Friction stir welding of as-extruded Mg–Al–Zn alloy with higher Al content. Part II: Influence of precipitates
Source abstract
Abstract
Abstract Extruded Mg–Al–Zn (AZ80) plates were subjected to friction stir welding at a welding speed of 100 mm·min − 1 and a tool rotation rates of 800 rpm. Different heat treatments were conducted before or after welding with the aim to evaluate the influence of precipitates on the weld properties. The welding joint with the solution treatment before welding exhibited enhanced ductility and decreased yield strength due to the dissolution of β-Mg 17 Al 12 and the coarsening of grains. After aging at 180 °C for 16 h, a banded structure consisting of different densities of discontinuous β-Mg 17 Al 12 precipitates was observed in the nugget zone of both joints with or without the solution treatment before welding. The yield strength of the joint without the solution before welding increased by 30% after aging, with the elongation being decreased. The fracture behavior of the aged joints was closely related to the banded structure where the crack propagated more easily along the coarse discontinuously precipitated bands.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
2. Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B10.1016/j.ijplas.2004.05.018 ↗
3. Effects of heat input on tensile properties and fracture behavior of friction stir welded Mg–3Al–1Zn alloy10.1016/j.msea.2009.09.044 ↗
4. Effects of rotation rates on microstructure, mechanical properties, and fracture behavior of friction stir-welded (FSW) AZ31 magnesium alloy10.1007/s11661-012-1373-4 ↗
5. Friction stir welding of AZ31 magnesium alloy rolled sheets: influence of processing parameters10.1016/j.actamat.2008.09.011 ↗
6. The influence of the ratio of “rotational speed/traverse speed” (ω/ν) on mechanical properties of AZ31 friction stir welds10.1016/j.ijmachtools.2006.01.007 ↗
7. Joint properties of friction stir welded AZ31B-H24 magnesium alloy10.1179/026708303225001867 ↗
8. Basal plane texture and flow pattern in friction stir weld of a magnesium alloy10.1007/s11661-003-0228-4 ↗
9. Effect of micro-texture on fracture location in friction stir weld of Mg alloy AZ61 during tensile test10.1016/S1359-6462(03)00210-0 ↗
10. The microstructure and mechanical properties of friction stir welded Mg–3Al–1Zn alloy at high rotation rates
11. Microstructural evolution and its effect on Hall–Petch relationship in friction stir welding of thixomolded Mg alloy AZ91D10.1023/A:1026351619636 ↗
12. The joint characteristics of friction stir welded AZ91D magnesium alloy10.2320/matertrans.44.917 ↗
13. Analysis of the grain orientation and texture of friction stir welded magnesium alloy10.4028/www.scientific.net/MSF.620-622.97 ↗
14. Effect of microstructural evolution on mechanical properties of friction stir welded ZK60 alloy10.1016/j.msea.2007.08.043 ↗
15. Microstructural evolution of a heat-resistant magnesium alloy due to friction stir welding10.1016/j.scriptamat.2005.01.003 ↗
16. Microstructural evolution and mechanical properties of friction stir welded Mg–Zn–Y–Zr alloy10.1016/j.msea.2007.03.041 ↗
17. Microstructure-property studies in friction-stir welded, thixomolded magnesium alloy AM6010.1023/A:1022321107957 ↗
18. Effect of Y addition on microstructure and mechanical properties of friction stir welded ZK60 alloy
19. Effects of friction stir welding parameters on microstructures and mechanical properties of ZK60 magnesium alloy joints
20. Effect of friction stir processing procedures on microstructure and mechanical properties of Mg–Al–Zn casting10.1007/s11661-009-9923-0 ↗
21. Microstructure and properties of AZ80 magnesium alloy prepared by hot extrusion from recycled machined chips
22. Enhanced mechanical properties of Mg–Al–Zn cast alloy via friction stir processing10.1016/j.scriptamat.2006.10.035 ↗
23. Quantitative characterization of Mg17Al12 phase and grain size in HPDC AZ91 magnesium alloy10.1016/j.jallcom.2007.07.017 ↗
24. Enhancing the high-cycle fatigue strength of Mg–9Al–1Zn casting by friction stir processing10.1016/j.scriptamat.2009.05.023 ↗
25. On the competition between continuous and discontinuous precipitations in binary Mg–Al alloys
26. Relationship between grain size and Zener–Holloman parameter during friction stir processing in AZ31 Mg alloys10.1016/j.scriptamat.2004.05.043 ↗
27. Recrystallization mechanism and the relationship between grain size and Zener–Hollomon parameter of Mg–Al–Zn–Ca alloys during hot compression10.1016/j.scriptamat.2010.04.012 ↗
28. Humphreys · 2004
29. Characterization of plastic flow and resulting microtextures in a friction stir weld10.1007/s11663-004-0018-4 ↗
30. On the formation of onion rings in friction stir welds10.1016/S0921-5093(01)01474-5 ↗
31. Microstructural studies of friction stir welds in 2024-T3 aluminum10.1016/S0921-5093(01)01358-2 ↗
32. A study of texture patterns in friction stir welds10.1016/j.actamat.2007.11.016 ↗
33. TEM study of continuous precipitation in Mg–9wt.%Al–1wt.%Zn alloy10.1016/S1359-6454(00)00004-5 ↗
34. Age hardening in a Mg–9 wt percent Al alloy10.1016/0001-6160(68)90109-0 ↗
35. A process model for friction stir welding of age hardening aluminum alloys10.1007/s11661-001-0128-4 ↗
36. Torque, power requirement and stir zone geometry in friction stir welding through modeling and experiments10.1016/j.scriptamat.2008.08.015 ↗
37. Microstructure, texture and residual stress in a friction-stir-processed AZ31B magnesium alloy10.1016/j.actamat.2007.12.020 ↗
38. Effects of solidification rate and ageing on the microstructure and mechanical properties of AZ91 alloy10.1016/S0921-5093(01)01467-8 ↗
39. Fracture behavior of AZ91 magnesium alloy10.1016/S0167-577X(00)00041-0 ↗