The effect of annealing on hardness, microstructure and delayed hydride cracking in Zr–2.5Nb pressure tube material
Source abstract
Abstract
Abstract The effect of annealing at 400 °C on hardness, microstructure and velocity of delayed hydride cracking (DHC) in Zr–2.5 pressure tube material in both the axial and radial directions was investigated. DHC velocity tests were performed at temperatures from 120 to 240 °C on specimens which had been annealed up to 1000 h. The β-phase initially was a thin, continuous film between α-grains providing a path for rapid hydrogen diffusion. Since the β-phase pathways were closely spaced in the axial direction but not in the radial direction, DHC velocity is 1.9 times faster in the axial direction initially. During annealing, the β-phase decomposed to discrete particles, the room temperature hardness dropped 10% and the axial DHC velocity decreased by a factor of five. The radial crack velocity decreased by a factor of three and the ratio of axial to radial DHC velocity decreased to 1.2. The decrease of this ratio corresponded to the large disruption of the β-phase caused by prolonged annealing. The activation energies for DHC velocity in these tests lay between 33 and 47 kJ/mol, suggesting that the existing theories for activation energy are incomplete.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Pickering pressure tube cracking experience
2. Effect of loading and thermal maneuvers on delayed hydride cracking in Zr–2.5 Nb alloys
3. Delayed hydrogen embrittlement in Zr–2.5wt% Nb10.1016/0022-3115(74)90174-3 ↗
4. Age hardening of Zr–2.5 wt% Nb slowly cooled from the (α+β) phase field10.1016/0022-3115(72)90004-9 ↗
5. Hydrogen diffusion in zirconium niobium alloys
6. The effect of microstructure on rates of delayed hydride cracking in Zr–2.5% Nb alloys10.1016/0022-3115(84)90533-6 ↗
7. The effects of stress, temperature and hydrogen content on hydride-induced crack growth in Zr–2.5 Pct Nb10.1007/BF02811655 ↗
8. Effect of heat treatment on delayed hydride cracking in Zr–2.5 wt pct Nb10.1007/BF02646200 ↗
9. Coleman CE, Sagat S, Amouzouvi K. Control of microstructure to increase the tolerance of zirconium alloys to hydride cracking. Report AECL-9524. Chalk River, ON, Canada: Atomic Energy Canada, 1987. p. 7.10.1016/B978-0-08-035764-5.50028-6 ↗
10. Effect of crack tip stress states and hydride matrix interaction stresses on delayed hydride cracking10.1007/BF02647211 ↗
11. CANDU-PHW pressure tubes: their manufacture, inspection and properties10.13182/NT82-A26307 ↗
12. Monitoring crack advance using acoustic emission and combined acoustic emission and potential drop in Zr–2.5% Nb10.1520/JTE11965J ↗
13. Hydride morphology and striation formation during delayed hydride cracking in Zr–2.5% Nb10.1016/0022-3115(96)00370-4 ↗
14. The ω phase in a Zr–2.5 at.% Ti alloy10.1016/0001-6160(69)90100-X ↗
15. Griffiths M, Winegar JE. The transformation behaviour of the beta phase in Zr–2.5 wt% Nb pressure tubes. Report AECL-10835. Chalk River, ON, Canada: Atomic Energy Canada, 1994. 20 pp.
16. The mechanism of hydrogen-induced delayed cracking in zirconium alloys
17. Mechanisms of hydrogen induced delayed cracking in hydride forming metals10.1007/BF02644858 ↗
18. Hydrogen diffusivity of α–β zirconium alloys and its role in delayed hydride cracking
19. Delayed hydrogen cracking in Zr–2.5 wt% Nb alloy
20. The effect of fluence and irradiation temperature on delayed hydride cracking in Zr–2.5 Nb
21. Diffusion coefficient of hydrogen in alpha zirconium, Zircaloy 2 and Zircaloy 410.1016/0022-3115(72)90065-7 ↗
22. Modelling of time dependent hydride growth at crack tips in zirconium alloys10.1088/0965-0393/2/5/008 ↗
23. The terminal solubility of hydrogen in zirconium alloys between 30 and 400°C