TEM microstructural characterization of melt-spun aged Al–6Si–3Cu–xMg alloys
Source abstract
Abstract
Three Al-6Si-3Cu-xMg alloys (x = 0.59, 3.80 and 6.78 wt.%) were produced using melt-spinning. As-melt-spun ribbons were aged at 150, 180 and 210 deg. C for times between 0.05 and 100 h. Microstructural changes were examined using transmission electron microscopy (TEM) and microhardness was measured. TEM analysis of the as-melt-spun alloys revealed 5 nm nanoparticles and larger particles (50 nm) composed of Al{sub 2}Cu ({theta}) for the 0.59% Mg alloy and Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} (Q) for 3.80% and 6.78% Mg alloys. Silicon solid solubility was extended to 9.0 at.% and Mg in solid solution reached 6.7 at.%. After aging treatments the 6.78% Mg alloy exhibited the most significant increase in microhardness, reaching 260 kg/mm{sup 2}. TEM analysis of aged specimens also showed {theta} and Q phase (5-20 nm nanoparticles and 35-40 nm particles). The combination of the volume fraction and size of the particles plays an important role in microhardness variation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Effect of Mg on the aging behaviour of Al–Si–Cu 319 type aluminium casting alloys10.1023/A:1004645928886 ↗
2. Effect of magnesium content on the ageing behaviour of water chilled Al–Si–Cu–Mg–Fe–Mn (380) alloy casting10.1007/BF00362130 ↗
3. Precipitation and age-hardening in Al–Si–Cu–Mg–Fe casting alloys10.4028/www.scientific.net/MSF.217-222.777 ↗
4. Precipitation strengthening and mechanical properties of hypereutectic P/M Al–Si–Cu–Mg alloys containing Fe and Ni10.4028/www.scientific.net/MSF.217-222.789 ↗
5. Atom probe studies on the early stages of precipitation in Al–Mg–Si alloys10.1016/S0921-5093(98)00548-6 ↗
6. Effect of alloying elements on the segregation and dissolution of Al2Cu phase in Al–Si–Cu 319 alloys10.1023/A:1022857703995 ↗
7. New directions in aluminum-based P/M materials for automotive applications
8. Quantitative evaluation of a-Al nano-particles in amorphous Al87Ni7Gd6 comparison of XRD, DSC, and TEM10.1016/S1359-6462(03)00127-1 ↗
9. Rapidly solidified alloys made by chill block melt-spinning processes10.1016/0022-0248(84)90308-7 ↗
10. Aging precipitation and recrystallization of rapidly solidified Cu–Cr–Zr–Mg alloy10.1016/S0921-5093(98)01149-6 ↗
11. A comparative study of primary Al precipitation in amorphous Al87Ni7La5Zr by means of WAXS, SAXS, TEM and DSC techniques10.1016/j.actamat.2004.07.005 ↗
12. Transformation and ageing behaviour of melt-spun Ni–Mn–Ga shape memory alloys10.1016/S0921-5093(99)00363-9 ↗
13. Characterization investigations of a melt-spun ternary Al–8Si–5.1Cu (in wt.%) alloy10.1016/S0167-577X(03)00051-X ↗
14. Amorphous, nanoquasicrystalline and nanocrystalline alloys in Al-based systems
15. Precipitation hardening in metals10.1179/026708399773002782 ↗