Heat treatment effects on creep behavior of polycrystalline SiC fibers
Source abstract
Abstract
Abstract Polycrystalline SiC fibers are being considered as potential reinforcement for ceramic matrix composites (CMCs). For these fibers with fine grain size, basic issues arise concerning thermo-mechanical properties and microstructural instability during fabrication and application of CMCs. To examine these issues, three commercially available SiC fibers were heat treated at elevated temperatures for 1 h in an Ar atmosphere. The creep resistance of SiC fibers was evaluated by the bend stress relaxation (BSR) method, and it was found that the creep resistance could be improved by heat treatment. Combining the results of the BSR tests with the results of X-ray diffraction examinations indicated that the creep resistance of SiC fibers is mainly related to the β-SiC grain size and the composition at or adjacent to the grain boundaries. Also, the apparent activation energy of creep for both Hi-Nicalon™ and Hi-Nicalon™ type S fiber increased with increasing heat treatment temperature. In the case of Tyranno™-SA fiber, the apparent activation energy of creep did not show an obvious dependence on the heat treatment temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Advanced ceramic composite materials for fusion/fission reactor systems
3. Potential application of ceramic matrix composites to aero-engine components10.1016/S1359-835X(98)00139-0 ↗
4. Recent advances in Nicalon ceramic fibers including Hi-Nicalon Type S10.1016/S0151-9107(01)80004-0 ↗
5. High-strength alkali-resistant sintered SiC fiber stable to 2200 °C10.1038/35820 ↗
6. Preparation of SiC/SiC composites by hot pressing, using Tyranno SA fiber as reinforcement10.1111/j.1151-2916.2003.tb03272.x ↗
7. Microstructural and mechanical characteristics of SiC/SiC composites with modified RS process10.1016/S0022-3115(00)00679-6 ↗
8. A simple test for thermomechanical evaluation of ceramic fibers10.1111/j.1151-2916.1992.tb05455.x ↗
9. Comparison of bend stress relaxation and tensile creep of CVD SiC fibers10.1111/j.1151-2916.1995.tb07960.x ↗
10. Self-diffusion of 14C in polycrystalline β-SiC10.1007/BF00737031 ↗
11. Si-30 diffusion in alpha-SiC and beta-SiC
12. Monotonic tension, fatigue and creep behavior of SiC-fiber-reinforced SiC-matrix composites: a review10.1016/S0266-3538(99)00014-7 ↗
13. High-temperature compressive creep of liquid phase sintered silicon carbide10.1016/S1359-6454(99)00072-5 ↗
14. Properties of polycarbosilane-derived silicon carbide fibers with various C/Si compositions10.1016/S0266-3538(99)00009-3 ↗
15. Fine diameter ceramic fibers10.1016/S0955-2219(00)00090-X ↗
16. Fracture mechanisms for SiC fibers and SiC/SiC composites under stress-rupture conditions at high temperatures10.1016/S0096-3003(03)00570-8 ↗
17. Effects of composition and heat treatment conditions on the tensile strength and creep resistance of SiC-based fibers10.1016/S0955-2219(99)00114-4 ↗