journal article·2009-08

Microstructure and mechanical properties of Hi-Nicalon™ Type S fibers annealed and crept in various oxygen partial pressures

J.J. Sha, T. Hinoki, A. Kohyama

Materials Characterization· Volume 60· Issue 8
Publisher page

Abstract

Abstract The microstructure and mechanical properties of Hi-Nicalon™ Type S fibers annealed and crept at elevated temperatures in various oxygen partial pressures were investigated. Observations and analyses of the microstructure indicated that (i) the morphologies of the fibers were heavily dependent on the oxygen partial pressure and mechanical state; (ii) the extent of fiber oxidation under creep conditions was greater in comparison to that of fibers under annealing conditions; and (iii) the transition from passive to active oxidation was accelerated by reducing the oxygen partial pressure. For the mechanical properties of fibers annealed at 1500 °C, the tensile strengths decreased with decreasing oxygen partial pressure, while the creep resistance increased slightly with decreasing oxygen partial pressure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Thermal properties of materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
2. Mechanical and thermal stabilities of Hi-Nicalon fiber under annealing and creep in various oxygen partial pressures10.1016/j.corsci.2008.08.003 ↗
3. Microstructural evolution under load and high temperature deformation mechanisms of a mullite/alumina fibre10.1016/S0955-2219(01)00461-7 ↗
4. Microstructural evolution of Hi-Nicalon™ SiC fibers annealed and crept in various oxygen partial pressure atmospheres10.1023/A:1004772000985 ↗
5. A theoretical and experimental approach to the active-to-passive transition in the oxidation of silicon carbide: experiments at high temperatures and low total pressures10.1023/A:1004313022769 ↗
6. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
7. Strength and fracture properties of advanced SiC-based fibers10.1007/s11029-006-0063-y ↗
8. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
9. A simple test for thermomechanical evaluation of ceramic fibers10.1111/j.1151-2916.1992.tb05455.x ↗
10. Active-to-passive oxidation transition for polycarbosilane-derived silicon carbide fibers heated in Ar-O2 gas mixtures10.1023/A:1014945823031 ↗
11. Oxidation behavior of Si-M-C-O fibers under wide range of oxygen partial pressures10.1023/A:1020608704120 ↗
12. Effect of heat treatment on the tensile strength and creep resistance of advanced SiC fibers10.1016/j.jnucmat.2004.04.123 ↗
13. Corrosion of Non-oxide ceramics10.1016/S0272-8842(96)00008-9 ↗
14. Thermal stability of low-oxygen silicon carbide fiber (Hi-Nicalon) subjected to selected oxidation treatment10.1111/j.1151-2916.2000.tb01409.x ↗
15. Some new perspectives on oxidation of silicon carbide and silicon nitride10.1111/j.1151-2916.1991.tb04348.x ↗
16. Pressure effects on the thermal-stability of silicon-carbide fibers10.1111/j.1151-2916.1989.tb06100.x ↗
17. Microstructural development of SCS-6 SiC fibers during high temperature creep10.1557/JMR.1998.0263 ↗
18. Fracture mechanisms for SiC fibers and SiC/SiC composites under stress-rupture conditions at high temperatures10.1016/S0096-3003(03)00570-8 ↗