jmrt.2023.10.265 ↗
31. Effect of Al addition on microstructure and mechanical properties of as-cast Mg-4Y-3Nd alloy10.1080/14786435.2019.1680888 ↗
32. Microstructure, tensile properties and creep behaviors of as-cast Mg–2Al–1Zn–xGd (x = 1, 2, 3, and 4 wt.%) alloys10.1016/j.jallcom.2012.01.084 ↗
33. The formation mechanism of the lamellar phase precipitated during solid solution treatment in the Mg-Gd-Al alloy10.1016/j.jmrt.2020.08.024 ↗
34. Influences of Al and high shearing dispersion technique on the microstructure and creep resistance of Mg-2.85Nd-0.92Gd-0.41Zr-0.29Zn alloy10.1016/j.msea.2019.138215 ↗
35. Tensile fracture behaviors of a laser powder deposited Fe-30Mn-10Cr-10Co-3Ni high-entropy alloy: in situ x-ray computed microtomography study10.1016/j.msea.2022.142948 ↗
36. In-situ X-ray computed tomography tensile tests and analysis of damage mechanism and mechanical properties in laser powder bed fused invar 36 alloy10.1016/j.jmst.2023.08.014 ↗
37. Failure of metals I: brittle and ductile fracture10.1016/j.actamat.2015.12.034 ↗
38. On the damage and fracture of commercially pure magnesium using x-ray microtomography10.1016/j.msea.2016.08.095 ↗
39. Effects of arc oscillation on interface behavior and properties of additive-manufactured 2319/5356 dissimilar aluminum alloy
40. Effects of Al addition on the microstructure and mechanical properties of Mg-4Y alloys10.1080/02670836.2017.1353664 ↗
41. Achieving excellent strength–ductility combination of Al-aided Mg-Gd-Al-Zr-Zn alloys fabricated by cold metal transfer-based wire-arc directed energy deposition via uniform equiaxed grains and multiple precipitates10.1016/j.tws.2024.111980 ↗
42. Crystal structure, phase content, and tensile properties of As-cast Mg-Gd-Y-Al alloys
43. High-strength Mg-10Gd-3Y-1Zn-0.5Zr alloy fabricated by wire-arc directed energy deposition: phase transformation behavior and mechanical properties
44. Phase stability, electronic, elastic and thermodynamic properties of Al-RE intermetallics in Mg-Al-RE alloy: a first principles study10.1016/j.jma.2015.08.003 ↗
45. Toward unraveling the effects of intermetallic compounds on the microstructure and mechanical properties of Mg–Gd–Al–Zn magnesium alloys in the as-cast, homogenized, and extruded conditions10.1016/j.msea.2016.10.084 ↗
46. Synergistic effect of Al and Gd on enhancement of mechanical properties of magnesium alloys10.1016/j.pnsc.2017.02.004 ↗
47. Interfacial bonding strengthening by thermal cycle and in-situ precipitation: wire arc additive manufacturing on forged substrate of Mg-Gd-Y-Zn-Zr alloy10.1016/j.jmrt.2025.07.103 ↗
48. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
49. Effect of diffusion bonding parameters on microstructural evolution and mechanical properties of lamellar-structured heterogeneous Mg alloy
50. Designing strong and ductile heterogeneous lamella-structured Mg alloy via diffusion bonding10.1016/j.msea.2024.146489 ↗
51. Microstructure and mechanical properties of extruded Mg-Sn alloys with a heterogeneous grain structure10.1016/j.jma.2024.05.007 ↗
52. Enhancing the formability of flame-retardant magnesium alloy through Zn alloying10.1016/j.jma.2024.11.001 ↗
53. Texture control by {10–12} twinning to improve the formability of Mg alloys: a review10.1016/j.jmst.2019.03.045 ↗
54. Transition of dominant deformation mode in bulk polycrystalline pure Mg by ultra-grain refinement down to sub-micrometer10.1016/j.actamat.2020.07.055 ↗
55. Effect of grain size on slip activity in pure magnesium polycrystals10.1016/j.actamat.2014.10.001 ↗
56. Enhancing strength-ductility synergy in a Mg-Gd-Y-Zr alloy at sub-zero temperatures via high dislocation density and shearable precipitates10.1016/j.jmst.2023.05.029 ↗
57. Revealing hetero-deformation induced (HDI) hardening and dislocation activity in a dual-heterostructure magnesium matrix composite10.1016/j.jma.2024.10.012 ↗
58. Comparative study on dislocation slip activity of the solid-solution and as-aged Mg-9.8Gd-3.5Y-2.0Zn-0.4Zr (wt%) alloys during ambient temperature quasi-in-situ compression10.1016/j.matchar.2022.112398 ↗
59. Enhancement of mechanical properties in AZ91D magnesium alloy via wire arc additive manufacturing: influence of rapid solidification and solute segregation on microstructure and deformation behavior10.1016/j.ijplas.2025.104376 ↗
60. Interface interlocking enhances mechanical strength of wire-arc directed energy deposited Mg-Al-Si/Mg-Gd-Y-Zn bimetals10.1016/j.msea.2025.148254 ↗
61. Deformation mechanisms and ductile fracture characteristics of a friction stir processed transformative high entropy alloy10.1016/j.actamat.2019.11.056 ↗
62. Grain size and void formation in Mg alloy AZ3110.1016/j.jallcom.2019.152618 ↗
63. Effects of void band orientation and crystallographic anisotropy on void growth and coalescence10.1016/j.jmps.2016.06.003 ↗
64. Visualization by X-ray tomography of void growth and coalescence leading to fracture in model materials10.1016/j.actamat.2008.02.027 ↗
65. Barnett a rationale for the influence of grain size on failure of magnesium alloy AZ31: an in situ X-ray microtomography study10.1016/j.actamat.2020.09.016 ↗
66. Uncovering the different roles of lack-of-fusion and keyhole defects on the tensile behavior of additively manufactured Ti-6Al-4V alloy