Characterisation of a centuries-old patinated copper roof tile from Queen Anne's Summer Palace in Prague
Source abstract
Abstract
This paper presents an in-depth characterisation study of the patina formed on a copper tile taken from the roof of Queen Anne's Summer Palace in Prague after > 300 years of exposure to the action of the atmosphere. A wide variety of techniques have been used, including metallographic and chemical analysis (electrogravimetry, AAS, XRF) of the copper matrix, and spectroscopic and microscopic investigations (GIXRD, FTIR, TEM/EDS and SEM/EDS) to determine the composition and structure of the patina. The major conclusions of the study are: (a) the base copper contains abundant inclusions mainly of rosiaite (PbSbO); (b) the patina is formed by an inner sublayer of cuprite (CuO) and an outer sublayer of brochantite [CuSO(OH)] and antlerite [CuSO(OH)] and traces of azurite [Cu(CO)(OH)]; and (c) the brochantite/antlerite crystals are randomly doped with Fe and C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Cultural Heritage Materials Analysis · Advanced Cellulose Research Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Morphological study of 16-year patinas formed on copper in a wide range of atmospheric exposures10.1016/j.corsci.2007.05.030 ↗
2. Critical review: copper runoff from outdoor copper surfaces at atmospheric conditions10.1021/es404410s ↗
3. Atmospheric Corrosion10.1002/9781118762134 ↗
4. Graedel · 1990
5. Atmospheric corrosion of copper and the colour, structure and composition of natural patinas on copper10.1016/j.corsci.2005.09.011 ↗
6. Atmospheric corrosion and conservation of copper and bronze10.2495/978-1-84564-032-3/04 ↗
7. Prediction of the long-term corrosion rate of copper alloy objects10.1002/maco.201408112 ↗
8. Analysis of historic copper patinas. Influence of inclusions on patina uniformity10.3390/ma10030298 ↗
9. Langner
10. Prediction of long-term corrosion rate of copper alloy objects
11. 2015
12. Pecharsky · 2005
13. Craddock · 1995
14. EN 1652 · 1997
15. Metallurgical and chemical characterization of copper alloy reference materials within laser ablation inductively coupled plasma mass spectrometry: method development for minimally-invasive analysis of ancient bronze objects10.1016/j.sab.2012.11.001 ↗
16. Study of ancient Islamic gilded pieces combining PIXE-RBS on external microprobe with SEM images10.1007/s00339-008-4497-z ↗
17. Welter · 2017
18. Effects of sulphur compounds on materials, including historic and cultural monuments
19. Mattsson · 1982 · 365
20. A mineralogical study of the deportment and reaction of silver during copper electrorefining10.1007/BF02696987 ↗
21. Reactions of copper patina compounds—I. Influence of some air pollutants10.1016/S1352-2310(98)00057-0 ↗
22. The characterization of patina components by X-ray diffraction and evolved gas analysis10.1016/0010-938X(87)90049-7 ↗
23. Copper and bronze
24. Copper patinas formed in the atmosphere—III. A semi-quantitative assessment of rates and constraints in the greater New York Metropolitan Area10.1016/0010-938X(87)90054-0 ↗
25. The evolution of outdoor copper patina10.1016/S0010-938X(01)00081-6 ↗
26. UN/ECE · 1998
27. Some applications of potential-pH diagrams to the study of localized corrosion10.1149/1.2132800 ↗
28. Copper patinas formed in the atmosphere—II. A qualitative assessment of mechanisms10.1016/0010-938X(87)90053-9 ↗
29. Corrosion on the Statue of Liberty. Part. IV—copper behaviour
30. The reaction of simulated rain with copper, copper patina, and some copper compounds10.1016/0010-938X(87)90052-7 ↗
31. The corrosion of bronze monuments in polluted urban sites: a report on the stability of copper mineral species at different pH levels
32. Heterogeneous reaction of SO2 with soot: the roles of relative humidity and surface composition of soot in surface sulfate formation10.1016/j.atmosenv.2017.01.005 ↗
33. Metallographic studies of the copper patina formed in the atmosphere10.1016/0010-938X(87)90048-5 ↗
34. EN ISO 9223 · 2012
35. Twenty-five years of continuous sulphur dioxide emission reduction in Europe10.5194/acp-7-3663-2007 ↗